Microstructure and creep properties of Sn-Ag-Cu lead-free solders bearing minor amounts of the rare earth cerium

被引:20
|
作者
Zhang, Liang [1 ]
Xue, Song-bai [1 ]
Gao, Li-li [1 ]
Chen, Yan [2 ]
Yu, Sheng-lin [1 ,3 ]
Sheng, Zhong [1 ]
Zeng, Guang [1 ]
机构
[1] Nanjing Univ Aeronaut & Astronaut, Coll Mat Sci & Technol, Nanjing 210016, Peoples R China
[2] Harbin Welding Inst, Harbin, Peoples R China
[3] China Elect Technol Grp Corp, Res Inst 14, Nanjing, Peoples R China
关键词
Solders; Alloys; Mechanical properties of materials; Thermodynamics; Creep; Chemical elements and inorganic compounds; MECHANICAL-PROPERTIES; INTERMETALLIC COMPOUNDS; INDENTATION CREEP; ALLOYS; NI; COMPOUND; BEHAVIOR; GROWTH; SOLDERABILITY; JOINTS;
D O I
10.1108/09540911011036262
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Purpose - The purpose of this paper is to investigate the effects of minor addition of the rare earth (RE) element cerium, Cc, on the microstructures and creep properties of Sn-Ag-Cu solder alloys. Design/methodology/approach - The pure Sn, Sn-Cu alloy, Sn-Ag alloy and Cu-Ce alloy were used as raw materials. Sn-Ag-Cu alloys with different contents of RE Cc were chosen to compare with Sn-Ag-Cu. The raw materials of Sn, Sn-Cu alloy, Sn-Ag alloy, Cu-Ce alloy were melted in a ceramic crucible, and were melted at 550 degrees C +/- 1 degrees C for 40 minutes. To homogenize the solder alloy, mechanical stirring was performed every ten minutes using a glass rod. During the melting, KG + LiCl (1.11), were used over the surface of liquid solder to prevent oxidation. The melted solder was chill cast into a rod. Findings - It is found that the microstructure exhibits smaller grains and the A0n/CU6Sn5 intermetallic compound (IMC) phases are modified in matrix with the addition of Cc. In particular, the addition of 0.03 wt.% Cc to the Sn-Ag-Cu solder can refine the microstructures and decrease the thickness of the IMC layers of Sn-Ag-Cu solder alloys. Meanwhile, thermodynamic analysis showed that these phenomena could be attributed to the reduction of the driving force for Cu-Sn IMC formation due to the addition of Cc. Results calculated using the thermodynamic method are close to the above experimental data. Thus, the optimum content of Cc in Sn-Ag-Cu solder alloys should be about 0.030 percent. Additionally, the effect of Cc on the creep rupture life of Sn-Ag-Cu soldered joints was studied. It was found that the creep rupture life may be increased up to 7.5 times more than that of the original Sn-Ag-Cu alloy, when Cc accounts for 0.030 percent. Originality/value - This paper usefully investigates the effects of the RE cerium (Cc), on the microstructures and creep properties of Sn-Ag-Cu solder alloys, optimizing the quantity of Cc in the Sn-Ag-Cu solder alloy through a thermodynamic method and by creep-rupture life testing.
引用
收藏
页码:30 / 36
页数:7
相关论文
共 50 条
  • [11] Study on microstructure and properties of Sn-Ag-Cu-Mg lead-free solders
    Lu, Sheng
    Chen, Jing
    Luo, Fei
    Wang, Baohua
    ESTC 2008: 2ND ELECTRONICS SYSTEM-INTEGRATION TECHNOLOGY CONFERENCE, VOLS 1 AND 2, PROCEEDINGS, 2008, : 1193 - +
  • [12] Creep rupture of lead-free Sn-3.5Ag-Cu solders
    Joo, DK
    Yu, J
    Shin, SW
    JOURNAL OF ELECTRONIC MATERIALS, 2003, 32 (06) : 541 - 547
  • [13] Creep rupture of lead-free Sn-3.5Ag-Cu solders
    D. K. Joo
    Jin Yu
    S. W. Shin
    Journal of Electronic Materials, 2003, 32 : 541 - 547
  • [14] Recent progress of Sn-Ag-Cu lead-free solders bearing alloy elements and nanoparticles in electronic packaging
    Wu, Jie
    Xue, Song-bai
    Wang, Jing-wen
    Liu, Shuang
    Han, Yi-long
    Wang, Liu-jue
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2016, 27 (12) : 12729 - 12763
  • [15] Temperature dependence of anelastic properties in Sn-Ag-Cu system and Sn-3.5Ag alloys of lead-free solders
    Nakamura, Y
    Ono, T
    JOURNAL OF MATERIALS SCIENCE, 2005, 40 (12) : 3267 - 3269
  • [16] Development of new Sn-Ag-Cu lead-free solders containing fourth elements
    Kim, KS
    Suganuma, K
    2003 3RD INTERNATIONAL SYMPOSIUM ON ENVIRONMENTALLY CONSCIOUS DESIGN AND INVERSE MANUFACTURING - ECODESIGN '03, 2003, : 414 - 415
  • [17] Temperature Dependence of Creep and Hardness of Sn-Ag-Cu Lead-Free Solder
    Han, Y. D.
    Jing, H. Y.
    Nai, S. M. L.
    Xu, L. Y.
    Tan, C. M.
    Wei, J.
    JOURNAL OF ELECTRONIC MATERIALS, 2010, 39 (02) : 223 - 229
  • [18] Temperature Dependence of Creep and Hardness of Sn-Ag-Cu Lead-Free Solder
    Y.D. Han
    H.Y. Jing
    S.M.L. Nai
    L.Y. Xu
    C.M. Tan
    J. Wei
    Journal of Electronic Materials, 2010, 39 : 223 - 229
  • [19] Properties and microstructure of Sn-0.7Cu-0.05Ni lead-free solders with rare earth Nd addition
    Liu, Shuang
    Xue, Song-bai
    Zhong, Su-juan
    Pei, Ying-ying
    Sun, Hua-wei
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2019, 30 (02) : 1400 - 1410
  • [20] Fatigue crack-growth behavior of Sn-Ag-Cu and Sn-Ag-Cu-Bi lead-free solders
    J. Zhao
    Y. Mutoh
    Y. Miyashita
    S. L. Mannan
    Journal of Electronic Materials, 2002, 31 : 879 - 886