Study on the microstructure and creep behavior of Inconel 718 superalloy fabricated by selective laser melting

被引:65
|
作者
Shi, J. J. [1 ,2 ]
Li, X. [1 ,2 ]
Zhang, Z. X. [1 ,2 ]
Cao, G. H. [1 ,2 ]
Russell, A. M. [3 ,4 ]
Zhou, Z. J. [5 ]
Li, C. P. [5 ]
Chen, G. F. [5 ]
机构
[1] Shanghai Univ, State Key Lab Adv Special Steel, 99 Shangda Rd, Shanghai 200444, Peoples R China
[2] Shanghai Univ, Sch Mat Sci & Engn, 99 Shangda Rd, Shanghai 200444, Peoples R China
[3] Iowa State Univ, Dept Mat Sci & Engn, Ames, IA 50011 USA
[4] US DOE, Div Mat Sci & Engn, Ames Lab, Ames, IA 50011 USA
[5] Siemens Ltd, Corp Technol, Mat & Mfg Qualificat Grp, Beijing 100102, Peoples R China
关键词
SLM; Inconel; 718; Creep; Microstructure; Dislocation density; DELTA-PHASE PRECIPITATION; NICKEL-BASED SUPERALLOYS; MECHANICAL-PROPERTIES; HEAT-TREATMENT; CRYSTALLOGRAPHIC TEXTURE; METALLIC COMPONENTS; HIGH-TEMPERATURE; STAINLESS-STEEL; BASE ALLOYS; NI;
D O I
10.1016/j.msea.2019.138282
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Horizontal-direction Inconel 718 alloy cylindrical rods were fabricated by selective laser melting (SLM) and subsequently subjected to solution or homogenization plus double aging (SA or HA) treatments. Lever arm creep tests were performed with the creep tensile axis perpendicular to the building direction of the samples with a constant stress of 650 MPa at 650 degrees C. Scanning and transmission microscopy and electron backscatter diffraction were used to clarify the microstructure of the SA and HA samples before and after creep. The experimental results revealed that the average grain sizes of the SA and HA samples were basically the same before creep, and larger gamma' and gamma '' strengthening phases existed in the HA sample. The grains tended to grow, and the higher dislocation density within grains and lower local misorientation values close to the grain boundaries occurred in the HA sample during creep, which contributed to the longer creep rupture life in comparison with the SA sample. The fracture surfaces of the SA and HA samples displayed intergranular features, and the creep voids and micro-cracks were formed around the 8 or Laves phases at the grain boundaries. The creep fracture mechanism was also discussed.
引用
收藏
页数:10
相关论文
共 50 条
  • [41] Influence of cooling rate during the heat treatment process on the precipitates and ductility behavior of inconel 718 superalloy fabricated by selective laser melting
    Yang, Peixin
    Su, Haijun
    Guo, Yinuo
    Zhou, Haotian
    Xia, Le
    Shen, Zhonglin
    Wang, Meng
    Zhang, Zhuo
    Guo, Min
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 902
  • [42] Effect of Heat Treatment on Microstructure and Mechanical Properties of Inconel 718 Alloy Fabricated by Selective Laser Melting
    Zhang, Rong
    Liu, Zhongqiang
    Huang, Jiahao
    Zhu, Quanli
    Xiao, Zhiyu
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2021, 50 (01): : 255 - 262
  • [43] Influence of Selective Laser Melting Additive Manufacturing Parameters in Inconel 718 Superalloy
    Kladovasilakis, Nikolaos
    Charalampous, Paschalis
    Tsongas, Konstantinos
    Kostavelis, Ioannis
    Tzovaras, Dimitrios
    Tzetzis, Dimitrios
    MATERIALS, 2022, 15 (04)
  • [44] Effect of Heat Treatment on Microstructure and Mechanical Properties of Inconel 718 Alloy Fabricated by Selective Laser Melting
    Zhang Rong
    Liu Zhongqiang
    Huang Jiahao
    Zhu Quanli
    Xiao Zhiyu
    RARE METAL MATERIALS AND ENGINEERING, 2021, 50 (01) : 255 - 262
  • [45] Heterogeneities of microstructure and mechanical properties for inconel 718 strut tensile sample fabricated by selective laser melting
    Zhang, Liang
    Shi, Xiaoxiao
    Li, Ning
    Zhao, Lun
    Chen, Wei
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 12 : 2396 - 2406
  • [46] Stress relaxation of inconel 718 superalloy manufactured by selective laser melting (SLM)
    Alikarami, Sh
    Nakhodchi, S.
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2025, 214
  • [47] Improved creep properties of Inconel 718 fabricated by selective laser melting from boron-phosphorus interaction
    Wang, Lilin
    Yang, Fan
    Gui, Tianhong
    Huang, Weiming
    Lin, Xin
    Huang, Weidong
    MATERIALS RESEARCH LETTERS, 2024, 12 (09): : 661 - 667
  • [48] Effect of standard heat treatment on the microstructure and mechanical properties of selective laser melting manufactured Inconel 718 superalloy
    Zhang, Dongyun
    Niu, Wen
    Cao, Xuanyang
    Liu, Zhen
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 644 : 32 - 40
  • [49] Deformation behavior of selective laser-melted Inconel 718 superalloy
    Zhang, Shuya
    Guo, Chunwen
    Lin, Xin
    Zhao, Hongliang
    Yang, Haiou
    Huang, Weidong
    MATERIALS CHARACTERIZATION, 2024, 216
  • [50] Microstructure Characteristics of Inconel 625 Superalloy Manufactured by Selective Laser Melting
    Shuai Li
    Qingsong Wei
    Yusheng Shi
    Zicheng Zhu
    Danqing Zhang
    JournalofMaterialsScience&Technology, 2015, 31 (09) : 946 - 952