Crevice Corrosion Behavior of Stainless Steels in a Flue Gas Desulfurization Environment

被引:0
|
作者
Yong Hu
Hao Zhang
HuiYing Zhang
MingHui Ouyang
YongQi Hu
LiHua Wang
Cheng Chu
JingChao Wang
JingTang Wang
机构
[1] Lanzhou University of Technology,State Key Laboratory of Advanced Processing and Recycling of Non
[2] Lanzhou University of Technology,Ferrous Metals
[3] Wenzhou Pump and Valve Engineering Research Institute,School of Materials Science and Engineering
[4] Lanzhou University of Technology,Institute of Materials
[5] Shanghai University,Institute of Corrosion
[6] Xuanda Industrial Group Co.,Resistant Special Metal Materials of Xuanda Zhejiang Province
[7] Ltd.,undefined
来源
Journal of Materials Engineering and Performance | 2023年 / 32卷
关键词
crevice corrosion; flue gas desulfurization; passive film; stainless steel;
D O I
暂无
中图分类号
学科分类号
摘要
In this study, cyclic potentiodynamic polarization, potentiodynamic–potentiostatic–potentiodynamic (PD–PS–PD) impedance, and semiconductor performance tests, combined with SEM/energy spectroscopy and XPS detection were used to systematically study the crevice corrosion behavior of SS904L, SS2205, SS2507, and SS254SMO stainless steels with synthetic crevice electrodes in simulated mixture solution of NaCl (10 g/L) and Na2SO4 (5.7 g/L) at 60 °C and pH = 3.5. The results showed that the corrosion behavior among the four stainless steels was most severe at the crevice mouth position, and the SS2507 formed passive films with better stability. Through the discussion of four stainless steels crevice corrosion mechanisms, the crevice geometry restricts the diffusion of metal ions and produces an autocatalytic effect to promote the development of crevice corrosion. Cr, Mo and N have a synergistic effect that improves resistance to crevice corrosion. The crevice corrosion resistance of the four stainless steels decreased in order of SS2507 > SS254SMO > SS904L > SS2205.
引用
收藏
页码:10567 / 10581
页数:14
相关论文
共 50 条
  • [41] Corrosion Investigation of Ammonia Flue Gas Desulfurization
    Lian, Zhouyang
    Luo, Zhengwei
    Yuan, Lirui
    Wei, Wuji
    MATERIALS PERFORMANCE, 2016, 55 (09) : 50 - 53
  • [42] CORROSION TESTS IN FLUE GAS DESULFURIZATION PROCESSES
    TICE, EA
    MATERIALS PERFORMANCE, 1974, 13 (04) : 26 - 33
  • [43] A discussion on evaluation criteria for crevice corrosion of various stainless steels
    Xuan Wu
    Yuanyuan Liu
    Yangting Sun
    Nianwei Dai
    Jin Li
    Yiming Jiang
    Journal of Materials Science & Technology, 2021, 64 (05) : 29 - 37
  • [44] ELECTROCHEMICAL STUDIES OF CREVICE CORROSION RATES ON STAINLESS-STEELS
    TROMANS, D
    FREDERICK, L
    CORROSION, 1983, 39 (08) : 305 - 312
  • [45] CALCULATION OF INCUBATION TIME OF CREVICE CORROSION OF STAINLESS-STEELS
    CROLET, JL
    DEFRANOU.JM
    CORROSION SCIENCE, 1973, 13 (08) : 575 - 585
  • [46] Effect of nickel alloying on crevice corrosion resistance of stainless steels
    Azuma, S
    Kudo, T
    Miyuki, H
    Yamashita, M
    Uchida, H
    CORROSION SCIENCE, 2004, 46 (09) : 2265 - 2280
  • [47] A discussion on evaluation criteria for crevice corrosion of various stainless steels
    Wu, Xuan
    Liu, Yuanyuan
    Sun, Yangting
    Dai, Nianwei
    Li, Jin
    Jiang, Yiming
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 64 : 29 - 37
  • [48] The Corrosion Behavior of WEDM Machined Stainless Steels in a Pyrolysis Environment
    Benes, Libor
    Mouralova, Katerina
    Midula, Pavol
    Snow, Jan
    Lysonkova, Irena
    Pilnaj, Dominik
    Burdova, Hana
    Prokes, Tomas
    Zahradnicek, Radim
    Fries, Jiri
    Kuran, Pavel
    Kubenka, Martin
    METALS, 2023, 13 (01)
  • [49] PITTING AND CREVICE CORROSION OF STAINLESS-STEELS IN CHLORIDE SOLUTIONS
    SCHEIDEGGER, R
    MULLER, RO
    WERKSTOFFE UND KORROSION-MATERIALS AND CORROSION, 1980, 31 (05): : 387 - 393
  • [50] Crevice corrosion of duplex stainless steels in natural and chlorinated seawater
    Larche, N.
    Thierry, D.
    Debout, V.
    Blanc, J.
    Cassagne, T.
    Peultier, J.
    Johansson, E.
    Taravel-Condat, C.
    REVUE DE METALLURGIE-CAHIERS D INFORMATIONS TECHNIQUES, 2011, 108 (7-8): : 451 - 463