Sliding contacts for the pharmaceutical industry: failure analysis and dry sliding tests for the replacement of hard Cr on AISI 316L steel

被引:4
|
作者
Ceschini, L. [1 ,2 ]
Martini, C. [1 ,2 ]
Rotundo, F. [2 ]
机构
[1] Univ Bologna, Dept Ind Engn, I-40136 Bologna, Italy
[2] Univ Bologna, Interdept Ctr Ind Res Adv Mech & Mat CIRI MAM, I-40136 Bologna, Italy
关键词
Sliding; Coating; Friction; Wear; TRIBOLOGICAL PROPERTIES; MECHANICAL-PROPERTIES; TITANIA COATINGS; WEAR BEHAVIOR; FRICTION; PERFORMANCE;
D O I
10.1016/j.triboint.2014.09.004
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Several alternatives were compared for the replacement of hard electroplated Cr coating to improve the tribological properties of the AISI 316L austenitic stainless steel for pharmaceutical packaging applications, including low temperature carburizing (LTC), thermal spray coatings (Al2O3-13TiO(2), WC-17Co), substitution of the AISI 301 reference counterface with polymeric materials (PTFE, UHMWPE, PEEK). In dry sliding block on ring tests, the LTC AISI 316L cylinders lead to the lowest wear rates of the AISI301 sliders under low loads (up to 10 N). When considering the polymer vs. uncoated AISI 316L couple, PEEK and UHMWPE lead to lower friction and comparable wear rates with respect to the reference couple (AISI 301 vs. Hard Cr coated-AISI 316L) in the whole range of tested loads. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:248 / 257
页数:10
相关论文
共 50 条
  • [41] Failure analysis of AISI 316L ball valves by salt bath nitriding
    Luo, Guandong
    Zheng, Zhi
    Ning, Likui
    Tan, Zheng
    Tong, Jian
    Liu, Enze
    ENGINEERING FAILURE ANALYSIS, 2020, 111
  • [42] Analysis of a premature failure of welded AISI 316L stainless steel pipes originated by microbial induced corrosion
    Otero, E
    Bastidas, JM
    Lopez, V
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 1997, 48 (07): : 447 - 454
  • [43] Sliding Wear Characteristics and Corrosion Behaviour of Selective Laser Melted 316L Stainless Steel
    Y. Sun
    A. Moroz
    K. Alrbaey
    Journal of Materials Engineering and Performance, 2014, 23 : 518 - 526
  • [44] A study on wear behavior of γ-UHMWPE sliding against 316L stainless steel counter face
    Raffi, N. Mohamad
    Srinivasan, V.
    WEAR, 2013, 306 (1-2) : 22 - 26
  • [45] Sliding Wear Properties of 316L Stainless Steel Produced by Additive/Subtractive Hybrid Manufacturing
    Tang Chengming
    Zhao Jibin
    Zhao Yuhui
    Wang Zhiguo
    ACTA OPTICA SINICA, 2023, 43 (11)
  • [46] Sliding Wear Characteristics and Corrosion Behaviour of Selective Laser Melted 316L Stainless Steel
    Sun, Y.
    Moroz, A.
    Alrbaey, K.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2014, 23 (02) : 518 - 526
  • [47] On Dry Wear of Metallic Materials in Different Configurations of Sliding Electrical Contacts Against a Quenched AISI 1045 Steel
    M. I. Aleutdinova
    V. V. Fadin
    Russian Physics Journal, 2023, 65 : 1768 - 1774
  • [48] On Dry Wear of Metallic Materials in Different Configurations of Sliding Electrical Contacts Against a Quenched AISI 1045 Steel
    Aleutdinova, M. I.
    Fadin, V. V.
    RUSSIAN PHYSICS JOURNAL, 2023, 65 (10) : 1768 - 1774
  • [49] Influence of duplex USSP/Nitriding surface treatments on the dry sliding behavior of Ti6Al4V/AISI 316L tribopairs
    Maire, L.
    Faure, L.
    Philippon, S.
    Novelli, M.
    Marcos, G.
    Czerwiec, T.
    Grosdidier, T.
    ICSI 2015 THE 1ST INTERNATIONAL CONFERENCE ON STRUCTURAL INTEGRITY FUNCHAL, 2015, 114 : 621 - 626
  • [50] ANALYSIS OF THE WORK HARDENING BEHAVIOUR OF A AISI 316L STAINLESS STEEL AT HIGH TEMPERATURE
    Angella, G.
    METALLURGIA ITALIANA, 2009, (01): : 45 - 50