Interfacial fracture of vitrified corundum (α-Al2O3)

被引:0
|
作者
Jackson, MJ [1 ]
Mills, B [1 ]
机构
[1] Univ Cambridge, Cavendish Lab, Cambridge CB3 0HE, England
关键词
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The study of bonding hard materials such as corundum (alumina) and the nature of interfacial cohesion between corundum and. glass is very important from a cuffing tool manufacturer's viewpoint. Vitrified grinding wheels are used to remove large volumes of metal and to produce components with very high tolerances. It is expected that the same grinding wheel be used for both rough and finish machining operations. Therefore, the grinding wheel, and in particular its bonding system, is expected to react differently to a variety of machining operations. In order to maintain the integrity of the grinding wheel, the bonding system that is used to hold abrasive grains in place will react differently to forces that are placed on individual bonding bridges. This paper examines the role of vitrification heat treatment on the development of strength between abrasive grains and bonding bridges, and the nature of fracture and wear in vitrified grinding wheels.
引用
收藏
页码:177 / 182
页数:6
相关论文
共 50 条
  • [41] Interfacial Structure and Passivation Properties of Al2O3 on Silicon
    Zhang, Wei
    Wang, Feng
    Davis, Kristopher O.
    Jiang, Kaiyun
    Schoenfeld, Winston V.
    Looney, J. Patrick
    2016 IEEE 43RD PHOTOVOLTAIC SPECIALISTS CONFERENCE (PVSC), 2016, : 1163 - 1167
  • [42] On the formation of interfacial and internal voids inα-Al2O3 scales
    B. A. Pint
    Oxidation of Metals, 1997, 48 : 303 - 328
  • [43] Improvement of Al2O3/Ge interfacial properties by O2-annealing
    Shibayama, Shigehisa
    Kato, Kimihiko
    Sakashita, Mitsuo
    Takeuchi, Wakana
    Nakatsuka, Osamu
    Zaima, Shigeaki
    THIN SOLID FILMS, 2012, 520 (08) : 3397 - 3401
  • [44] HEAT-CAPACITY CALCULATIONS FOR AL2O3 CORUNDUM AND MGSIO3 ILMENITE
    MCMILLAN, PF
    ROSS, NL
    PHYSICS AND CHEMISTRY OF MINERALS, 1987, 14 (03) : 225 - 234
  • [45] STRENGTH OF AL2O3 AND AL2O3-TIC CERAMICS IN RELATION TO THEIR FRACTURE SOURCES
    WATANABE, M
    FUKUURA, I
    AMERICAN CERAMIC SOCIETY BULLETIN, 1981, 60 (03): : 394 - 394
  • [46] Broadband near infrared photoluminescence of Cu2+-doped corundum (α-Al2O3)
    Romanov, Alexey N.
    Haula, Elena V.
    Kapustin, Arseny A.
    Kostyukov, Alexey A.
    Egorov, Anton E.
    Kuzmin, Vladimir A.
    Korchak, Vladimir N.
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2024, 107 (02) : 979 - 983
  • [47] Surface and catalytic properties of Al2O3, CuO/Al2O3 and ZnO/Al2O3 systems
    El-Nabarawy, Th.
    Attia, A.A.
    Hassan, N.A.
    Youssef, A.M.
    Adsorption Science and Technology, 1995, 12 (02):
  • [48] Oxidation and interfacial fracture behaviour of NiCrAlY/Al2O3 coatings on an orthorhombic-Ti2AlNb alloy
    Li, H. Q.
    Wang, Q. M.
    Jiang, S. M.
    Ma, J.
    Gong, J.
    Sun, C.
    CORROSION SCIENCE, 2011, 53 (03) : 1097 - 1106
  • [49] Vibrational properties of OH groups associated with divalent cations in corundum (α-Al2O3)
    Jollands, Michael C.
    Jin, Shiyun
    Curti, Martial
    Guillaumet, Maxime
    Beneut, Keevin
    Giura, Paola
    Balan, Etienne
    EUROPEAN JOURNAL OF MINERALOGY, 2023, 35 (05) : 873 - 890
  • [50] Influences of microfine α-Al2O3 and cement additions on properties of corundum based castable
    Liu, Xuexin
    Ke, Changming
    2002, Luoyang Naihuo Cailiao Yanjiusuo (36):