Degradation of Nextel 610-based oxide-oxide ceramic composites by aluminum oxychloride decomposition products

被引:13
|
作者
Hay, Randall S. [1 ]
Keller, Kristin A. [1 ,2 ]
Zawada, Larry P. [1 ,3 ]
Jacobson, Nathan S. [4 ]
Fair, Geoff E. [5 ]
机构
[1] US Air Force, Res Lab, Mat & Mfg Directorate, Wright Patterson AFB, OH 45433 USA
[2] UES Inc, Dayton, OH USA
[3] UTC Inc, Beavercreek, OH USA
[4] NASA, Glenn Res Ctr, Cleveland, OH USA
[5] 3M Corp, Minneapolis, MN USA
关键词
alumina; ceramic matrix composites; degradation; fibers; mechanical; properties; STRESS-CORROSION CRACKING; TEMPERATURE MECHANICAL-BEHAVIOR; MONAZITE COATINGS; TENSILE-STRENGTH; FIBER STRENGTH; POROUS-MATRIX; AIR; FATIGUE; GROWTH; CREEP;
D O I
10.1111/jace.15573
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Nextel 610 alumina fibers and alumina-YAG (yttrium-aluminum garnet) matrices were used to make oxide-oxide ceramic matrix composites (CMCs) with and without monazite (LaPO4) fiber-matrix interfaces. Twelve sequential aluminum oxychloride (AlOCl) infiltrations with 1 hour heat treatments at 1100 degrees C and a final 1 hour heat treatment at 1200 degrees C were used for matrix densification. This matrix processing sequence severely degraded CMC mechanical properties. CMC tensile strengths and interlaminar tensile (ILT) strengths were less than 10 MPa and 1 MPa, respectively. Axial fracture of Nextel 610 fibers was observed after ILT testing, highlighting the extreme degradation of fiber strength. Extensive characterization was done to attempt to determine the responsible degradation mechanisms. Changes in Nextel 610 fiber microstructure after CMC processing were characterized by optical microscopy, SEM, and extensively by TEM. In AlOCl degraded fibers, grain boundaries near the fiber surface were wetted with a glass that contained Y2O3/SiO2 or Y2O3/La2O3/P2O5/SiO2, and near-surface pores were partially filled with Al2O3. This glass must also contain some Al2O3 and initially some chlorine. AlOCl decomposition products were predicted using the FactSage((R)) Thermochemical code, and were characterized by mass spectrometry. Effects of AlOCl precursors on monazite coated and uncoated Nextel 610 fibers tow and filament strength were evaluated. A mechanism for the severe degradation of the oxide-oxide CMCs and Nextel 610 fibers that involves subcritical crack growth promoted by release of chlorine containing species during breakdown of intergranular glasses in an anhydrous environment is proposed.
引用
收藏
页码:4203 / 4223
页数:21
相关论文
共 50 条
  • [21] Aluminum oxide ceramic fibers and materials based on them
    Grashchenkov, D. V.
    Balinova, Yu A.
    Tinyakova, E. V.
    GLASS AND CERAMICS, 2012, 69 (3-4) : 130 - 133
  • [22] Slurry-based protective coatings for Oxide/Oxide ceramic matrix composites
    Mechnich, Peter
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2021, 129 (01) : 32 - 39
  • [23] STRENGTH DEGRADATION OF OXIDE/OXIDE AND SiC/SiC CERAMIC MATRIX COMPOSITES IN CMAS AND CMAS/SALT EXPOSURES
    Faucett, David C.
    Choi, Sung R.
    PROCEEDINGS OF THE ASME TURBO EXPO 2011, VOL 1, 2011, : 497 - 504
  • [24] INFLUENCE OF ELEVATED TEMPERATURE SOLID PARTICLE EROSION ON STRENGTH DEGRADATION OF OXIDE/OXIDE CERAMIC MATRIX COMPOSITES
    Mirza, Farhan
    Panakarajupally, Ragav P.
    Rassi, J. E.
    Morscher, Gregory N.
    Abdi, Frank
    Choi, Sung
    PROCEEDINGS OF ASME TURBO EXPO 2023: TURBOMACHINERY TECHNICAL CONFERENCE AND EXPOSITION, GT2023, VOL 2, 2023,
  • [25] Ceramic Composites of the Zirconium Dioxide and Aluminum Oxide System Including Strontium Hexaaluminate
    Podzorova, L. I.
    Il'icheva, A. A.
    Sirotinkin, V. P.
    Antonova, O. S.
    Baikin, A. S.
    Kutuzova, V. E.
    Pen'kova, O. I.
    GLASS AND CERAMICS, 2021, 78 (5-6) : 231 - 236
  • [26] Ceramic Composites of the Zirconium Dioxide and Aluminum Oxide System Including Strontium Hexaaluminate
    L. I. Podzorova
    A. A. Il’icheva
    V. P. Sirotinkin
    O. S. Antonova
    A. S. Baikin
    V. E. Kutuzova
    O. I. Pen’kova
    Glass and Ceramics, 2021, 78 : 231 - 236
  • [27] HYDROSTATIC PRESSING OF CERAMIC TUBES BASED ON ALUMINUM-OXIDE
    ARTEMOVA, KK
    SOROKINA, AI
    MASLOVA, GY
    CHATOVA, LA
    REFRACTORIES, 1980, 21 (1-2): : 52 - 54
  • [28] Sintering of Composite Ceramic Based on Zirconium and Aluminum Oxide Powders
    Komolikov, Yu. I.
    Kashcheev, I. D.
    Khrustov, V. R.
    REFRACTORIES AND INDUSTRIAL CERAMICS, 2015, 56 (04) : 418 - 420
  • [29] Sintering of Composite Ceramic Based on Zirconium and Aluminum Oxide Powders
    Yu. I. Komolikov
    I. D. Kashcheev
    V. R. Khrustov
    Refractories and Industrial Ceramics, 2015, 56 : 418 - 420
  • [30] Thermal expansion of β-eucryptite in oxide-based ceramic composites
    Pelletant, A.
    Reveron, H.
    Chevalier, J.
    Fantozzi, G.
    Guinot, F.
    Blanchard, L.
    Falzon, F.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2013, 33 (03) : 531 - 538