摘要
In present paper, the influence of copper on wear-friction behaviour of hypereutectic Al-Si alloy (Al-18% Si-0.5% Mg) has been investigated. Sliding tests were conducted under dry sliding conditions against hardened steel En-31 counter surface over a range of sliding speed from 2.0 to 7.0 m/s and contact load from 10 to 80 N. It was observed that the wear rate is a function of contact load, sliding speed, composition and thermal softening characteristics of sliding metal. Wear of hypereutectic aluminium-silicon alloy is not appreciably affected with the addition of copper. However, addition of copper increases the transition load at 2.0 m/s sliding speed. Copper addition more than 2%, did not show any effect on the transition load. (C) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:323 / 328
页数:6
相关论文
共 50 条
  • [1] Dry Sliding Friction and Wear Behaviour of an Electron Beam Melted Hypereutectic Al–Si Alloy
    J. C. Walker
    J. Murray
    S. Narania
    A. T. Clare
    Tribology Letters, 2012, 45 : 49 - 58
  • [2] Transition in dry sliding friction and wear behaviour of cast Al-Si base alloy
    Dwivedi, D.K.
    Journal of the Institution of Engineers (India), Part MM: Metallurgy and Material Science Division, 2001, 82 (02): : 69 - 74
  • [3] Dry Sliding Friction and Wear Behaviour of an Electron Beam Melted Hypereutectic Al-Si Alloy
    Walker, J. C.
    Murray, J.
    Narania, S.
    Clare, A. T.
    TRIBOLOGY LETTERS, 2012, 45 (01) : 49 - 58
  • [4] Influence of vibration on the solidification behaviour and tensile properties of an Al-18 wt%Si alloy
    Chirita, G.
    Stefanescu, I.
    Soares, D.
    Silva, F. S.
    MATERIALS & DESIGN, 2009, 30 (05) : 1575 - 1580
  • [5] Superplasticity of the Al-18% Si microcrystalline hypereutectic alloy
    V. N. Chuvil’deev
    M. Yu. Gryaznov
    V. I. Kopylov
    A. N. Sysoev
    Yu. G. Lopatin
    Doklady Physics, 2008, 53
  • [6] Superplasticity of the Al-18% Si microcrystalline hypereutectic alloy
    Chuvil'deev, V. N.
    Gryaznov, M. Yu.
    Kopylov, V. I.
    Sysoev, A. N.
    Lopatin, Yu. G.
    DOKLADY PHYSICS, 2008, 53 (03) : 148 - 151
  • [7] Dry sliding wear behaviour of Al-12Si-4Mg alloy with cerium addition
    Anasyida, A. S.
    Daud, A. R.
    Ghazali, M. J.
    MATERIALS & DESIGN, 2010, 31 (01) : 365 - 374
  • [8] Evolution of microstructure in spray formed Al-18%Si alloy
    Srivastava, VC
    Mandal, RK
    Ojha, SN
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 383 (01): : 14 - 20
  • [9] Influence of contact area on the sliding friction and wear behaviour of an electrochemical jet textured Al-Si alloy
    Walker, J. C.
    Cinti, S.
    Kamps, T. J.
    Mitchell-Smith, J.
    Clare, A. T.
    WEAR, 2019, 426 : 1336 - 1344
  • [10] Sliding temperature and wear behaviour of cast Al-Si-Mg alloys
    Dwivedi, DK
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 382 (1-2): : 328 - 334