Sulphur poisoning of LaCr0.5-xMnxMg0.5O3•yMgO catalysts for methane combustion

被引:34
|
作者
Rosso, I [1 ]
Saracco, G [1 ]
Specchia, V [1 ]
Garrone, E [1 ]
机构
[1] Politecn Torino, Dipartimento Sci Mat & Ingn Chim, I-10129 Turin, Italy
关键词
LaCr0.5-xMnxMg0.5O3 center dot yMgO; perovskite; methane catalytic combustion; sulphur poisoning;
D O I
10.1016/S0926-3373(02)00153-4
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
LaCr0.5-xMnxMg0.5O3.yMgO catalysts (x = 0, 0.25, y = 0, 17) were prepared, characterised (X-ray diffraction, BET analysis, scanning electron microscopy-energy dispersion spectroscopy, transmission electron microscopy, FTIR spectroscopy, chemical and atomic absorption analyses), tested for high-temperature methane combustion and aged in presence of SO2 to investigate the effect of sulphur on their catalytic activity. The role of chromium presence in the perovskite structure have been assessed by comparison with earlier studies on Cr-free perovskites: (i) it worsens the activity of catalysts in the fresh state; (ii) owing to its acidic nature, it makes perovskites less prone to adsorb SO2 and so more resistant to sulphur poisoning; (iii) it renders catalyst regeneration by NH3 leaching less effective because of the partial solubility of chromium oxide in basic media. Conversely, MgO promotes catalytic activity of fresh LaCr0.5Mg0.5O3.yMgO catalysts and slows down sulphur poisoning of the LaCr0.25Mn0.25Mg0.5O3.17MgO catalyst only. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:195 / 205
页数:11
相关论文
共 50 条
  • [41] Removal of Cooking Fume by Catalytic Combustion on Pt/La-Al2O3+Ce0.5Zr0.5O2 Catalyst
    王健礼
    钟俊波
    龚茂初
    刘志敏
    赵明
    陈耀强
    [J]. Journal of Rare Earths, 2006, (05) : 633 - 635
  • [42] Oxidative coupling of methane in Ba0.5Sr0.5Co0.8Fe0.2O3-δ tubular membrane reactors
    Wang, HH
    Cong, Y
    Yang, WS
    [J]. CATALYSIS TODAY, 2005, 104 (2-4) : 160 - 167
  • [43] Effect of laser ablation on Ba0.5Sr0.5Co0.8Fe0.2O3-δ membrane for methane conversion
    Shen, Zigang
    Guo, Xiaorui
    Zhang, Wuqing
    Pan, Lijun
    [J]. MECHANICS, SOLID STATE AND ENGINEERING MATERIALS, 2011, 279 : 61 - +
  • [44] OXIDATIVE COUPLING OF METHANE OVER BA2SB(LA0.5BI0.5)O6 AND OTHER PEROVSKITE OXIDE CATALYSTS
    BATTLE, PD
    CARR, SW
    COPPLESTONE, FA
    ALMAER, SA
    [J]. JOURNAL OF THE CHEMICAL SOCIETY-CHEMICAL COMMUNICATIONS, 1992, (11) : 826 - 827
  • [45] Influence of mixing time on the purity and physical properties of SrFe0.5Ti0.5O3-δ powders produced by solution combustion
    Baharuddin, Nurul Akidah
    Muchtar, Andanastuti
    Somalu, Mahendra Rao
    Seyednezhad, Mohadeseh
    [J]. POWDER TECHNOLOGY, 2017, 313 : 382 - 388
  • [46] Dry reforming of methane by La0.5Sr0.5NiO3 perovskite oxides: influence of preparation method on performance and structural features of the catalysts
    Mousavi, Maryam
    Nakhaei Pour, Ali
    Gholizadeh, Mostafa
    Mohammadi, Ali
    Kamali Shahri, Seyed Mehdi
    [J]. JOURNAL OF CHEMICAL TECHNOLOGY AND BIOTECHNOLOGY, 2020, 95 (11) : 2911 - 2920
  • [47] MnOx/Ce0.5+xZr0.4-xLa0.1O1.95-Al2O3 catalysts used for benzene catalytic combustion
    Liao Chuanwen
    Li Xiaoshuang
    Wang Jianli
    Chen Yongdong
    Cao Hongyan
    Chen Yaoqiang
    Gong Maochu
    [J]. JOURNAL OF RARE EARTHS, 2011, 29 (02) : 109 - 113
  • [48] Catalytic Combustion of Diesel Soot over Ce0.5+xZr0.4-xLa0.1O2-Al2O3 Catalysts
    Zhu Yi
    Wang Jian-Li
    Chen Yong-Dong
    Liao Chuan-Wen
    Wang Shi-Dan
    Gong Mao-Chu
    Chen Yao-Qiang
    [J]. ACTA PHYSICO-CHIMICA SINICA, 2011, 27 (04) : 925 - 931
  • [49] A kinetic study of methane and carbon dioxide interconversion over 0.5%Pt/SrTiO3 catalysts
    Topalidis, A.
    Petrakis, D. E.
    Ladavos, A.
    Loukatzikou, L.
    Pomonis, P. J.
    [J]. CATALYSIS TODAY, 2007, 127 (1-4) : 238 - 245
  • [50] Partial oxidation of methane in Ba0.5Sr0.5Co0.8Fe0.2O3-δ membrane reactor at high pressures
    Lu, H
    Tong, JH
    Cong, Y
    Yang, WS
    [J]. CATALYSIS TODAY, 2005, 104 (2-4) : 154 - 159