Sliding wear and friction behaviour of Al-18% Si-0.5% Mg alloy

被引:57
|
作者
Dwivedi, DK [1 ]
Arjun, TS [1 ]
Thakur, P [1 ]
Vaidya, H [1 ]
Singh, K [1 ]
机构
[1] Reg Engn Coll, Dept Mech Engn, Hamirpur 177005, India
关键词
sliding speed; contact load; interface temperature; microstructures; mild oxidative wear and severe wear;
D O I
10.1016/j.jmatprotec.2004.04.379
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In present paper, the influence of copper on wear-friction behaviour of hypereutectic Al-Si alloy (Al-18% Si-0.5% Mg) has been investigated. Sliding tests were conducted under dry sliding conditions against hardened steel En-31 counter surface over a range of sliding speed from 2.0 to 7.0 m/s and contact load from 10 to 80 N. It was observed that the wear rate is a function of contact load, sliding speed, composition and thermal softening characteristics of sliding metal. Wear of hypereutectic aluminium-silicon alloy is not appreciably affected with the addition of copper. However, addition of copper increases the transition load at 2.0 m/s sliding speed. Copper addition more than 2%, did not show any effect on the transition load. (C) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:323 / 328
页数:6
相关论文
共 50 条
  • [41] Characterization of Al-12Si alloy and its composites in dry sliding friction and wear at elevated temperature
    Du, J
    Liu, YH
    Yu, SR
    Wang, W
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2003, 13 (03) : 636 - 640
  • [42] Shear bands in Fe-3% Si-0.5% Cu alloy
    Lobanov M.L.
    Rusakov G.M.
    Redikul'tsev A.A.
    Karabanalov M.S.
    Lobanova L.V.
    Steel in Translation, 2011, 41 (7) : 559 - 564
  • [43] Al-18%Si合金的温度处理
    坚增运,杨根仓,周尧和
    中国有色金属学报, 1995, (04) : 133 - 135+144
  • [44] Refinement of primary silicon in Al-18%Si alloy under gradient high magnetic field
    Jin Fangwei
    Ren Zhongming
    Ren Weili
    Deng Kang
    Zhong Yunbo
    ACTA METALLURGICA SINICA, 2007, 43 (05) : 521 - 528
  • [45] Aging Behavior of Ultra-Fine Grained Al-0.5%Si-0.5%Ge Alloy Fabricated by ARB Process
    Nakagawa, Keiyu
    Tsuji, Nobuhiro
    Terada, Daisuke
    Nakano, Toshihiko
    Nizam, Khairul
    Kanadani, Teruto
    MATERIALS TRANSACTIONS, 2014, 55 (02) : 249 - 254
  • [46] Adhesive wear of stir cast hypereutectic Al-Si-Mg alloy under reciprocating sliding conditions
    Reddy, T. V. S.
    Dwivedi, D. K.
    Jain, N. K.
    WEAR, 2009, 266 (1-2) : 1 - 5
  • [47] Thermography of the Phase Transformations in a Hypoeutectic Al-7% Si-0.5% Mg Silumin at High Pressures and Temperatures
    Padalko, A. G.
    Belov, N. A.
    Veselov, A. N.
    Talanova, G. V.
    RUSSIAN METALLURGY, 2009, 1 (01): : 65 - 69
  • [48] Dry sliding friction and wear behavior of woodceramics/Al-Si composites
    Xie, XQ
    Fan, TX
    Sun, BH
    Zhang, D
    Sakata, T
    Mori, H
    Okabe, T
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 342 (1-2): : 287 - 293
  • [49] Sliding Wear Behaviour of In Situ TiB2 Reinforced Hypoeutectic Al-Si Alloy Composites
    M. K. Hullur
    Dayanand M. Goudar
    K. Venkateshwaralu
    S. A. Kori
    International Journal of Metalcasting, 2023, 17 : 1179 - 1190
  • [50] Sliding Wear Behaviour of In Situ TiB2 Reinforced Hypoeutectic Al-Si Alloy Composites
    Hullur, M. K.
    Goudar, Dayanand M.
    Venkateshwaralu, K.
    Kori, S. A.
    INTERNATIONAL JOURNAL OF METALCASTING, 2023, 17 (02) : 1179 - 1190