Effect of Powder Reuse Times on Additive Manufacturing of Ti-6Al-4V by Selective Electron Beam Melting

被引:1
|
作者
H. P. Tang
M. Qian
N. Liu
X. Z. Zhang
G. Y. Yang
J. Wang
机构
[1] Northwestern Institute for Nonferrous Metal Research,State Key Laboratory of Porous Metal Materials
[2] RMIT University,School of Aerospace, Mechanical and Manufacturing Engineering, Centre for Additive Manufacturing
[3] Northeastern University,School of Materials and Metallurgy
来源
JOM | 2015年 / 67卷
关键词
Powder Particle; Additive Manufacturing; Tensile Sample; Powder Characteristic; Tensile Mechanical Property;
D O I
暂无
中图分类号
学科分类号
摘要
An advantage of the powder-bed-based metal additive manufacturing (AM) processes is that the powder can be reused. The powder reuse or recycling times directly affect the affordability of the additively manufactured parts, especially for the AM of titanium parts. This study examines the influence of powder reuse times on the characteristics of Ti-6Al-4V powder, including powder composition, particle size distribution (PSD), apparent density, tap density, flowability, and particle morphology. In addition, tensile samples were manufactured and evaluated with respect to powder reuse times and sample locations in the powder bed. The following findings were made from reusing the same batch of powder 21 times for AM by selective electron beam melting: (i) the oxygen (O) content increased progressively with increasing reuse times but both the Al content and the V content remained generally stable (a small decrease only); (ii) the powder became less spherical with increasing reuse times and some particles showed noticeable distortion and rough surfaces after being reused 16 times; (iii) the PSD became narrower and few satellite particles were observed after 11 times of reuse; (iv) reused powder showed improved flowability; and (v) reused powder showed no measurable undesired influence on the AM process and the samples exhibited highly consistent tensile properties, irrespective of their locations in the powder bed. The implications of these findings were discussed.
引用
收藏
页码:555 / 563
页数:8
相关论文
共 50 条
  • [31] Effect of Build Orientation in Electron Beam Melting of Ti-6Al-4V Specimens
    Muller-Kamskii, Gary
    Stepanov, Stepan
    Strokin, Evgeny
    Kolomiets, Anastasia
    Kovalevskyi, Igor
    Popov, Artemiy
    [J]. PROCEEDINGS OF THE 2020 IEEE 10TH INTERNATIONAL CONFERENCE ON NANOMATERIALS: APPLICATIONS & PROPERTIES (NAP-2020), 2020,
  • [32] Massive transformation in Ti-6Al-4V additively manufactured by selective electron beam melting
    Lu, S. L.
    Qian, M.
    Tang, H. P.
    Yan, M.
    Wang, J.
    StJohn, D. H.
    [J]. ACTA MATERIALIA, 2016, 104 : 303 - 311
  • [33] Surface characteristics of laser polished Ti-6Al-4V parts produced by electron beam melting additive manufacturing process
    Safak Nesli
    Oguzhan Yilmaz
    [J]. The International Journal of Advanced Manufacturing Technology, 2021, 114 : 271 - 289
  • [34] Surface characteristics of laser polished Ti-6Al-4V parts produced by electron beam melting additive manufacturing process
    Nesli, Safak
    Yilmaz, Oguzhan
    [J]. INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2021, 114 (1-2): : 271 - 289
  • [35] The effect of hot isostatic pressure on the corrosion performance of Ti-6Al-4V produced by an electron-beam melting additive manufacturing process
    Leon, Avi
    Levy, Galit Katarivas
    Ron, Tomer
    Shirizly, Amnon
    Aghion, Eli
    [J]. ADDITIVE MANUFACTURING, 2020, 33
  • [36] Hybrid Electron Beam Powder Bed Fusion Additive Manufacturing of Ti-6Al-4V: Processing, Microstructure, and Mechanical Properties
    Tosi, R.
    Muzangaza, E.
    Tan, X. P.
    Wimpenny, D.
    Attallah, M. M.
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2022, 53 (03): : 927 - 941
  • [37] Additive Manufacturing of Ti-6Al-4V Using a Pulsed Laser Beam
    Nassar, Abdalla R.
    Reutzel, Edward W.
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2015, 46A (06): : 2781 - 2789
  • [38] Additive Manufacturing of Ti-6Al-4V Using a Pulsed Laser Beam
    Abdalla R. Nassar
    Edward W. Reutzel
    [J]. Metallurgical and Materials Transactions A, 2015, 46 : 2781 - 2789
  • [39] Toward Manufacturing Quality Ti-6Al-4V Lattice Struts by Selective Electron Beam Melting (SEBM) for Lattice Design
    Zhang, X. Z.
    Tang, H. P.
    Leary, M.
    Song, T.
    Jia, L.
    Qian, M.
    [J]. JOM, 2018, 70 (09) : 1870 - 1876
  • [40] Toward Manufacturing Quality Ti-6Al-4V Lattice Struts by Selective Electron Beam Melting (SEBM) for Lattice Design
    X. Z. Zhang
    H. P. Tang
    M. Leary
    T. Song
    L. Jia
    M. Qian
    [J]. JOM, 2018, 70 : 1870 - 1876