摘要
In this study, the basic properties of waste gypsum (WG), WG and reactive MgO-activated slag (MAS-WG) binders were experimentally explored. The effects of WG content in MAS-WG binders on the unconfined compressive strength (UCS) development of cemented paste backfill (CPB) from sulphide-rich mine tailings were investigated as well. The corresponding stabilization mechanisms were assessed through mineralogical and micro-structure analysis and leaching tests. The results showed that when the content of citric acid exceeded 0.15 wt% of WG content, the initial setting time and 28 d UCS of the WG plaster of 180 mm slump were over 1 h and 15.5 MPa, respectively. The appropriate WG incorporation improved the particle gradation of MAS-WG and MAS-WG-CPB mixtures. The main hydration products of MASWG plaster and MAS-WG-CPB from sulphide-rich tailings were crystalline CaSO4 center dot 2H(2)O, ettringite (AFt) and amorphous hydrated products (C-S-H/M-S-H). The proper WG incorporation in the MAS-WG binder also significantly enhanced the early age (14 d and 28 d) UCSs of MAS-WG plaster and MAS-WG-CPB, in which the reason is that appropriate WG incorporation accelerated the hydration process of GGBS in the alkaline solution by forming ettringite (AFt) and enhanced amorphous phase development resulting in the denser microstructure. A lot of WG incorporation made the 28 d UCSs of MAS-WG-CPB decrease due to the loose micro-structure resulted from the decrease of amorphous hydration products. However, the long-stage UCSs of MAS-WG-CPB after 120 d of curing were all stable (i.e., no strength loss) regardless of WG incorporation content, which were attributed to the low-alkalinity solution in MASWG-CPB preventing the secondary expansive hydration product formation. The long-stage (180 d) UCS of MAS-WG-CPB had positive correlations with the refined pore structure and the alkalinity of the leaching solution. (C) 2021 Elsevier Ltd. All rights reserved.
引用
收藏
页数:10
相关论文
共 50 条
  • [21] Stabilization/solidification of hexavalent chromium containing tailings using low-carbon binders for cemented paste backfill
    Zhang, Shiyu
    Zhao, Yingliang
    Guo, Zhenbang
    Ding, Hangxing
    [J]. JOURNAL OF ENVIRONMENTAL CHEMICAL ENGINEERING, 2021, 9 (01):
  • [22] Study on the Strength Development of Cemented Backfill Body from Lead-Zinc Mine Tailings with Sulphide
    Zheng, Juanrong
    Guo, Lijie
    Sun, Xiaoxiao
    Li, Wenchen
    Jia, Qi
    [J]. ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2018, 2018
  • [23] Pore and strength characteristics of cemented paste backfill using sulphide tailings: Effect of sulphur content
    Liu, Lang
    Xin, Jie
    Huan, Chao
    Qi, Chongchong
    Zhou, Wenwu
    Song, KI-IL
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2020, 237
  • [24] Dual waste utilization in cemented paste backfill using steel slag and mine tailings and the heavy metals immobilization effects
    Shi, Xiaoling
    Wang, Xiaolei
    Wang, Xiangling
    [J]. POWDER TECHNOLOGY, 2022, 403
  • [25] Utilization of Flotation Phosphate Tailings and Water Treatment Sludge in Cemented Paste Backfill Based on Phosphate Tailings
    Mei, Fu-Ding
    Li, Yan-Jie
    Hu, Chuan-Yu
    Mei, Zhi-Heng
    Ye, Feng
    [J]. SCIENCE OF ADVANCED MATERIALS, 2019, 11 (09) : 1306 - 1314
  • [26] Factors affecting natural development of soil on 35-year-old sulphide-rich mine tailings
    Néel, C
    Bril, H
    Courtin-Nomade, A
    Dutreuil, JP
    [J]. GEODERMA, 2003, 111 (1-2) : 1 - 20
  • [27] Utilization of Foaming Technology in Cemented Paste Backfill of High-Mud Superfine Unclassified Tailings
    Zhao, Jian-wen
    Wang, Xin-min
    Peng, Kang
    Li, Shuai
    [J]. ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2017, 2017
  • [28] Properties of Gobi Aggregate and Sulfide-Rich Tailings Cemented Paste Backfill and Its Application in a High-Stress Metal Mine
    Deng, D. Q.
    Liang, Y. H.
    Huangfu, F. C.
    [J]. ADVANCES IN CIVIL ENGINEERING, 2021, 2021
  • [29] Geotechnical properties of cemented paste backfill from Cannington Mine, Australia
    Rankine R.M.
    Sivakugan N.
    [J]. Geotechnical and Geological Engineering, 2007, 25 (4) : 383 - 393
  • [30] Integrated mine tailings management by combining environmental desulphurization and cemented paste backfill:: Application to mine Doyon, Quebec, Canada
    Benzaazoua, Mostafa
    Bussiere, Bruno
    Demers, Isabelle
    Aubertin, Michel
    Fried, Eliane
    Blier, Annie
    [J]. MINERALS ENGINEERING, 2008, 21 (04) : 330 - 340