Experimental programs were carried out tl, study compressive strength and microstructure of high performance concrete (HPC) subjected to high temperature compared with normal strength concrete (NSC). After the concrete specimens were exposed to a peak temperature of 800 degrees C, the compressive strength was tested. Changes of porosity and pore size distribution of the concrete were measured by using mercury intrusion porosimetry (MIP). Test results show that high performance concrete had higher residual strength although the strength of high performance concrete degenerated much more than the normal strength concrete after high temperature exposed. Variations in pore structure of high performance concrete after high temperature indicated the degradation of the mechanical properties. A model by optimizing the parameters ill Ryshkewitch model was developed to predict the relationship between porosity and compressive strength of the high performance concrete.
引用
下载
收藏
页码:294 / 298
页数:5
相关论文
共 50 条
  • [31] Dynamic Compressive Performance of Concrete Exposed to High Temperature Based on Microstructure Analysis
    Yang, Shao-wei
    Liu, Zhi-guo
    Wang, Yong-wei
    Liu, Zi-rui
    Ba, Heng-jing
    ARCHITECTURE, BUILDING MATERIALS AND ENGINEERING MANAGEMENT, PTS 1-4, 2013, 357-360 : 1389 - +
  • [32] Effect of high temperature and cooling regimes on the compressive strength and pore properties of high performance concrete
    Chan, SYN
    Luo, X
    Sun, W
    CONSTRUCTION AND BUILDING MATERIALS, 2000, 14 (05) : 261 - 266
  • [33] Residual properties of high-strength fiber reinforced concrete after exposure to high temperatures
    Tang, Chao-Wei
    COMPUTERS AND CONCRETE, 2019, 24 (01): : 63 - 71
  • [34] The effects of low temperature curing on the compressive strength of ordinary and high performance concrete
    Husem, M
    Gozutok, S
    CONSTRUCTION AND BUILDING MATERIALS, 2005, 19 (01) : 49 - 53
  • [35] Residual strength of Super High Strength Concrete Used Stone-chip after exposure to high temperatures
    Chen, Guocan
    Xu, Zhisheng
    Tang, Weihong
    SUSTAINABLE DEVELOPMENT OF URBAN ENVIRONMENT AND BUILDING MATERIAL, PTS 1-4, 2012, 374-377 : 2456 - +
  • [36] Residual strength of hybrid-fiber-reinforced high-strength concrete after exposure to high temperatures
    Bing, C
    Liu, JY
    CEMENT AND CONCRETE RESEARCH, 2004, 34 (06) : 1065 - 1069
  • [37] Application of artificial neural network in the prediction of compressive strength of long standing concrete after exposure to high temperature
    Lu, Tian-Qi
    Zhao, Guo-Fan
    Lin, Zhi-Shen
    Gongcheng Lixue/Engineering Mechanics, 2003, 20 (06): : 52 - 57
  • [38] Compressive strength of fiber reinforced concrete with slag powder after high temperature
    Gao D.-Y.
    Yang S.-H.
    Zhao J.
    Jianzhu Cailiao Xuebao/Journal of Building Materials, 2010, 13 (06): : 711 - 715
  • [39] Effect of high temperature curing on compressive strength of concrete
    School of Materials Science and Engineering, Southwest University of Science and Technology, Mianyang 621010, China
    Jianzhu Cailiao Xuebao, 2006, 4 (473-476):
  • [40] Compressive Strength of Self-Compacting Concrete during High-Temperature Exposure
    Tao, Jin
    Yuan, Yong
    Taerwe, Luc
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2010, 22 (10) : 1005 - 1011