Fatigue strength and fracture behaviour of CHS-to-RHS T-joints subjected to out-of-plane bending

被引:0
|
作者
Li-Chun Bian
Jae-Kyoo Lim
Yon Jig Kim
机构
[1] Nanjing University of Technology Nanjing,College of Mechanical and Power Engineering
[2] Chonbuk National University,Department of Mechanical Design, Automobile Hi
来源
关键词
Hollow Section; Welded Joint; Fatigue; Hot Spot Stress; Stress Concentration Factor;
D O I
暂无
中图分类号
学科分类号
摘要
The fatigue behaviour of six different hollow section T-joints subjected to out-of-plane bending moment was investigated experimentally using scaled steel models. The joints had circular brace members and rectangular chord members. Hot spot stresses and the stress concentration factors (SCFs) were determined experimentally. Fatigue testing was carried out under constant amplitude loading in air. The test results have been statistically evaluated, and show that the experimental SCF values for circular-to-rectangular (CHS-to-RHS) hollow section joints were found to be below those of circular-to-circular (CHS-to-CHS) hollow section joints. The fatigue strength, referred to experimental hot spot stress, was in reasonably good agreement with referred fatigue design codes for tubular joints.
引用
下载
收藏
页码:207 / 214
页数:7
相关论文
共 50 条
  • [41] Fracture mechanics analysis for a mooring system subjected to tension and out-of-plane bending
    Xue, X.
    Chen, N-Z
    FIRST CONFERENCE OF COMPUTATIONAL METHODS IN OFFSHORE TECHNOLOGY (COTECH2017), 2017, 276
  • [42] Design formulae for predicting the stress concentration factors of concrete-filled T-joints under out-of-plane bending
    Matti, Feleb N.
    Mashiri, Fidelis R.
    STRUCTURES, 2020, 28 : 2073 - 2095
  • [43] Fatigue behaviour of thin-walled tube-to-tube T-joints under in-plane bending
    Mashiri, FR
    Zhao, XL
    Grundy, P
    TUBULAR STRUCTURES IX, 2001, : 259 - 268
  • [44] Out-of-plane bending fire response of steel tubular T-joints: A sequentially coupled thermal-stress modelling
    Ahmadpour, F.
    Zeinoddini, M.
    Rashnooie, R.
    Mo'tamedi, M.
    Zandi, A. P.
    THIN-WALLED STRUCTURES, 2022, 171
  • [45] Parametric study and equations of the maximum SCF for concrete filled steel tubular T-joints under in-plane and out-of-plane bending
    Musa, Idris A.
    Mashiri, Fidelis R.
    THIN-WALLED STRUCTURES, 2019, 135 : 245 - 268
  • [46] Fatigue strength of thin-walled tube-to-plate T-Joints under in-plane bending
    Mashiri, FR
    Zhao, XL
    Grundy, P
    ADVANCES IN STEEL STRUCTURES, VOLS 1 AND 2, 1999, : 983 - 990
  • [47] Assessment of fatigue strength of cruciform welded joints failing from weld roots under out-of-plane bending
    Mori T.
    Uchida D.
    Fukuoka T.
    Myoken M.
    Doboku Gakkai Ronbunshuu A, 2010, 66 (03) : 568 - 575
  • [48] Behavior of thick-walled CHS X-joints under cyclic out-of-plane bending
    Wang, Wei
    Chen, Yiyi
    Meng, Xiande
    Leon, Roberto T.
    JOURNAL OF CONSTRUCTIONAL STEEL RESEARCH, 2010, 66 (06) : 826 - 834
  • [49] Cold-formed high strength steel CHS-to-RHS T- and X-joints: Performance and design after fire exposures
    Pandey, Madhup
    Young, Ben
    THIN-WALLED STRUCTURES, 2023, 189
  • [50] Bending behavior of single hat-shaped composite T-joints under out-of-plane loading for lightweight automobile structures
    Hou, Wenbin
    Xu, Xianzhe
    Wang, Haifeng
    Tong, Liyong
    JOURNAL OF REINFORCED PLASTICS AND COMPOSITES, 2018, 37 (12) : 808 - 823