Synthesis, phase transformation and dielectric properties of sol-gel derived Bi2Ti2O7 ceramics

被引:78
|
作者
Su, WF [1 ]
Lu, YT [1 ]
机构
[1] Natl Taiwan Univ, Dept Mat Sci & Engn, Taipei, Taiwan
关键词
sol-gel; Bi2Ti2O7; ferroelectricity; metal alkoxides;
D O I
10.1016/S0254-0584(03)00089-0
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Sol-gel derived Bi2Ti2O7 ceramic powders have been prepared from methoxyethoxides of bismuth and titanium (molar ratio of Ti/Bi = 1.23 and water/alkoxides = 1.31). The Bi2Ti2O7 phase was stable at a low temperature (700 degreesC), but it then transformed into mixed phases of Bi4Ti3O12 and B2Ti4O11 at 850-1150 degreesC. The single phase of Bi2Ti2O7 reoccurred at 1200 degreesC. Dielectric properties and ferroelectric behavior of samples sintered at 1150 and 1200 degreesC were examined. Under frequency of 1 MHz, samples sintered at 1150 and 1200 degreesC had a dielectric constant of 101.3 and 104.2, and a loss tangent of 0.0193 and 0.0145, respectively. Only the sample sintered at 1150 degreesC showed ferroelectric behavior, where remanent polarization is 3.77 muC cm(-2) and coercive field is 24kV cm(-1). Thus, the Bi2Ti2O7 did not exhibit ferroelectricity, but the mixed phase of Bi4Ti3O12 and Bi2Ti4O11 did. (C) 2003 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:632 / 637
页数:6
相关论文
共 50 条
  • [21] Dielectric properties of Bi2Ti2O7 films grown on Si(100) substrate by APMOCVD
    Wang, H
    Shang, SX
    Yao, WF
    Hou, Y
    Xu, XH
    Wang, D
    Wang, M
    Yu, JZ
    FERROELECTRICS, 2002, 271 : 1707 - 1713
  • [22] Structure and properties of Bi2Ti2O7 pyrochlore type phase stabilized by lithium
    Lelievre, Jerome
    Marchet, Pascal
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 732 : 178 - 186
  • [23] Structure and properties of Bi2Ti2O7 pyrochlore type phase stabilized by lithium
    Marchet, Pascal (pascal.marchet@unilim.fr), 1600, Elsevier Ltd (732):
  • [24] Dielectric and ferroelectric properties of nanocrystalline Bi2Ti2O7 prepared by a metallorganic decomposition method
    Hou, Y
    Wang, M
    Xu, XH
    Wang, D
    Wang, H
    Shang, SX
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2002, 85 (12) : 3087 - 3089
  • [25] Synthesis, dielectric properties of Bi2/3Cu3Ti4O12 ceramics by the sol–gel method
    Zhao Yang
    Pengfei Liang
    Longhai Yang
    Pinging Shi
    Xiaolian Chao
    Zupei Yang
    Journal of Materials Science: Materials in Electronics, 2015, 26 : 1959 - 1968
  • [26] GRAIN-ORIENTATION IN SOL-GEL DERIVED LN2TI2O7 CERAMICS (LN = LA, ND)
    PRASADARAO, AV
    SELVARAJ, U
    KOMARNENI, S
    BHALLA, AS
    MATERIALS LETTERS, 1991, 12 (05) : 306 - 310
  • [27] Phase Characterization and Dielectric Properties of Zn2SiO4 Ceramics Derived from a Sol-Gel Process
    Yue, Zhenxing
    Dong, Mingzhi
    Meng, Siqin
    Li, Longtu
    FERROELECTRICS, 2009, 387 : 184 - 188
  • [28] Synthesis and thermal decomposition of bismuth peroxotitanate to Bi2Ti2O7
    V Parvanova
    Journal of Thermal Analysis and Calorimetry, 2006, 86 : 443 - 447
  • [29] Synthesis of La2Ti2O7 Nanoscale Powder and Ceramics Based on It by Sol-Gel Synthesis and Spark Plasma Sintering
    Shichalin, O. O.
    Papynov, E. K.
    Belov, A. A.
    Pervakov, K. A.
    Gribanova, S. S.
    Pisarev, S. M.
    Fedorets, A. N.
    Pogodaev, A. V.
    Lembikov, A. O.
    Zernov, Ya. G.
    Marmaza, P. A.
    Kapustina, O. V.
    Gridasova, E. A.
    Buravlev, I. Yu.
    RUSSIAN JOURNAL OF INORGANIC CHEMISTRY, 2024, 69 (04) : 617 - 623
  • [30] Synthesis and thermal decomposition of bismuth peroxotitanate to Bi2Ti2O7
    Parvanova, V.
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2006, 86 (02) : 443 - 447