Synthesis and tribological properties of ultrafine Cr2AlC MAX phase

被引:7
|
作者
Tan, Lian [1 ]
Guan, Chunlong [2 ]
Tian, Ye [3 ]
Dang, Pei [3 ]
Wang, Shun [2 ]
Li, Jinling [2 ]
Li, Wenfeng [2 ]
Zhao, Zhiwei [2 ]
机构
[1] North China Univ Water Resources & Elect Power, Sch Elect Power, Zhengzhou 450000, Henan, Peoples R China
[2] Henan Univ Technol, Sch Mat Sci & Engn, Engn Lab High Temp Resistance Wear Mat, Zhengzhou 450007, Henan, Peoples R China
[3] Henan Univ Technol, Sch Mech & Elect Engn, Zhengzhou 450007, Henan, Peoples R China
基金
中国国家自然科学基金;
关键词
Cr2AlC powder; Ultrafine Cr2AlC powder; Microwave hybrid heating; Tribological properties; LOW-TEMPERATURE SYNTHESIS; HIGH-PURITY; CERAMICS; MICROSTRUCTURE; NANOLAMELLAS; OXIDATION; MECHANISM; BEHAVIOR;
D O I
10.2109/jcersj2.18184
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A microwave hybrid heating method was used for the synthesis of Cr2AlC powder using two carbon sources of graphite and Cr3C2, and tribological behaviour of Cr2AlC powders was investigated. The purity of Cr2AlC is sensitive to the synthesis temperature and the starting materials used. For a Cr/Al/C system, Cr2AlC with a small amount of Cr7C3 was synthesised at 1100 degrees C for 3 min. For Cr/Al/Cr3C2 system, high purity Cr2AlC was synthesized at 1050 degrees C for 3 min. Ultrafine Cr2AlC powder with a grain diameter of less than 500 nm (denoted by u-Cr2AlC) could be prepared by ball-milling and ultrasonic treatment. The tribological properties of as-synthesised and ultrafine Cr2AlC powders as an additive in 150SN base oil were evaluated by an MMW-1A four-ball friction and wear tester. The results show that the base oil containing 2 wt % Cr2AlC presented good tribological performance under a load of 300 N. In addition, the particle size plays an important role in the tribological performance. Ultrafine Cr2AlC powder shows a better tribological performance than MoS2 and assynthesised Cr2AlC. The improved tribological properties of the u-Cr2AlC sample could be attributed to the formation of a tribo-film under friction. (C) 2019 The Ceramic Society of Japan. All rights reserved.
引用
收藏
页码:754 / 760
页数:7
相关论文
共 50 条
  • [41] Type II Hot Corrosion Screening Tests of a Cr2AlC MAX Phase Compound
    James L. Smialek
    Simon Gray
    Oxidation of Metals, 2018, 90 : 555 - 570
  • [42] Type II Hot Corrosion Screening Tests of a Cr2AlC MAX Phase Compound
    Smialek, James L.
    Gray, Simon
    OXIDATION OF METALS, 2018, 90 (5-6): : 555 - 570
  • [43] Pulsed electrospark deposition of MAX phase Cr2AlC based coatings on titanium alloy
    Zamulaeva, E. I.
    Levashov, E. A.
    Sviridova, T. A.
    Shvyndina, N. V.
    Petrzhik, M. I.
    SURFACE & COATINGS TECHNOLOGY, 2013, 235 : 454 - 460
  • [44] Alumina scale buckling during high temperature oxidation of Cr2AlC MAX Phase
    Zuber, A.
    Parry, G.
    Coupeau, C.
    Renault, P. O.
    Gauthier-Brunet, V.
    Dubois, S.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2023, 43 (16) : 7334 - 7340
  • [45] Electron correlation effects in the MAX phase Cr2AlC from first-principles
    Du, Y. L.
    Sun, Z. M.
    Hashimoto, H.
    Barsoum, M. W.
    JOURNAL OF APPLIED PHYSICS, 2011, 109 (06)
  • [46] Effect of Cr2AlC content on the properties of a Cu-Cr2AlC composite
    Wang, Xin-Sheng
    Lu, Zhen-Lin
    Lin, Gao-Ting
    Jia, Lei
    Chen, Jiang-Xian
    RESULTS IN PHYSICS, 2016, 6 : 789 - 795
  • [47] Reaction Synthesis of Cr2AlC Ceramics Powders
    Guan, Chunlong
    Zhang, Ziping
    Shan, Yingchun
    Wang, Chunhua
    CHINESE CERAMICS COMMUNICATIONS III, 2013, 624 : 13 - +
  • [48] Synthesis and characterization of Cr2AlC with nanolaminated particles
    Su, Zhongliang
    Zeng, Shu
    Zhou, Jian
    Sun, Zhimei
    CHINESE SCIENCE BULLETIN, 2014, 59 (26): : 3266 - 3270
  • [49] Synthesis and characterization of Cr2AlC with nanolaminated particles
    Zhongliang Su
    Shu Zeng
    Jian Zhou
    Zhimei Sun
    Science Bulletin, 2014, (26) : 3266 - 3270
  • [50] Molten salts electrochemical synthesis of Cr2AlC
    Abdelkader, Amr M.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2016, 36 (01) : 33 - 42