Fretting wear of micro-arc oxidation coating prepared on Ti6Al4V alloy

被引:46
|
作者
Lin Xiu-zhou [1 ,2 ]
Zhu Min-hao [1 ]
Zheng Jian-feng [1 ]
Luo Jun [1 ]
Mo Ji-liang [1 ]
机构
[1] SW Jiaotong Univ, Tribol Res Inst, Tract Power State Key Lab, Chengdu 610031, Peoples R China
[2] Sichuan Univ Sci & Engn, Sichuan Prov Key Lab Corros & Protect Mat, Zigong 643000, Peoples R China
基金
中国国家自然科学基金;
关键词
titanium alloy; micro-arc oxidation; friction and wear; fretting wear; PLASMA ELECTROLYTIC OXIDATION; CERAMIC COATINGS; TI-6AL-4V ALLOY; TITANIUM-ALLOY; TRIBOLOGICAL BEHAVIOR; MICROSTRUCTURE; LUBRICATION; STEEL; OXIDE;
D O I
10.1016/S1003-6326(09)60175-8
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Micro-arc oxidation (MAO) coating was prepared on Ti6Al4V alloy surface and its characterizations were detected by Vickers hardness tester, profilometer, scanning electric microscope (SEM), energy dispersive X-ray spectrometer (EDX) and X-ray diffractometer (XRD). Fretting wear behaviors of the coating and its substrate were comparatively tested without lubrication under varied displacement amplitudes (D) in a range of 3-40 mu m, constant normal load (F-n) of 300 N and frequency of 5 Hz. The results showed that the MAO coating, presenting rough and porous surface and high hardness, mainly consisted of rutile and anatase TiO2 phases. Compared with the substrate, the MAO coating could shift the mixed fretting regime (MFR) and slip regime (SR) to a direction of smaller displacement amplitude. In the partial slip regime (PSR), lower friction coefficients and slight damage appeared due to the coordination of elastic deformation of contact zones. In the MFR, the friction coefficient of the coating was lower than that of the substrate as a result of the prevention of plastic deformation by the hard ceramic surface. With the increase of the displacement amplitude, the degradation of the MAO coating and the substrate increased extremely. The fretting wear mechanisms of the coating were abrasive wear and delamination with some material transfer of specimen. In addition, the coating presented a better property for alleviating fretting wear.
引用
收藏
页码:537 / 546
页数:10
相关论文
共 50 条
  • [1] Fretting wear of micro-arc oxidation coating prepared on Ti6Al4V alloy
    林修洲
    朱旻昊
    郑健峰
    罗军
    莫继良
    Transactions of Nonferrous Metals Society of China, 2010, 20 (04) : 537 - 546
  • [2] Growth characteristics of scanning micro-arc oxidation coating on Ti6Al4V alloy
    Wang, Ye
    Shen, Jie
    Wu, Guolong
    Yao, Jianhua
    SURFACE ENGINEERING, 2023, 39 (02) : 218 - 228
  • [3] Microstructure and Tribological Performance of Micro-Arc Oxidation Coating on Ti6Al4V Alloy
    Zhang Chao
    Wei Nan
    Kong Dejun
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2023, 76 (04) : 961 - 967
  • [4] Microstructure and Tribological Performance of Micro-Arc Oxidation Coating on Ti6Al4V Alloy
    Zhang Chao
    Wei Nan
    Kong Dejun
    Transactions of the Indian Institute of Metals, 2023, 76 : 961 - 967
  • [5] Investigation on biocompatibility of micro-arc oxidation Ti6Al4V alloy
    Liu, Zhongde
    Luo, Rui
    Cheng, Xiaonong
    Zhou, Xinghua
    Zhang, Yingtao
    Yan, Feixiang
    Cailiao Yanjiu Xuebao/Chinese Journal of Materials Research, 2013, 27 (04): : 355 - 359
  • [6] Fretting wear behaviour of ceramic coating prepared by micro-arc oxidation on Al-Si alloy
    Zhu, M. H.
    Cai, Z. B.
    Lin, X. Z.
    Ren, P. D.
    Tan, J.
    Zhou, Z. R.
    WEAR, 2007, 263 (472-480) : 472 - 480
  • [7] Corrosion and wear properties of micro-arc oxidation treated Ti6Al4V alloy prepared by selective electron beam melting
    Yang, Xin
    Wang, Wan-lin
    Ma, Wen-jun
    Wang, Yan
    Yang, Jun-gang
    Liu, Shi-feng
    Tang, Hui-ping
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2020, 30 (08) : 2132 - 2142
  • [8] Fretting Wear Behavior of Ceramic Coating Prepared by Micro-arc Oxidation on TC4 Alloy
    Li Kang
    Fu Xuesong
    Hu Jianjun
    Zhou Wenlong
    RARE METAL MATERIALS AND ENGINEERING, 2017, 46 (03) : 765 - 769
  • [9] Effects of oxidation time on micro-arc oxidation coatings formed on Ti6Al4V alloy
    Liu Z.
    Sun M.
    Fu H.
    Zhang Z.
    Xiang Z.
    Jiangsu Daxue Xuebao (Ziran Kexue Ban) / Journal of Jiangsu University (Natural Science Edition), 2010, 31 (02): : 160 - 164
  • [10] The biocompatibility of hydroxyapatite film deposition on micro-arc oxidation Ti6Al4V alloy
    Luo, Rui
    Liu, Zhongde
    Yan, Feixiang
    Kong, Yang
    Zhang, Yingtao
    APPLIED SURFACE SCIENCE, 2013, 266 : 57 - 61