Titanium oxide films produced on commercially pure titanium by anodic oxidation with different voltages

被引:203
|
作者
Kuromoto, Neide K.
Simao, Renata A.
Soares, Gloria A.
机构
[1] Univ Fed Rio de Janeiro, PEMM, BR-21941972 Rio De Janeiro, Brazil
[2] Univ Fed Parana, Dept Fis, Ctr Politecn, BR-81531990 Curitiba, Parana, Brazil
关键词
titanium; anodic oxidation; titanium oxide film; phosphoric acid;
D O I
10.1016/j.matchar.2006.03.020
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Titanium oxide films produced on commercially pure Ti by anodic oxidation with different voltages were analyzed. Anodic oxidation was carried out at room temperature using 1.4 M H3PO4 electrolyte and a platinum counter-electrode, in potentiostatic mode under the following conditions: 50 V, 100 V, 150 V, 200 V and 250 V It was observed that porous titanium layers were formed at all voltage values but morphological differences were observed. Initially, the film was thin but with increasing voltage it broke down locally and porous regions became evident due to the dielectric breakdown. The porosity and the pore size increased with the increasing voltage. The surface morphology in samples formed with 200 V had substantially different porous structures than those formed with other voltage values. The anodic film surface displayed pores and craters formed on the relatively flat ground oxide surface. AFM images showed that higher voltages produced thicker titanium oxide films. (c) 2006 Elsevier Inc. All rights reserved.
引用
收藏
页码:114 / 121
页数:8
相关论文
共 50 条
  • [31] Superplasticity in commercially pure titanium
    Zhu, XJ
    Tan, MJ
    Zhou, W
    PROCEEDINGS OF THE 1ST INTERNATIONAL CONFERENCE ON NEW FORMING TECHNOLOGY, 2004, : 683 - 688
  • [32] HIGH-TEMPERATURE OXIDATION OF COMMERCIALLY PURE TITANIUM IN THE AIR
    TAKAYAMA, I
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (13): : 1639 - 1639
  • [33] Enhancement of pure titanium localized corrosion resistance by anodic oxidation
    Prando, Davide
    Brenna, Andrea
    Pedeferri, MariaPia
    Ormellese, Marco
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2018, 69 (04): : 503 - 509
  • [34] Fabrication of titanium oxide nanotube arrays by anodic oxidation
    Zhao, JL
    Wang, XH
    Chen, RZ
    Li, LT
    SOLID STATE COMMUNICATIONS, 2005, 134 (10) : 705 - 710
  • [35] Titanium oxide nanotube arrays prepared by anodic oxidation
    Gong, D
    Grimes, CA
    Varghese, OK
    Hu, WC
    Singh, RS
    Chen, Z
    Dickey, EC
    JOURNAL OF MATERIALS RESEARCH, 2001, 16 (12) : 3331 - 3334
  • [36] Titanium oxide nanotube arrays prepared by anodic oxidation
    Dawei Gong
    Craig A. Grimes
    Oomman K. Varghese
    Wenchong Hu
    R. S. Singh
    Zhi Chen
    Elizabeth C. Dickey
    Journal of Materials Research, 2001, 16 : 3331 - 3334
  • [37] Preparation and battery performance of titanium oxide nanotube arrays films by anodic oxidation method
    Wang, Yan-Xiang
    Li, Hai-Chao
    Fan, Xue-Yun
    Yang, Zhi-Sheng
    Huang, Li-Qun
    Sun, Jian
    Rengong Jingti Xuebao/Journal of Synthetic Crystals, 2014, 43 (08): : 1975 - 1980
  • [38] FORMATION OF COLORED OXIDE-FILMS ON TITANIUM-ALLOYS BY ANODIC-OXIDATION
    PEKSHEVA, NP
    JOURNAL OF APPLIED CHEMISTRY OF THE USSR, 1980, 53 (06): : 1016 - 1018
  • [39] STUDY OF POROUS LAYERS FORMED BY ANODIC-OXIDATION OF TITANIUM AT HIGH VOLTAGES
    MARCHENOIR, JC
    LOUP, JP
    MASSON, J
    THIN SOLID FILMS, 1980, 66 (03) : 357 - 369
  • [40] Macroscopic Studies on the Properties of the Anodic Oxide Films on Titanium
    G.A.EL-Mahdy (Chemistry Dept.
    Journal of Materials Science & Technology, 1998, (03) : 241 - 246