Retardation of thermal degradation of PMMA and PVC by C60

被引:75
|
作者
Troitskii, BB [1 ]
Troitskaya, LS [1 ]
Yakhnov, AS [1 ]
Lopatin, MA [1 ]
Novikova, MA [1 ]
机构
[1] Russian Acad Sci, Razuvaev Inst Organomet Chem, Nizhnii Novgorod, Russia
关键词
D O I
10.1016/S0014-3057(97)00048-7
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Investigations were made on the effects of C-60 upon the rate of depolymerization of PMMA films during the thermal degradation in vacuo at 300 and 332 degrees C by thermogravimetric method and upon the rates of dehydrochlorination of PVC during the thermal degradation in vacuo with continuous and effective removal of HCl and in the presence of volatile products at 200 degrees C. It was shown that C-60 retards the thermal depolymerization of PMMA and the autocatalytic thermal dehydrochlorination of PVC in the presence of HCl and does not decrease the rate of PVC nonautocatalytic degradation with removal of HCl. The suggestion was made that the retarding effect of C-60 is connected with its interaction with macroradicals, which generate in the thermal degradation of PMMA and PVC, with formation of less active compounds. In the case of PVC, there is the probability of interaction of C-60 with chlorine atoms too. (C) 1997 Elsevier Science Ltd.
引用
收藏
页码:1587 / 1590
页数:4
相关论文
共 50 条
  • [21] Surface tracks by MeV C60 impacts on mica and PMMA
    Paul Scherrer Inst, Zurich, Switzerland
    Nucl Instrum Methods Phys Res Sect B, 4 (503-512):
  • [22] Experimental observation of negative group velocity in C60 PMMA
    Wang, Hao
    Zhang, Yundong
    Ma, Lei
    He, Zhusong
    Tian, He
    Wang, Nan
    Yuan, Ping
    OPTIK, 2009, 120 (13): : 673 - 675
  • [23] Surface tracks by MeV C60 impacts on mica and PMMA
    Dobeli, M
    Ames, F
    Musil, CR
    Scandella, L
    Suter, M
    Synal, HA
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 1998, 143 (04): : 503 - 512
  • [24] Optical and structural properties of PMMA/C60 composites with different concentrations of C60 molecules and its possible applications
    I. Stankovic
    Lidija Matija
    M. Jankov
    B. Jeftic
    I. Koruga
    Dj Koruga
    Journal of Polymer Research, 2020, 27
  • [25] Thermal stability of solid C60
    Phys Rev B, 1 (127):
  • [26] Extensive ozonation of C60:: Degradation or polymerization?
    Manning, TJ
    Olsen, K
    Hardin, L
    Purcell, J
    Ayers, TM
    Duncan, MA
    Phillips, D
    OZONE-SCIENCE & ENGINEERING, 2006, 28 (03) : 177 - 180
  • [27] The enhancement of the optical properties of CdS/PMMA by adding fullerence C60
    Maged, Fatma Abdel
    Mansour, A. F.
    PHYSICA SCRIPTA, 2022, 97 (07)
  • [28] Preparation and study of the flame retardant properties of C60/PMMA microspheres
    Xu, Lanjuan
    Jiang, Juncheng
    Ni, Lei
    Chen, Zhiquan
    Li, Chao
    RSC ADVANCES, 2022, 12 (35) : 22623 - 22630
  • [29] Nano-structural studies on C60/PMMA composite films
    Li, YL
    Chen, GH
    Zou, YJ
    Wang, B
    Yan, H
    JOURNAL OF INORGANIC MATERIALS, 2002, 17 (01) : 167 - 171
  • [30] Simulation of the thermal fragmentation of fullerene C60
    L. A. Openov
    A. I. Podlivaev
    JETP Letters, 2006, 84 : 68 - 72