摘要
A detailed study of the high-temperature oxidation behavior of reactively powder processed nanostructure nickel aluminides Ni3Al and NiAl (with and without microalloying additions) starting from elemental nanopowders in air at two different temperatures (800 and 1000 degrees C) for 200 h was carried out, as well as the sulphidation behavior (in 10% SO2, 90% He atmosphere) at 800 degrees C for 100 h. The weight gain per unit area (mg/cm(2)) due to oxide scale formation at a given exposure time t (h) and temperature was discussed. Thermodynamics and kinetics were used to explain the oxidation mechanism. The high temperature oxidation/or sulphidation resistance was improved due to nanostructure grains formation. Also, additions of a small amount of Nb (up to 4 wt%) as microalloying element resulted in a significant increase in the high temperature oxidation/ or sulphidation resistance compared to the microalloying free intermetallics. Also, the results indicated that nanostructure NiAl (with and without micro-alloying elements) showed superior high temperature oxidation/or sulphidation resistance compared to the nanostructure Ni3Al (with and without micro-alloying elements). Both XRD and SEM/EDS-analysis were used to identify the oxide phases present after the high temperature oxidation/or sulphidation exposure of nanostructure aluminides at 1000 degrees C after 200 h, and at 800 degrees C after 100 h, respectively. (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:178 / 188
页数:11
相关论文
共 50 条
  • [21] HIGH-TEMPERATURE DEFORMATION OF TITANIUM ALUMINIDE ALLOYS
    SABINASH, CM
    SASTRY, SML
    JERINA, KL
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1995, 192 : 837 - 847
  • [22] DEVELOPMENT OF OXIDATION RESISTANT HIGH-TEMPERATURE INTERMETALLICS
    GRABKE, HJ
    BRUMM, M
    STEINHORST, M
    MATERIALS SCIENCE AND TECHNOLOGY, 1992, 8 (04) : 339 - 344
  • [23] HIGH-TEMPERATURE INTERMETALLICS - WITH PARTICULAR EMPHASIS ON TIAL
    YAMAGUCHI, M
    MATERIALS SCIENCE AND TECHNOLOGY, 1992, 8 (04) : 299 - 307
  • [24] MELTING AND CASTING PROCESSES FOR HIGH-TEMPERATURE INTERMETALLICS
    SEN, S
    STEFANESCU, DM
    JOM-JOURNAL OF THE MINERALS METALS & MATERIALS SOCIETY, 1991, 43 (05): : 30 - 34
  • [25] High-temperature internal friction on TiAl intermetallics
    Pérez-Bravo, M
    Nó, ML
    Madariaga, I
    Ostolaza, K
    San Juan, J
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 370 (1-2): : 240 - 245
  • [26] High-temperature corrosion of nickel alloy TsNK7P with a protective aluminide coating
    Smyslov, AM
    Nev'yantseva, RR
    Bybin, AA
    Parfenov, EV
    PROTECTION OF METALS, 2004, 40 (05): : 497 - 500
  • [27] High-temperature oxidation resistance of a range of intermetallics
    Kurokawa, Kazuya
    Taniguchi, Shigeji
    Zairyo to Kankyo/ Corrosion Engineering, 1999, 48 (03): : 117 - 122
  • [28] High-Temperature Corrosion of Nickel Alloy TsNK7P with a Protective Aluminide Coating
    A. M. Smyslov
    R. R. Nev'yantseva
    A. A. Bybin
    E. V. Parfenov
    Protection of Metals, 2004, 40 : 497 - 500
  • [29] Nano-scale reactants in the self-propagating high-temperature synthesis of nickel aluminide
    Hunt, EM
    Plantier, KB
    Pantoya, ML
    ACTA MATERIALIA, 2004, 52 (11) : 3183 - 3191
  • [30] A Method for Computing the Service Life and Phase Composition of Aluminide Coatings on High-Temperature Nickel Alloys
    V. N. Simonov
    Yu. P. Shkretov
    L. V. Yazonkin
    Metal Science and Heat Treatment, 2004, 46 : 445 - 448