Improvement of microstructure, mechanical properties and cutting performance of Ti(C,N)-based cermets by ultrafine La2O3 additions

被引:31
|
作者
Kang, Xiyue [1 ]
Lin, Nan [2 ]
He, Yuehui [1 ]
Zhang, Qiankun [3 ]
Zhang, Meimei [1 ]
Yan, Yan [4 ]
Liu, Yi [4 ]
机构
[1] Cent South Univ, State Key Lab Powder Met, Changsha 410083, Peoples R China
[2] Hunan Univ, Coll Mat Sci & Engn, Changsha 410082, Hunan, Peoples R China
[3] Xiangtan Univ, Sch Mech Engn, Xiangtan 411105, Peoples R China
[4] METCERA Crop Ltd, Chengdu 610000, Peoples R China
基金
中国国家自然科学基金;
关键词
Ti(C; N)-based cermets; Ultrafine La2O3; Microstructure; Core-rim structure; Mechanical properties; WC-10CO ALLOYS; TOOL WEAR; RIM PHASE; WC-CO; Y2O3; TI(C; TAC;
D O I
10.1016/j.ceramint.2021.03.328
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Ti(C,N)-WC-Mo2C-TaC-Co-Ni cermets with various content of La2O3 were prepared by gas-pressure sintering at 1450 degrees C. The effects of ultrafine La2O3 additions (0, 0.05, 0.1 and 0.2 wt%) on the microstructure, mechanical properties, wear resistance and cutting performance of cermets were explored. In the microstructure of cermets, the La2O3 particles and dissolved La element in binder phases were observed, which could inhibit the dissolutionprecipitation process of ceramics phases during liquid-sintering. Furthermore, the La2O3 could absorb and react with the impurity Al element with low melting point from raw powders, avoiding the appearance of liquid phase at the low temperature and partial overheating during sintering process. These mechanisms could inhibit the abnormal growth of Ti(C,N) core-(Ti,W,Mo,Ta)(C,N) rim structures effectively, leading to the thinning of brittle rim phases and coarsening of wear-proof Ti(C,N) particles. The decrease of proportion of brittle rim phase and ultrafine Ti(C,N) particles promoted the fracture toughness. The increase of proportion and grain size of Ti(C,N) improved the hardness, wear resistance and cutting performance significantly. However, the excessive addition of La2O3 would result in the agglomeration of La2O3, causing the sharp decline of mechanical properties and cutting performance. The cermet with 0.1 wt% La2O3 addition possessed the optimal mechanical properties with Vickers hardness, transverse rupture strength and fracture toughness of 1710 (HV30) Kgf/mm2, 2480 MPa and 11.7 MPa m1/2, respectively.
引用
收藏
页码:19934 / 19944
页数:11
相关论文
共 50 条
  • [21] Microstructure and properties of the cermets based on Ti(C, N)
    Zhou, Shiquan
    Zhao, Wei
    Xiong, Weihao
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2009, 27 (01): : 26 - 32
  • [22] Effect of VC/Cr3C2 on microstructure and mechanical properties of Ti(C,N)-based cermets
    Zhan Bin
    Liu Ning
    Jin Zhi-bo
    Li Qi-long
    Shi Jin-gang
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2012, 22 (05) : 1096 - 1105
  • [23] MICROSTRUCTURE AND PROPERTIES OF THE CERMETS BASED ON Ti(C,N)
    Zhou, S. Q.
    Zhao, W.
    Xiong, W. H.
    MECHANICAL PROPERTIES AND PROCESSING OF CERAMIC BINARY,TERNARY, AND COMPOSITE SYSTEMS, 2009, 29 (02): : 41 - 50
  • [24] Microstructure and properties of CVD coated Ti(C, N)-based cermets with varying WC additions
    You, Qianbing
    Xiong, Ji
    Guo, Zhixing
    Liu, Junbo
    Yang, Tian'en
    Qin, Chengtao
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2019, 81 : 299 - 306
  • [25] EFFECT OF MICROSTRUCTURE ON MECHANICAL-PROPERTIES AND CUTTING PERFORMANCE OF AL2O3-TI(C, N) CERAMICS
    KOYAMA, T
    UCHIDA, S
    NISHIYAMA, A
    NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1992, 100 (04): : 520 - 524
  • [26] Effects of metal phases and carbides on the microstructure and mechanical properties of Ti(C,N)-based cermets cutting tool materials
    Zhou, Huijun
    Huang, Chuanzhen
    Zou, Bin
    Liu, Hanlian
    Zhu, Hongtao
    Yao, Peng
    Wang, Jun
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 618 : 462 - 470
  • [27] Microstructure and cutting performance of Ti(C, N)-based cermets heat-treated in nitrogen
    LIU Wenjun1
    RareMetals, 2007, (04) : 352 - 358
  • [28] Microstructure and cutting performance of Ti(C, N)-based cermets heat-treated in nitrogen
    Liu Wenjun
    Xiong Weihao
    Zheng Yong
    Shi Zengmin
    Ye Jiajian
    RARE METALS, 2007, 26 (04) : 352 - 358
  • [29] Effect of diamond addition on microstructure and mechanical properties of Ti(C,N)-based cermets
    Zhou, Haojun
    Tao, Hongliang
    Huang, Mingchu
    Yang, Hao
    Wu, Ning
    Li, Yimin
    Yin, Yuhang
    Luo, Fenghua
    CERAMICS INTERNATIONAL, 2021, 47 (02) : 2294 - 2302
  • [30] Effect of heating rate on the mechanical properties and microstructure of Ti(C,N)-based cermets
    Xu, Qingzhong
    Ai, Xing
    Zhao, Jun
    Zhang, Hongshan
    Qin, Wenzhen
    Gong, Feng
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 628 : 281 - 287