Low stress abrasive wear response of boron steel under three body abrasion: Effect of heat treatment and peening intensities

被引:0
|
作者
Singh, Dushyant [2 ]
Mondal, D. P. [1 ]
Modi, O. P. [1 ]
Sethi, V. K. [3 ]
机构
[1] CSIR, Adv Mat & Proc Res Inst, Bhopal 462026, India
[2] Cent Inst Agr Engn, Bhopal 462038, India
[3] Rajiv Gandhi Tech Univ, UIT, Bhopal, India
关键词
Heat treatment cycle; Shot peening; Shot peening intensity; Abrasive wear; Boron steel; MICROSTRUCTURE; RESISTANCE;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The wear behaviour of medium carbon boron steel with various heat-treatment cycles (annealing, intercritical annealing, and quenching and tempering) has been examined after and prior to shot peening. Shot peening intensity varies in the range 0.17 - 0.47 mm ALMEN 'A'. The wear rate of intercritical annealed and quenched and tempered steels are considerably less than those of as-received and annealed steels, irrespective of the peening intensity. It is further noted that the wear rate reduced significantly irrespective of heat-treatment schedule at the critical peening intensity of 0.27 A, mm ALMEN.
引用
收藏
页码:208 / 218
页数:11
相关论文
共 50 条
  • [31] Effect of microstructure and mechanical properties on two body abrasive wear resistance of medium-carbon low-alloy steel
    Miao Jun
    Wang Li-jun
    Liu Chun-ming
    ADVANCES IN MECHANICAL ENGINEERING, PTS 1-3, 2011, 52-54 : 1247 - 1252
  • [32] Effect of boron addition on three-body abrasive wear characteristics of high chromium based multi-component white cast iron
    Purba, Riki Hendra
    Shimizu, Kazumichi
    Kusumoto, Kenta
    Gaqi, Yila
    Todaka, Takayuki
    MATERIALS CHEMISTRY AND PHYSICS, 2022, 275
  • [33] Effect of red mud addition on abrasive wear rate of isotactic polypropylene/low density polyethylene blend under low stress conditions
    Chand, N
    Hashmi, SAR
    JOURNAL OF SCIENTIFIC & INDUSTRIAL RESEARCH, 1999, 58 (10): : 795 - 798
  • [34] Two- and three-body abrasive wear behaviour of different heat-treated boron alloyed high chromium cast iron grinding balls
    Izciler, M
    Çelik, H
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2000, 105 (03) : 237 - 245
  • [35] Effect of Dual-stage Ageing and RRA Treatment on the Three-body Abrasive Wear of the AW7075 Alloy
    Lachowicz, Marzena M.
    Lesniewski, Tadeusz
    Lachowicz, Maciej B.
    STROJNISKI VESTNIK-JOURNAL OF MECHANICAL ENGINEERING, 2022, 68 (7-8): : 493 - 505
  • [36] The effects of particle angularity on low-stress three-body abrasion-corrosion of 316L stainless steel
    Stachowiak, Grazyna B.
    Salasi, Mobin
    Rickard, William D. A.
    Stachowiak, Gwidon W.
    CORROSION SCIENCE, 2016, 111 : 690 - 702
  • [37] Effect of nanoscale V2C precipitates on the three-body abrasive wear behavior of high-Mn austenitic steel
    Zhou, Zaifeng
    Shan, Quan
    Jiang, Yehua
    Li, Zulai
    Zhang, ZheXuan
    WEAR, 2019, 436
  • [38] Effect of WC grain size and content on low stress abrasive wear of manual arc welded hardfacings with low-carbon or stainless steel matrix
    Jankauskas, Vytenis
    Antonov, Maksim
    Varnauskas, Valentinas
    Skirkus, Remigijus
    Goljandin, Dmitri
    WEAR, 2015, 328 : 378 - 390
  • [39] Effect of Heat Treatment on Tribological Properties of Ni-B Coatings on Low Carbon Steel: Wear Maps and Wear Mechanisms
    Arias, Sandra
    Castano, Juan G.
    Correa, Esteban
    Echeverria, Felix
    Gomez, Maryory
    JOURNAL OF TRIBOLOGY-TRANSACTIONS OF THE ASME, 2019, 141 (09):
  • [40] Effect of cementation and heat treatment of steel 10G{cyrillic}12 on metastable austenite in the structure, Abrasive and impact wear resistance
    Malinov, L.S.
    Kharlashkin, V.A.
    Metallurgical and Mining Industry, 2011, 3 (02): : 58 - 62