SHOCK RESPONSE OF SILICON NITRIDE

被引:0
|
作者
Dandekar, D. P. [1 ]
Casem, D. T. [1 ]
Motoyashiki, Y. [2 ]
Sato, E. [2 ]
机构
[1] USA, Res Lab, Aberdeen Proving Ground, MD 21005 USA
[2] Inst Space & Astronaut Sci, Kanagawa 2298510, Japan
关键词
Shock response; silicon nitride; Hugoniot Elastic Limit; spall strength;
D O I
暂无
中图分类号
O469 [凝聚态物理学];
学科分类号
070205 ;
摘要
Silicon nitride is suitable for varied applications because its properties can be tailored through processing and doping. The current work presents shock response of silicon nitride marketed as SN282. The density of this material, 3.4 Mg/m(3), exceeds its single crystal density, 3.2 Mg/m(3), due to the presence of lutetium oxide as an additive around 5% by weight in the material. While the average grain size is 3.4 microns, the aspect ratio of the grains exceed 3. Preliminary results of shock wave experiments may be summarized as follows: (1) The Hugoniot Elastic Limit (HEL) of SN282 lies between 10.8 and 11.9 GPa. (2) The magnitude of the inelastic wave velocity just above the HEL is 8.73 km/s, suggesting that inelastic deformation above the HEL is due to shock induced plasticity in the material. (3) The value of the spall strength lies between 0.57 and 0.65 GPa. The spall strength of SN282 remains unchanged even when shocked beyond the HEL to at least 19.2 GPa unlike other brittle ceramics.
引用
收藏
页码:985 / +
页数:2
相关论文
共 50 条
  • [21] Thermal shock behavior of isotropic and anisotropic porous silicon nitride
    [J]. She, J., 1600, American Ceramic Society (86):
  • [22] Thermal shock of porous silicon nitride with preferentially aligned grains
    Vandeperre, LJ
    Inagaki, Y
    Clegg, WJ
    [J]. JOURNAL OF MATERIALS RESEARCH, 2003, 18 (11) : 2724 - 2729
  • [23] Erosion response of highly anisotropic silicon nitride
    Zhang, Y
    Cheng, YB
    Lathabai, S
    Hirao, K
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2005, 88 (01) : 114 - 120
  • [24] Inelastic response of silicon to shock compression
    A. Higginbotham
    P. G. Stubley
    A. J. Comley
    J. H. Eggert
    J. M. Foster
    D. H. Kalantar
    D. McGonegle
    S. Patel
    L. J. Peacock
    S. D. Rothman
    R. F. Smith
    M. J. Suggit
    J. S. Wark
    [J]. Scientific Reports, 6
  • [25] Inelastic response of silicon to shock compression
    Higginbotham, A.
    Stubley, P. G.
    Comley, A. J.
    Eggert, J. H.
    Foster, J. M.
    Kalantar, D. H.
    McGonegle, D.
    Patel, S.
    Peacock, L. J.
    Rothman, S. D.
    Smith, R. F.
    Suggit, M. J.
    Wark, J. S.
    [J]. SCIENTIFIC REPORTS, 2016, 6
  • [26] Sintering behavior and mechanical and thermal shock properties of silicon nitride-boron nitride composites
    Orgaz, F
    Capel, F
    Rodríguez, MA
    [J]. EURO CERAMICS VIII, PTS 1-3, 2004, 264-268 : 1067 - 1070
  • [27] EQUATION OF STATE OF ALUMINUM NITRIDE AND ITS SHOCK RESPONSE
    DANDEKAR, DP
    ABBATE, A
    FRANKEL, J
    [J]. JOURNAL OF APPLIED PHYSICS, 1994, 76 (07) : 4077 - 4085
  • [28] Urgent communication - Shock-wave synthesis of cubic silicon nitride
    Yunoshev, AS
    [J]. COMBUSTION EXPLOSION AND SHOCK WAVES, 2004, 40 (03) : 370 - 373
  • [29] Transient thermal shock behavior simulation of porous silicon nitride ceramics
    Chen, Meng
    Wang, Hongjie
    Jin, Haiyun
    Pan, Xide
    Jin, Zhihao
    [J]. CERAMICS INTERNATIONAL, 2016, 42 (02) : 3130 - 3137