Fretting wear of micro-arc oxidation coating prepared on Ti6Al4V alloy

被引:46
|
作者
Lin Xiu-zhou [1 ,2 ]
Zhu Min-hao [1 ]
Zheng Jian-feng [1 ]
Luo Jun [1 ]
Mo Ji-liang [1 ]
机构
[1] SW Jiaotong Univ, Tribol Res Inst, Tract Power State Key Lab, Chengdu 610031, Peoples R China
[2] Sichuan Univ Sci & Engn, Sichuan Prov Key Lab Corros & Protect Mat, Zigong 643000, Peoples R China
基金
中国国家自然科学基金;
关键词
titanium alloy; micro-arc oxidation; friction and wear; fretting wear; PLASMA ELECTROLYTIC OXIDATION; CERAMIC COATINGS; TI-6AL-4V ALLOY; TITANIUM-ALLOY; TRIBOLOGICAL BEHAVIOR; MICROSTRUCTURE; LUBRICATION; STEEL; OXIDE;
D O I
10.1016/S1003-6326(09)60175-8
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Micro-arc oxidation (MAO) coating was prepared on Ti6Al4V alloy surface and its characterizations were detected by Vickers hardness tester, profilometer, scanning electric microscope (SEM), energy dispersive X-ray spectrometer (EDX) and X-ray diffractometer (XRD). Fretting wear behaviors of the coating and its substrate were comparatively tested without lubrication under varied displacement amplitudes (D) in a range of 3-40 mu m, constant normal load (F-n) of 300 N and frequency of 5 Hz. The results showed that the MAO coating, presenting rough and porous surface and high hardness, mainly consisted of rutile and anatase TiO2 phases. Compared with the substrate, the MAO coating could shift the mixed fretting regime (MFR) and slip regime (SR) to a direction of smaller displacement amplitude. In the partial slip regime (PSR), lower friction coefficients and slight damage appeared due to the coordination of elastic deformation of contact zones. In the MFR, the friction coefficient of the coating was lower than that of the substrate as a result of the prevention of plastic deformation by the hard ceramic surface. With the increase of the displacement amplitude, the degradation of the MAO coating and the substrate increased extremely. The fretting wear mechanisms of the coating were abrasive wear and delamination with some material transfer of specimen. In addition, the coating presented a better property for alleviating fretting wear.
引用
收藏
页码:537 / 546
页数:10
相关论文
共 50 条
  • [21] Micro-arc oxidation of Ti6Al4V and Ti6Al7Nb alloys for biomedical applications
    Cimenoglu, Huseyin
    Gunyuz, Mert
    Kose, Gamze Torun
    Baydogan, Murat
    Ugurlu, Faysal
    Sener, Cem
    MATERIALS CHARACTERIZATION, 2011, 62 (03) : 304 - 311
  • [22] Biocompatibility of micro-arc oxidation coatings developed on Ti6Al4V alloy in a solution containing organic phosphate
    Zhang, R. F.
    Qiao, L. P.
    Qu, B.
    Zhang, S. F.
    Chang, W. H.
    Xiang, J. H.
    MATERIALS LETTERS, 2015, 153 : 77 - 80
  • [23] The effect of Micro-arc Oxidation treatment on the microstructure and properties of open cell Ti6Al4V alloy foams
    Korkmaz, Kemal
    SURFACE & COATINGS TECHNOLOGY, 2015, 272 : 72 - 78
  • [24] Effects of TaC microparticles on structure and properties of micro-arc oxidation coating on Ti-6Al-4V alloy
    Ding Zhi-Song
    Gao Wei
    Wei Jing-Peng
    Jin Yao-Hua
    Zhao Chen
    Yang Wei
    ACTA PHYSICA SINICA, 2022, 71 (02)
  • [25] Influence of thermal oxidation duration on the microstructure and fretting wear behavior of Ti6Al4V alloy
    Wang, Song
    Liao, Zhenhua
    Liu, Yuhong
    Liu, Weiqiang
    MATERIALS CHEMISTRY AND PHYSICS, 2015, 159 : 139 - 151
  • [26] Antifouling property of micro-arc oxidation coating incorporating Cu2O nanoparticles on Ti6Al4V
    Zhao, Dan
    Lu, Yuhui
    Zeng, Xing
    Wang, Zhong
    Liu, Shaogang
    Wang, Tao
    SURFACE ENGINEERING, 2017, 33 (10) : 796 - 802
  • [27] Effects of Li2SO4 Content in the Electrolyte on Characteristics of Coating on Ti6Al4V by Micro-Arc Oxidation
    Zhang Yaping
    Liu Xiangdong
    Lue Kai
    Wu Di
    Nan Hai
    RARE METAL MATERIALS AND ENGINEERING, 2010, 39 (05) : 809 - 813
  • [28] Effect of Micro-arc Oxidation on the Mechanical Properties of Hierarchical Porous Ti6Al4V Prepared by Selective Laser Melting
    Yihou, Xiang
    Liwei, Tang
    Jinghui, Wang
    Guolong, Wu
    Qunli, Zhang
    Jianhua, Yao
    Surface Technology, 2024, 53 (13): : 84 - 95
  • [29] Characteristics of the Molten Pool Temperature Field and Its Influence on the Preparation of a Composite Coating on a Ti6Al4V Alloy in the Micro-Arc Oxidation Process
    Li, Xinyi
    Dong, Chaofang
    Zhao, Qing
    Cheng, Fasong
    MATERIALS, 2020, 13 (02)
  • [30] Fretting wear behaviors of micro-arc oxidation coating sealed by grease
    Zhu, M. H.
    Cai, Z. B.
    Lin, X. Z.
    Zheng, J. F.
    Luo, J.
    Zhou, Z. R.
    WEAR, 2009, 267 (1-4) : 299 - 307