Smelting Reduction of Iron Ore-Coal Composite Pellets

被引:4
|
作者
Sah, R. [1 ]
Dutta, S. K. [2 ]
机构
[1] Smt SR Patel Engn Coll, Mehsana 384170, Gujarat, India
[2] Maharaja Sayajirao Univ Baroda, Fac Tech & Engg, Met & Mat Engg Dept, Vadodara 390001, Gujarat, India
关键词
Composite pellet; Cold bonding; Reduction; Smelting; Kinetics; dissolution; Iron ore; Coal; HEARTH FURNACE PROCESS; MOLTEN SLAG; VOLATILE REDUCTION; OXIDE REDUCTION; PREREDUCED IRON; SOLID CARBON; KINETICS; FEO; HEMATITE; MECHANISM;
D O I
10.1002/srin.200900113
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Smelting reduction of iron ore-coal composite pellets has been carried out in an induction furnace. The pellets, tied with tungsten wire, were immersed into the liquid metal bath. The experiments were carried out in the temperature range of 1713 K to 1733K. For 16-18 mm diameter pellets, it was observed that (i) the time required for complete dissolution in liquid metal bath is 83-90 seconds, (ii) the fraction of reduction for 40 seconds of immersion varied from 0.68-0.87 for Jharia coal pellets and 0.73-0.92 for Bhilai coal pellets, and (iii) the fraction of reduction increases with decreasing Fe/C ratio and increasing immersion period. X-ray diffraction (XRD)of reduced pellets showed that the reduction occurred topochemically. Scanning electron microscopic (SEM) examination of partially reduced pellets evinced the structural changes in pellets. The present investigation aims to assess the effect of Fe/C ratio in pellet, volatile matter in coal, and time of pellet immersion into liquid metal bath on reduction of iron ore-coal composite pellets.
引用
收藏
页码:426 / 433
页数:8
相关论文
共 50 条
  • [41] THERMOCHEMISTRY OF ORE-COAL PELLET REDUCTION
    KOZHEVNIKOV, IY
    GULTYAY, II
    RUSSIAN METALLURGY-METALLY-USSR, 1969, (03): : 5 - +
  • [42] Study on Direct Reduction of Low-Grade Iron Ore-Coal Mini-pellets in Coal-Based Rotary Kiln
    Liang, Zhikai
    Huang, Zhucheng
    Yi, Lingyun
    Zhong, Ronghai
    9TH INTERNATIONAL SYMPOSIUM ON HIGH-TEMPERATURE METALLURGICAL PROCESSING, 2018, : 465 - 475
  • [43] A finite control volume method for the reduction of an iron ore-coal composite pellet in an axisymmetric temperature field
    Shi, JY
    McElwain, DLS
    Donskoi, E
    CURRENT TRENDS IN SCIENTIFIC COMPUTING, 2003, 329 : 299 - 306
  • [44] Reduction kinetics of iron ore-coal pellet during fast heating
    Wang, Q.
    Yang, Z.
    Tian, J.
    Li, W.
    Sun, J.
    Ironmaking and Steelmaking, 1998, 25 (06): : 443 - 447
  • [45] Particularities in strengthening the ore-coal pellets with streams of compressed air
    Pavlovets, V.M.
    2001, Izdatel'stvo Moskovskogo Instituta Stali i Splavov
  • [46] DETERMINATION OF SPECIFIC HEAT OF ORE-COAL PELLETS DURING METALLIZATION
    STOROZHE.YI
    TELEGIN, AS
    ZAVARZIN, VP
    STEEL IN THE USSR, 1971, 1 (05): : 331 - &
  • [47] Mathematical Model to Estimate the Rate Parameters and Thermal Efficiency for the Reduction of Iron Ore-Coal Composite Pellets in Multi-layer Bed at Rotary Hearth Furnace
    Kumari, Vandana
    Roy, G. G.
    Sen, P. K.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2015, 68 (01) : 109 - 116
  • [48] Mathematical modelling of non-isothermal reduction in highly swelling iron ore-coal char composite pellet
    Donskoi, E
    McElwain, DLS
    IRONMAKING & STEELMAKING, 2001, 28 (05) : 384 - 389
  • [49] Insight of iron ore-coal composite reduction in a pilot scale rotary kiln: A post-mortem study
    Liang, Zhikai
    Yi, Lingyun
    Huang, Zhucheng
    Lu, Biao
    Jiang, Xiong
    Cai, Wei
    Tian, Baizhou
    Jin, Yunyun
    POWDER TECHNOLOGY, 2019, 356 : 691 - 701
  • [50] INVESTIGATION OF TECHNICAL PARAMETERS IN PRODUCTION OF PARTLY REDUCED ORE-COAL PELLETS
    SPEKTOR, AN
    POKHVISN.AN
    YARKHO, EN
    RUSSIAN METALLURGY, 1966, (01): : 3 - &