Elastic-plastic deformation behavior of sapphire M-plane under static loading using nano-indentation

被引:14
|
作者
Yan, Shaohua [1 ,2 ]
Nawaz, Ahmad [3 ,4 ]
Islam, Bilal [5 ]
Qin, Qing-Hua [2 ]
Mao, Weiguo [6 ]
Shen, Yaogen [4 ]
Ahmad, Ishaq [7 ,8 ]
Hussain, Iftikhar [9 ]
机构
[1] Shenzhen Univ, Coll Phys & Optoelect Engn, Shenzhen 518060, Peoples R China
[2] Australian Natl Univ, Res Sch Elect Energy & Mat Engn, Canberra, ACT 2601, Australia
[3] Univ Technol Nowshera, Dept Mech Technol, Amangarh 24100, Kpk, Pakistan
[4] City Univ Hong Kong, Dept Mech & Biomed Engn, Kowloon, Hong Kong, Peoples R China
[5] Univ Engn & Technol Peshawar, Dept Mech Engn, Kpk 25120, Pakistan
[6] Xiangtan Univ, Minist Educ, Key Lab Low Dimens Mat & Applicat Technol, Xiangtan 411105, Hunan, Peoples R China
[7] Quaid I Azam Univ Campus, Natl Ctr Phys NCP, Expt Phys Directorate EPD, Islamabad 45320, Pakistan
[8] Northwestern Polytech Univ, Int Res Ctr Adv Nanomat & Defects Engn, Xian, Shaanxi, Peoples R China
[9] Univ Engn & Technol Peshawar, Dept Ind Engn, Kpk 25120, Pakistan
关键词
Elastic-plastic transition; Indentation size effect; Principle stresses; Maximum shear stress; Phase transformation; BRITTLE-DUCTILE TRANSITION; MECHANICAL-PROPERTIES; THIN-FILM; AL-ALLOYS; NANOINDENTATION; NANOSCALE; HARDNESS; MICROSTRUCTURE; DISLOCATIONS; MODULUS;
D O I
10.1016/j.ceramint.2021.05.069
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Elastic-plastic response of M-plane single crystal sapphire was explored via a nano-indenter with a Berkovich tip. Elastic-plastic transition was observed with eight different points (ranging from 0.30 to 0.55 mN) subject to respective peak load. Mechanical properties i.e., Oliver-Pharr hardness and elastic modulus were also determined in the onset elastic and elastic-plastic regions. Stable value of elastic modulus estimated from Oliver-Pharr nanoindentation experiments was around 430 +/- 15.0 GPa. However, Oliver-Pharr hardness in purely elastic and elastic-plastic (ISE) regions was approximately 2.19 and 2.0 times greater than the non-ISE hardness values respectively. Values of hardness in the non-ISE region were also in compliance with the depth independent hardness calculated through Nix-Gao and proportional specimen resistance models. Additionally, principal stresses and maximum shear stress were estimated on pop-in burst using Hertzian contact theory. Values of the critical resolved shear stress (CRSS) and maximum possible shear strength were also calculated at the first pop-in burst. Moreover, plastic zone size enhanced 1.36 times by shifting of critical load from 0.30 to 0.55 mN. Multiplication of Schmid factor and interplanar spacing indicated two slip systems i.e., prism {01 (11) over bar} <10<(11)over bar>> and pyramidal {11 (2) over bar0} <<(1)over bar>100>, which are verified in the Transmission electron microscopy (TEM) images. Estimated values of maximum contact pressures at respective critical loads were much lower in comparison to phase transformation pressure of sapphire. Maximum tensile stress was also calculated using Hertzian contact theory relations. Obtained value of maximum tensile strength was 3.58 times lower than cleavage fracture stress at the first pop-in.
引用
收藏
页码:23528 / 23538
页数:11
相关论文
共 50 条
  • [1] Effects of elastic-plastic properties of materials on residual indentation impressions in nano-indentation using sharp indenter
    Lee, Jung-Min
    Lee, Chan-Joo
    Lee, Kyung-Hun
    Kim, Byung-Min
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2012, 22 : S585 - S595
  • [2] Effects of elastic-plastic properties of materials on residual indentation impressions in nano-indentation using sharp indenter
    Jung-Min LEE
    Chan-Joo LEE
    Kyung-Hun LEE
    Byung-Min KIM
    Transactions of Nonferrous Metals Society of China, 2012, 22(S3) (S3) : 585 - 595
  • [4] Estimation of elastic-plastic tensile properties using nano-indentation tests and FE simulations
    Kim, Yun-Jae
    Song, Tae-Kwang
    Hanh, Jun-Hee
    Park, Jun-Hyub
    Experimental Mechanics in Nano and Biotechnology, Pts 1 and 2, 2006, 326-328 : 361 - 364
  • [5] Dislocation slip systems in c-plane and m-plane AlN single crystals under nano-indentation
    Chen, Jingjing
    Chen, Kebei
    Su, Xujun
    Niu, Mutong
    Wang, Qiqi
    Xu, Ke
    THIN SOLID FILMS, 2024, 791
  • [6] Influence of nano-indentation depth on the elastic-plastic transformation of 6H-SiC simulated
    Wu, Nanxing
    Jiang, Peng
    Zhang, Huiling
    Feng, Xiaoyu
    Zheng, Qi
    AIP ADVANCES, 2023, 13 (02)
  • [7] Elastic-Plastic Indentation and Flat Plate Rolling under Plane Strain Conditions
    Ali, M. Y.
    Pan, J.
    SAE INTERNATIONAL JOURNAL OF MATERIALS AND MANUFACTURING, 2011, 4 (01) : 125 - 137
  • [8] Elastic-plastic beam-on-foundation under quasi-static loading
    Chen, XW
    Yu, TX
    INTERNATIONAL JOURNAL OF MECHANICAL SCIENCES, 2000, 42 (12) : 2261 - 2281
  • [9] MODELING OF ELASTIC-PLASTIC DEFORMATION OF POLYCRYSTALLINE AND COMPOSITE-MATERIALS UNDER LOADING
    LEYCIN, VN
    MAKAROV, PV
    NIKOLAEV, AP
    SMOLIN, IY
    JOURNAL DE PHYSIQUE III, 1991, 1 (C3): : 949 - 954
  • [10] ELASTIC-PLASTIC DEFORMATION OF CYLINDRICAL PRESSURE-VESSELS UNDER CYCLIC LOADING
    CHANG, TY
    CHU, SC
    NUCLEAR ENGINEERING AND DESIGN, 1974, 27 (02) : 228 - 237