摘要
Control of the deposition of SiC, BxC, Si-B-C, BN and Si-B-N layers for making multilayered composites is shown. SiC/B4C/SiC and SiC/Si-B-C/SiC layered materials allow self-healing of the matrix. The microstructure of BN interphase can be controlled to modify its properties and the Si-B-N ternary system can be used as a more oxidation resistant material and also to increase the interfacial bonding with the reinforcement fibers. The oxidation resistance of SiCf/BN/SiC is improved at moderate temperature when compared to SiCf/C/SiC. From the combination of self-healing properties at different temperatures of BxC and Si-B-C used with SiC in multilayered matrices and the ability of the mechanical compliant BN used as interphase to deviate the microcracks farther from the fibers, the preservation of the ceramic matrix composite properties for long duration, in oxidative environments, under high temperature fatigue, thermal and mechanical cycling is discussed.
引用
收藏
页码:63 / 68
页数:6
相关论文
共 50 条
  • [11] Self-Propagating High-Temperature Synthesis of Complex Chromium-Containing Silicon and Boron Oxides
    M. V. Kuznetsov
    Glass and Ceramics, 2001, 58 : 138 - 139
  • [12] High-temperature boron and phosphorus ion implantation in silicon
    Gadiyak, GV
    Bibik, AV
    ION BEAM MODIFICATION OF MATERIALS, 1996, : 810 - 814
  • [13] Oxidation of Silicon and Boron in Boron Containing Molten Iron
    Zhong-dong Y.
    Su-lan L.
    Zhe-fu L.
    Xiang-xin X.
    Journal of Iron and Steel Research International, 2007, 14 (6) : 32 - 36
  • [14] Oxidation of silicon and boron in boron containing molten iron
    Yang Zhong-dong
    Liu Su-lan
    Li Zhe-fu
    Xue Xiang-xin
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2007, 14 (06) : 32 - 36
  • [15] Oxidation of Silicon and Boron in Boron Containing Molten Iron
    YANG Zhong-dong
    Journal of Iron and Steel Research(International), 2007, (06) : 32 - 36
  • [16] High temperature oxidation of silicon and copper-silicon containing steels
    Martinez-Cazares, G. M.
    Mercado-Solis, R. D.
    Colas, R.
    Garza-Montes-de-Oca, N. F.
    IRONMAKING & STEELMAKING, 2013, 40 (03) : 221 - 230
  • [17] Experimental technique for high temperature and high strain rate testing of CMCs
    Puente, I
    Sanchez, JM
    MartinMeizoso, A
    CMMC 96 - PROCEEDINGS OF THE FIRST INTERNATIONAL CONFERENCE ON CERAMIC AND METAL MATRIX COMPOSITES, PTS 1 AND 2, 1997, 127-3 : 737 - 744
  • [18] Boron and silicon containing conjugated macromolecules
    Sengupta, Arijit
    Doshi, Ami
    Jaekle, Frieder
    Peetz, Ralf M.
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2012, 244
  • [19] Experimental technique for high temperature and high strain rate testing of CMCs
    Universidad de Navarra, San Sebastian, Spain
    Key Eng Mat, Pt 2 (737-744):
  • [20] BORON-CONTAINING STEELS FOR HIGH-STRENGTH FIXING COMPONENTS.
    Bykadorov, A.T.
    Kheifets, I.L.
    Soviet Forging and Sheet Metal Stamping Technology (English Translation of Kuznechno-Shtampovochno, 1986, (01): : 50 - 54