Aqueous Corrosion Characteristics of Iron Aluminides

被引:1
|
作者
Yoo, Yun Ha [1 ]
Kim, Jung Gu [1 ]
机构
[1] Sungkyunkwan Univ, Dept Adv Mat Engn, Suwon 440746, South Korea
来源
关键词
Iron aluminide; Corrosion; Pitting; Crevice; Molybdenum;
D O I
10.4028/www.scientific.net/AMR.26-28.23
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Aqueous corrosion behaviors of Fe3Al-based iron aluminides were investigated. From the result of cyclic anodic polarization tests conducted in 3.5 wt.% NaCl solution at 25, 48, 72 and 95 degrees C, as the temperature increased, the resistance to pitting corrosion decreased significantly, especially over the range of 25 similar to 48 degrees C. From the result of crevice corrosion tests, no crevice corrosion occurred on FAL-Mo in the lower chloride-containing solution (200 ppm Cl-), however, FAL-Mo did not perform as well as the 304L SS in the higher chloride-containing solution (3.5 wt.% NaCl). From the result of anodic polarization tests performed in sulfur-compound solutions, additions of Cr and Mo to the Fe3Al-based iron aluminides tend to improve the aqueous corrosion resistance. Aqueous corrosion behaviors with different Al content evaluated by cyclic anodic polarization test in the chloride-containing solution exhibited the more stable passive behavior and the higher pitting resistance as Al contents increased.
引用
收藏
页码:23 / +
页数:5
相关论文
共 50 条
  • [41] Some effects of aqueous silica on the corrosion of iron
    Rushing, JC
    McNeill, LS
    Edwards, M
    WATER RESEARCH, 2003, 37 (05) : 1080 - 1090
  • [42] DUCTILITY IMPROVEMENT IN IRON ALUMINIDES
    BAHADUR, A
    KUMAR, BR
    MOHANTY, ON
    JOURNAL OF MATERIALS SCIENCE, 1995, 30 (14) : 3690 - 3696
  • [43] The strength properties of iron aluminides
    Yoshimi, K
    Hanada, S
    JOM-JOURNAL OF THE MINERALS METALS & MATERIALS SOCIETY, 1997, 49 (08): : 46 - 49
  • [44] Electrical properties of iron aluminides
    Lilly, AC
    Deevi, SC
    Gibbs, ZP
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 258 (1-2): : 42 - 49
  • [45] Commercialization of nickel and iron aluminides
    Sikka, VK
    INTERNATIONAL SYMPOSIUM ON NICKEL AND IRON ALUMINIDES: PROCESSING, PROPERTIES, AND APPLICATIONS, 1997, : 361 - 375
  • [46] Environmental effects in iron aluminides
    Balasubramaniam, R
    BULLETIN OF MATERIALS SCIENCE, 1999, 22 (03) : 571 - 579
  • [47] Hot salt corrosion of titanium aluminides
    Nicholls, JR
    Leggett, J
    Andrews, P
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 1997, 48 (01): : 56 - 64
  • [48] The strength properties of iron aluminides
    Kyosuke Yoshimi
    Shuji Hanada
    JOM, 1997, 49 : 46 - 49
  • [49] Hot corrosion of carbon-alloyed Fe3Al-based iron aluminides
    Das, D
    Balasubramaniam, R
    Mungole, MN
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 338 (1-2): : 24 - 32
  • [50] Environmental effects in iron aluminides
    R Balasubramaniam
    Bulletin of Materials Science, 1999, 22 : 571 - 579