Investigation on the electrochemical assisted magnetic abrasive finishing for a stainless steel of SUS304

被引:12
|
作者
Sun, Xu [1 ,2 ,3 ]
Fu, Yongjian [2 ]
Lu, Wei [2 ]
Hang, Wei [4 ]
机构
[1] LongYan Univ, Special Vehicle Technol Res Ctr, Longyan 364000, Peoples R China
[2] Huaqiao Univ, Engn Res Ctr Brittle Mat Machining, Quanzhou 361000, Peoples R China
[3] Utsunomiya Univ, Grad Sch Engn, 7-1-2 Yoto, Utsunomiya, Tochigi 3218585, Japan
[4] Zhejiang Univ Technol, Key Lab E&M, Hangzhou 310014, Peoples R China
关键词
electrochemical effect; magnetic abrasive finishing; electrochemical magnetic abrasive finishing; passive films; high machining efficiency; PLANE;
D O I
10.1007/s00170-021-07529-x
中图分类号
TP [自动化技术、计算机技术];
学科分类号
0812 ;
摘要
In order to obtain a high accuracy with high machining efficiency for finishing hard alloy metal material, we proposed a hybrid finishing method which is electrochemical (ECM) effects assisted magnetic abrasive finishing (MAF). In this study, the electrochemical magnetic abrasive finishing (EMAF process) was divided into EMAF stage and MAF stage. The metal surface can be easily finished with the passive films formed in electrochemical reactions. Simultaneously, the passive films can be removed by frictional action between magnetic brush and workpiece surface. Thus, the essence of EMAF process is to form and remove the passive films on the workpiece surface. This study focused on investigating the finishing mechanism and finishing characteristics of EMAF process. Compared with traditional MAF process, it can be confirmed that the finishing efficiency is remarkably improved more than 75% by EMAF process, and the surface roughness is also lower in EMAF process. The optimal experimental result of EMAF process showed that the surface roughness was reduced to less than 30 nm from the original surface roughness 178 nm after 4 min in EMAF stage, and the surface roughness was finally reduced to 20 nm after 10 min in MAF stage. The material removal rate in hybrid finishing stage was nearly 7 times than that in MAF stage. Additionally, the effective finishing area in EMAF process was about 70% of that in MAF process.
引用
收藏
页码:1509 / 1522
页数:14
相关论文
共 50 条
  • [31] Effect of preheating in air on gas nitriding of SUS304 stainless steel
    Sueyoshi, H
    Hamaishi, K
    Kadomatsu, S
    Shiomizu, T
    Ohzono, Y
    MATERIALS TRANSACTIONS JIM, 1997, 38 (02): : 148 - 154
  • [32] Effects of Tritiated Water on Passivation Behavior of SUS304 Stainless Steel
    Oyaidzu, M.
    Isobe, K.
    Yamanishi, T.
    CORROSION POSTERS (GENERAL) - 222ND ECS MEETING/PRIME 2012, 2013, 50 (50): : 63 - 69
  • [33] Effect of Pulse Current on the Tensile Deformation of SUS304 Stainless Steel
    Xifeng Li
    Shen Wang
    Shuangjun Zhao
    Wei Ding
    Jun Chen
    Guohong Wu
    Journal of Materials Engineering and Performance, 2015, 24 : 5065 - 5070
  • [34] FRETTING PROPERTIES OF SUS304 STAINLESS STEEL IN A VACUUM ENVIRONMENT.
    Iwabuchi, A.
    Kato, K.
    Kayaba, T.
    1600, (110): : 3 - 4
  • [35] Dependence of deformation-induced magnetic field on plastic deformation for SUS304 stainless steel
    Li, Hongmei
    Chen, Zhenmao
    Li, Yong
    Takagi, Toshiyuki
    Uchimoto, Tetsuya
    Chigusa, Naoki
    Yoshida, Yasuhiko
    INTERNATIONAL JOURNAL OF APPLIED ELECTROMAGNETICS AND MECHANICS, 2012, 38 (01) : 17 - 26
  • [36] Effect of magnetic field on isothermal martensitic transformation in a sensitized SUS304 austenitic stainless steel
    Choi, Ju-young
    Fukuda, Takashi
    Kakeshita, Tomoyuki
    JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 577 : S605 - S608
  • [37] Effect of Hydrogen on Creep Properties of SUS304 Austenitic Stainless Steel
    Takazaki, Daisuke
    Tsuchiyama, Toshihiro
    Komoda, Ryosuke
    Dadfarnia, Mohsen
    Somerday, Brian P.
    Sofronis, Petros
    Kubota, Masanobu
    CORROSION, 2021, 77 (03) : 256 - 265
  • [38] RESEARCH OF THE WRINKLING ELIMINATION OF STAINLESS STEEL SUS304 BY VISCOUS PRESSURE
    Gao, Tiejun
    Yu, Kun
    Liu, Xiaojun
    Zhang, Hepeng
    ENGINEERING REVIEW, 2019, 39 (02) : 141 - 147
  • [39] FRETTING PROPERTIES OF SUS304 STAINLESS-STEEL IN A VACUUM ENVIRONMENT
    IWABUCHI, A
    KATO, K
    KAYABA, T
    WEAR, 1986, 110 (3-4) : 205 - 216
  • [40] Photoinhibition of stress corrosion cracking of sensitized SUS304 stainless steel
    Haruna, Takumi
    Onishi, Kozo
    Shibata, Toshio
    Nippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals, 1999, 63 (10): : 1365 - 1366