摘要
The thermal fatigue of a heat-resistant Fe-0.45C-26Cr-33Ni-2Si-2Nb alloy is studied during thermal cycling in the temperature range 50-900°C up to 1000 cycles. The alloy is investigated in the initial as-cast state and after isothermal annealing during 1000 h at a temperature of 800, 900, 1000, or 1100°C; these conditions imitate the temperature conditions of operation and the structural state of various layers in a reaction pipe in the radiant furnace coils of ethylene production installations. After isothermal annealing, the thermal fatigue life of the alloy is found to decrease by a factor of 1.7-1.2 as compared to the initial as-cast state. It is shown that isothermal annealing and subsequent thermal cycling lead to the formation of carbide precipitates of various sizes in the alloy structure that affect the thermal fatigue life of the alloy. Thermal fatigue cracks are shown to form and grow predominantly at the sites of accumulation of fine carbide precipitates. Coarse (>10 μm) precipitates retard crack growth, and cracks branch near such precipitates. © 2011 Pleiades Publishing, Ltd.
引用
收藏
页码:228 / 233
页数:5
相关论文
共 50 条
  • [41] 330Cb alloy (Fe-35Ni-18Cr-1Nb-2Si) oxidation study between 800 and 1000 °C
    Issartel, C.
    Buscail, H.
    Nguyen, C. T.
    Fleurentin, A.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2010, 61 (11): : 929 - 938
  • [42] Influence of carburisation on the 330Cb (Fe-35Ni-18Cr-1Nb-2Si) alloy oxidation at 900 degrees C
    Buscail, H.
    Issartel, C.
    Nguyen, C. T.
    Perrier, S.
    Fleurentin, A.
    MATERIAUX & TECHNIQUES, 2010, 98 (03): : 209 - 218
  • [43] Influence of Nb on the Hot Corrosion Behaviors of a Fe-Cr-Ni Heat-Resistant Steel Weld Metal in the Na2SO4-NaCl Molten Salt at 700?
    Zhang, Xu
    Wan, Jinchu
    Zhu, Liang
    Zhou, Hui
    Yang, Zonghui
    METALS AND MATERIALS INTERNATIONAL, 2023, 29 (12) : 3645 - 3654
  • [44] Segregation engineering in a promising heat-resistant AlCoCrFeMo0.05Ni2 high entropy alloy
    Ye, Qilu
    Yang, Gang
    Yang, Bin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 869
  • [45] Transformation of Niobium Carbide in Heat-Resistant Alloys Based on Fe – 25Cr – 35Ni at 900°C and 1150°C
    E. V. Zabavicheva
    S. N. Petrov
    S. Yu. Kondrat’ev
    Metal Science and Heat Treatment, 2024, 65 : 605 - 612
  • [46] Effect of Al/Ti Ratio on Hot Deformation Characteristics and Microstructure Evolution of 15Cr-30Ni-Fe Heat-Resistant Alloy
    Zhang, Huai
    Shi, Chengbin
    Wang, Shizhou
    Lan, Peng
    Li, Jing
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024,
  • [47] Thermal and Electron Microprobe Analyses of an Ni-0.5C-15Cr-3.2Si-2B Alloy
    Il'inykh, A. S.
    Zamyatin, V. M.
    Barbin, N. M.
    RUSSIAN METALLURGY, 2014, 2014 (02): : 135 - 139
  • [48] Influence of thermal treatment on microstructure of Fe75Ni2Si8B13C2 amorphous alloy
    Minic, Dusan M.
    Blagojevic, Vladimir A.
    David, Bohumil
    Pizurova, Nadezda
    Zak, Tomas
    Minic, Dragica M.
    INTERMETALLICS, 2012, 25 : 75 - 79
  • [49] Effect of Grain-Boundary Fe2Nb Phase on Stress-Assisted Grain-Boundary Oxidation Behavior in Novel Austenitic Heat-Resistant Steel of Fe-20Cr-35Ni-2.5Nb
    Sueishi, Y.
    Takeyama, M.
    Tezuka, H.
    PROCEEDINGS OF THE 9TH INTERNATIONAL SYMPOSIUM ON SUPERALLOY 718 & DERIVATIVES: ENERGY, AEROSPACE, AND INDUSTRIAL APPLICATIONS, 2018, : 477 - 487
  • [50] EXPERIMENTAL AND COMPUTATIONAL STUDY ON GRAIN BOUNDARY AND GRAIN INTERIOR PRECIPITATION OF FE2NB LAVES PHASE IN FE-CR-NI-NB AUSTENITIC HEAT RESISTANT STEELS
    Kikuchi, Kenta
    Nakashima, Hirotoyo
    Takeyama, Masao
    JOINT EPRI - 123HIMAT INTERNATIONAL CONFERENCE ON ADVANCES IN HIGH-TEMPERATURE MATERIALS, 2019, 2019, : 1408 - 1417