Degradation of Nextel 610-based oxide-oxide ceramic composites by aluminum oxychloride decomposition products

被引:13
|
作者
Hay, Randall S. [1 ]
Keller, Kristin A. [1 ,2 ]
Zawada, Larry P. [1 ,3 ]
Jacobson, Nathan S. [4 ]
Fair, Geoff E. [5 ]
机构
[1] US Air Force, Res Lab, Mat & Mfg Directorate, Wright Patterson AFB, OH 45433 USA
[2] UES Inc, Dayton, OH USA
[3] UTC Inc, Beavercreek, OH USA
[4] NASA, Glenn Res Ctr, Cleveland, OH USA
[5] 3M Corp, Minneapolis, MN USA
关键词
alumina; ceramic matrix composites; degradation; fibers; mechanical; properties; STRESS-CORROSION CRACKING; TEMPERATURE MECHANICAL-BEHAVIOR; MONAZITE COATINGS; TENSILE-STRENGTH; FIBER STRENGTH; POROUS-MATRIX; AIR; FATIGUE; GROWTH; CREEP;
D O I
10.1111/jace.15573
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Nextel 610 alumina fibers and alumina-YAG (yttrium-aluminum garnet) matrices were used to make oxide-oxide ceramic matrix composites (CMCs) with and without monazite (LaPO4) fiber-matrix interfaces. Twelve sequential aluminum oxychloride (AlOCl) infiltrations with 1 hour heat treatments at 1100 degrees C and a final 1 hour heat treatment at 1200 degrees C were used for matrix densification. This matrix processing sequence severely degraded CMC mechanical properties. CMC tensile strengths and interlaminar tensile (ILT) strengths were less than 10 MPa and 1 MPa, respectively. Axial fracture of Nextel 610 fibers was observed after ILT testing, highlighting the extreme degradation of fiber strength. Extensive characterization was done to attempt to determine the responsible degradation mechanisms. Changes in Nextel 610 fiber microstructure after CMC processing were characterized by optical microscopy, SEM, and extensively by TEM. In AlOCl degraded fibers, grain boundaries near the fiber surface were wetted with a glass that contained Y2O3/SiO2 or Y2O3/La2O3/P2O5/SiO2, and near-surface pores were partially filled with Al2O3. This glass must also contain some Al2O3 and initially some chlorine. AlOCl decomposition products were predicted using the FactSage((R)) Thermochemical code, and were characterized by mass spectrometry. Effects of AlOCl precursors on monazite coated and uncoated Nextel 610 fibers tow and filament strength were evaluated. A mechanism for the severe degradation of the oxide-oxide CMCs and Nextel 610 fibers that involves subcritical crack growth promoted by release of chlorine containing species during breakdown of intergranular glasses in an anhydrous environment is proposed.
引用
收藏
页码:4203 / 4223
页数:21
相关论文
共 50 条
  • [1] Joining and mechanical testing of oxide/oxide (Nextel ™610/alumina-zirconia) ceramic composites
    Akram, Muhammad Yasir
    Casalegno, Valentina
    Ferraris, Monica
    Puchas, Georg
    Krenkel, Walter
    Roszeitis, Sven
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2019, 39 (07) : 2510 - 2517
  • [2] Fabrication technologies for oxide-oxide ceramic matrix composites based on electrophoretic deposition
    Stoll, E
    Mahr, P
    Krüger, HG
    Kern, H
    Thomas, BJC
    Boccaccini, AR
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2006, 26 (09) : 1567 - 1576
  • [3] The evaluation of novel interphases for oxide-oxide ceramic matrix composites
    Tye, A
    Lewis, MH
    ENGINEERING WITH CERAMICS, 1999, (59): : 177 - 186
  • [4] A model for the creep response of oxide-oxide ceramic matrix composites
    Zuiker, JR
    THERMAL AND MECHANICAL TEST METHODS AND BEHAVIOR OF CONTINUOUS-FIBER CERAMIC COMPOSITES, 1997, 1309 : 250 - 263
  • [5] Evaluation of all-oxide composites based on coated Nextel™ 610 and 650 fibers
    Keller, KA
    Mah, T
    Parthasarathy, TA
    Boakye, EE
    Cinibulk, M
    25TH ANNUAL CONFERENCE ON COMPOSITES, ADVANCED CERAMICS, MATERIALS, AND STRUCTURES: A, 2001, 22 (03): : 667 - 675
  • [6] All-oxide ceramic matrix composites (OCMC) based on low cost 3M Nextel™ 610 fabrics
    Pritzkow, Walter E. C.
    Almeida, Renato S. M.
    Mateus, Luisa B.
    Tushtev, Kamen
    Rezwan, Kurosch
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2021, 41 (05) : 3177 - 3187
  • [7] Investigation of Feedstock Preparation for Injection Molding of Oxide-Oxide Ceramic Composites
    Tulumen, Hasan Metin
    Hanemann, Thomas
    Piotter, Volker
    Stenzel, David
    JOURNAL OF MANUFACTURING AND MATERIALS PROCESSING, 2019, 3 (01):
  • [8] Optimization of Alumina Slurry for Oxide-Oxide Ceramic Composites Manufactured by Injection Molding
    Billotte, Catherine
    Fotsing, Edith Roland
    Ruiz, Edu
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2017, 2017
  • [9] Evaluation of surface finish technology in the manufacture of Oxide-Oxide ceramic matrix composites
    Tontisakis, A.
    Simpson, W.
    Lincoln, J.
    Dhawan, R.
    Opliger, M.
    CERAMICS INTERNATIONAL, 2021, 47 (04) : 5347 - 5363
  • [10] Application of terahertz time domain spectroscopy for NDT of oxide-oxide ceramic matrix composites
    Wu, Datong
    Haude, Christoph
    Burger, Ruben
    Peters, Ole
    INFRARED PHYSICS & TECHNOLOGY, 2019, 102