A metal/Al2O3/ZrO2/SiO2/Si (MAZOS) structure for high-performance non-volatile memory application

被引:25
|
作者
Liu, Jing [1 ]
Wang, Qin [1 ]
Long, Shibing [1 ]
Zhang, Manhong [1 ]
Liu, Ming [1 ]
机构
[1] Chinese Acad Sci, Lab Nanofabricat & Novel Devices Integrated Techn, Inst Microelect, Beijing 100029, Peoples R China
基金
中国国家自然科学基金;
关键词
FLOATING-GATE;
D O I
10.1088/0268-1242/25/5/055013
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
In this paper, we report a metal/Al2O3/ZrO2/SiO2/Si (MAZOS) structure with a ZrO2 charge-trapping layer for non-volatile memory application. The superiority of this device over the traditional metal/Al2O3/Si3N4/SiO2/Si (MANOS) devices is much better data retention and enhanced program/erase efficiency. The MAZOS device exhibits excellent memory characteristics, including a large memory window of 7.1 V under +/- 11 V capacitance-voltage sweep, and a greatly improved data retention (only 16% charge loss for 10 years time) along with good endurance. The MAZOS device has a strong potential for future high-performance non-volatile memory application.
引用
收藏
页数:4
相关论文
共 50 条
  • [31] Performance improvement for Metal/Al2O3/HfO2/SiO2/Si structure nonvolatile flash memory by fluorine plasma treatment
    Wang, Chen-Jie
    Huo, Zong-Liang
    Liu, Ming
    2012 IEEE 11TH INTERNATIONAL CONFERENCE ON SOLID-STATE AND INTEGRATED CIRCUIT TECHNOLOGY (ICSICT-2012), 2012, : 775 - 777
  • [32] Electronic energy loss of swift protons in the oxides Al2O3, SiO2 and ZrO2
    Abril, I
    Garcia-Molina, R
    Arista, NR
    Sanz-Navarro, CF
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2002, 190 : 89 - 94
  • [33] FRICTION AND WEAR OF AL2O3, ZRO2 AND SIO2 RUBBED AGAINST PURE METALS
    HIRATSUKA, K
    ENOMOTO, A
    SASADA, T
    WEAR, 1992, 153 (02) : 361 - 373
  • [34] SOL-GEL PREPARATION OF SIO2 GLASSES CONTAINING AL2O3 OR ZRO2
    NOGAMI, M
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 1994, 178 (pt 2) : 320 - 326
  • [35] Concept of Inclusion Capacity of Slag and Its Application on the Dissolution of Al2O3, ZrO2 and SiO2 Inclusions in CaO-Al2O3-SiO2 Slag
    Gou, Lan
    Liu, Hong
    Ren, Ying
    Zhang, Lifeng
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2023, 54 (03): : 1314 - 1325
  • [36] Heat-Insulating Properties of High-Alumina Materials Filament-Reinforced with Glass Fiber of the Al2O3–SiO2 and Al2O3–SiO2–ZrO2 Systems
    R. V. Zubashchenko
    Refractories and Industrial Ceramics, 2019, 59 : 552 - 554
  • [37] Porous Nanocomposites 2: Pore-Structure Stability of Pure ZrO2, ZrO2(matrix)-Al2O3 and Al2O3(matrix)-ZrO2 Nanocomposites
    Padmakumar Nair
    Jalajakumari Nair
    E.B.M. Doesburg
    J.G. van Ommen
    J.R.H. Ross
    A.J. Burggraaf
    Y. Oosawa
    F. Mizukami
    Journal of Porous Materials, 1999, 6 : 69 - 76
  • [38] Porous nanocomposites 2:: Pore-structure stability of pure ZrO2, ZrO2(matrix)-Al2O3 and Al2O3(matrix)-ZrO2 nanocomposites
    Nair, P
    Nair, J
    Doesburg, EBM
    Van Ommen, JG
    Ross, JRH
    Burggraaf, AJ
    Oosawa, Y
    Mizukami, F
    JOURNAL OF POROUS MATERIALS, 1999, 6 (01) : 69 - 76
  • [39] STRUCTURE OF INCOHERENT ZRO2/AL2O3 INTERFACES
    KRAUSLANTERI, SP
    MITCHELL, TE
    HEUER, AH
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1986, 69 (03) : 256 - 258