TAILORING SP2/SP3 RATIO IN DIAMOND-LIKE CARBON FILMS VIA DEPOSITION PARAMETERS IN A HIGH VOLTAGE ANODIC VACUUM PLASMA

被引:0
|
作者
Badulescu, M. [1 ]
Anghel, A. [1 ]
Surdu-Bob, C. C. [1 ]
Logofatu, C. [2 ]
Luculescu, C. [1 ]
机构
[1] Natl Inst Lasers Plasma & Radiat Phys, POB MG 36, Bucharest 77125, Romania
[2] Natl Inst Mat Phys, POB MG 7, Bucharest 77125, Romania
关键词
diamond-like carbon thin films; Raman spectra; XPS spectra; sp(2)/sp(3) ratio; RAMAN-SPECTRA; SP(3) CONTENT; DLC FILMS; SP(2)/SP(3) RATIO; COATINGS; PHOTOEMISSION;
D O I
暂无
中图分类号
O4 [物理学];
学科分类号
0702 ;
摘要
Tailoring sp(2)/sp(3) ratio in diamond-like carbon thin films offers new surface engineering solutions for the continuously increasing devices requirements in various fields. We report here the control of sp(2)/sp(3) carbon content using the high voltage anodic plasma in vacuum. Correlation of data obtained by visible Raman Spectroscopy and XPS spectra of our DLC films with deposition parameters showed an increase in sp(3) bonding of about 10% when decreasing the discharge voltage from 600 V to 200 V or increasing the anode-substrate distance from 15 cm to 36 cm.
引用
收藏
页数:14
相关论文
共 50 条
  • [1] Chemical kinetics simulation of deposition and sp2/sp3 bond ratio of diamond-like carbon film in plasma
    Shokri, Babak
    Maziar, S. Yaghmaee
    Sarani, Abdollah
    Niknam, Ali Reza
    VACUUM, 2009, 83 : S140 - S144
  • [2] A NEW METHOD FOR EVALUATION OF SP3/SP2 RATIO IN DIAMOND-LIKE FILMS FROM OPTICAL MEASUREMENTS
    DEMICHELIS, F
    PIRRI, CF
    TAGLIAFERRO, A
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 1991, 137 : 839 - 842
  • [3] Effects of sp2/sp3 bonding ratios on field emission properties of diamond-like carbon films grown by microwave plasma chemical vapor deposition
    Umehara, Y
    Murai, S
    Koide, Y
    Murakami, M
    DIAMOND AND RELATED MATERIALS, 2002, 11 (07) : 1429 - 1435
  • [4] Blood compatibility and sp3/sp2 contents of diamond-like carbon (DLC) synthesized by plasma immersion ion implantation-deposition
    Chen, JY
    Wang, LP
    Fu, KY
    Huang, N
    Leng, Y
    Leng, YX
    Yang, P
    Wang, J
    Wan, GJ
    Sun, H
    Tian, XB
    Chu, PK
    SURFACE & COATINGS TECHNOLOGY, 2002, 156 (1-3): : 289 - 294
  • [5] On the determination of the sp(3) to sp(2) ratio in diamond-like carbon thin films
    Mahajan, SS
    Barshilia, HC
    Mehta, BR
    Vankar, VD
    THIN SOLID FILMS, 1997, 302 (1-2) : 250 - 255
  • [6] Tailoring mechanical properties and wettability of nanocrystalline diamond films by control of sp2/sp3 bonding ratio
    Park, Jong Cheon
    Jeong, Ok Geun
    Hwang, Sungu
    Lee, Hee Soo
    Kim, Tae Gyu
    Kim, Jin Kon
    Cho, Hyun
    JOURNAL OF CERAMIC PROCESSING RESEARCH, 2014, 15 (06): : 549 - 554
  • [7] Control over the sp2/sp3 ratio by tuning plasma parameters of the Thermoionic Vacuum Arc
    Surdu-Bob, C.
    Vladoiu, R.
    Badulescu, M.
    Musa, G.
    DIAMOND AND RELATED MATERIALS, 2008, 17 (7-10) : 1625 - 1628
  • [8] Relationship between tribological properties and sp3/sp2 structure of nitrogenated diamond-like carbon deposited by plasma CVD
    Yamamoto, Shuji
    Kawana, Atsuo
    Ichimura, Hiroshi
    Masuda, Chitoshi
    SURFACE & COATINGS TECHNOLOGY, 2012, 210 : 1 - 9
  • [9] EVALUATION OF THE [C(SP3)]/[C(SP2)] RATIO IN DIAMOND-LIKE FILMS THROUGH THE USE OF A COMPLEX DIELECTRIC-CONSTANT
    DEMICHELIS, F
    PIRRI, CF
    TAGLIAFERRO, A
    PHYSICAL REVIEW B, 1992, 45 (24) : 14364 - 14370
  • [10] Effect of sp3/sp2 Ratio on Boron Doped Diamond Films for Producing Persulfate
    de Paiva Barreto, Jessica Pires
    de Freitas Araujo, Karla C.
    de Araujo, Danyelle Medeiros
    Martinez-Huitle, Carlos A.
    ECS ELECTROCHEMISTRY LETTERS, 2015, 4 (12) : E9 - E11