Oxidation Resistance of Shot Peened Austenitic Stainless Steel Superheater Tubes in Steam

被引:0
|
作者
Tossey, Brett M. [1 ]
Khan, Hassan [2 ]
Andress, Tom [2 ]
机构
[1] DNV GL, 5777 Frantz Rd, Dublin, OH 43017 USA
[2] Amer Elect Power Co, One Riverside Plaza, Columbus, OH 43215 USA
来源
ADVANCES IN MATERIALS TECHNOLOGY FOR FOSSIL POWER PLANTS: PROCEEDINGS FROM THE EIGHTH INTERNATIONAL CONFERENCE, 2016 | 2016年
关键词
Shot peening; shot blasted; steam; oxidation resistance; Type; 304H; austenitic; exfoliation; superheater; SA213;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Steam-side oxidation and the resultant exfoliation of iron-based scales cause unplanned shutdowns at coal-fired power generation plants. Exfoliate removal is currently limited to frequent unit cycling to minimize the volume of exfoliated scale, upgrading a plant with a "blow down" system, or installing a higher alloy. This paper discusses the rate of steam-side oxidation on Type 304H stainless steel (304H) tube after shot peening the internal surface with commercially available techniques. Shot peening the ID of Type 304H austenitic stainless steel superheater tubes has been shown to improve the overall oxidation resistance in steam. Decreasing the oxidation rate directly impacts the volume of exfoliated scale. The adherent spinel scales are thinner and more robust than non-shot peened tubes of the same alloy. Most of the improved oxidation resistance can be attributed to the presence of a spinel oxide layer combined with a continuous chromia layer formed near the steam touched surfaces. The presence of a continuous chromia layer vastly reduces the outward diffusion of iron and minimizes the formation of iron-based scales that exfoliate. This work showed that a uniform cold-worker layer along the tube ID has a profound effect on oxidation resistance. Incomplete coverage allows oxidation to proceed in the non-hardened regions at a rate comparable to the oxidation rate on unpeened Type 304H.
引用
收藏
页码:855 / 866
页数:12
相关论文
共 50 条
  • [31] Thermodynamic Consideration of the Steam Oxidation Resistance of Austenitic Stainless Steels Forming Intermetallic Compound
    Kochi, Norifumi
    Nishiyama, Yoshitaka
    MATERIALS TRANSACTIONS, 2018, 59 (12) : 1903 - 1910
  • [32] OXIDATION RESISTANCE OF A NEW CLASS OF HIGH ALUMINUM AUSTENITIC STAINLESS-STEEL
    MCGURTY, JA
    NEKKANTI, R
    MOTEFF, J
    JOURNAL OF METALS, 1984, 36 (07): : 41 - 41
  • [33] Corrosion resistance of austenitic stainless steel using cathodic plasma electrolytic oxidation
    Heo, Jun
    Lee, Jaewoo
    Kim, Sungwoo
    Alfantazi, Akram
    Cho, Sung Oh.
    SURFACE & COATINGS TECHNOLOGY, 2023, 462
  • [34] Oxidation behaviour of austenitic stainless steel 304HCu in Advanced Ultra Supercritical (AUSC) steam and the efficacy of shot-peening treatment
    Sundaresan, C.
    Ghule, Bhagwat
    Dey, H. C.
    Ningshen, S.
    Vijayshankar, Dandapani
    Raja, V. S.
    CORROSION SCIENCE, 2024, 235
  • [35] Stress Relaxation of the Shot-Peened Austenitic Stainless Steels at Temperatures Lower than 350℃
    Takemoto, Mikio
    Nakamura, Motoaki
    Ueno, Shuichi
    Zairyo to Kankyo/ Corrosion Engineering, 2021, 70 (07): : 217 - 227
  • [36] Exploring the effect of shot peening coverage on the stress corrosion cracking resistance of austenitic stainless steel
    Ralls, Alessandro M.
    John, Merbin
    Misra, Manoranjan
    Menezes, Pradeep L.
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2025, 136 (02): : 801 - 826
  • [37] Assessment of remaining life of superheater austenitic steel tubes in oil shale PF boilers
    Thermal Engineering Department, Tallinn University of Technology , 116 Kopli St., 11712 Tallinn, Estonia
    Oil Shale, 2006, 3 (267-274)
  • [38] Assessment of remaining life of superheater austenitic steel tubes in oil shale PF boilers
    Klevtsov, I.
    Tallermo, H.
    Bojarinova, T.
    Dedov, A.
    OIL SHALE, 2006, 23 (03) : 267 - 274
  • [39] Fatigue Failure of 321 Stainless Steel Superheater Tubes from a Thermal Incinerator
    Elshawesh, F.
    Abusowa, K.
    ElRagei, O.
    El Haddad, F.
    Mahfud, H.
    JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2008, 8 (01) : 54 - 59
  • [40] Steam oxidation resistance of selected austenitic steels
    Osgerby, S
    Fry, AT
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS, 2004, 461-464 : 1023 - 1030