Oxidation behavior of C-SiC composites with a Si-W coating from room temperature to 1500°C

被引:17
|
作者
Cheng, LF [1 ]
Xu, YD [1 ]
Zhang, LT [1 ]
Gao, R [1 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
关键词
carbon-carbon composites; coating; oxidation;
D O I
10.1016/S0008-6223(00)00066-X
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Oxidation tests of carbon fiber reinforced silicon carbide composites with a Si-W coating were conducted in dry air from room temperature to 1500 degreesC for 5 h. A continuous series of empirical functions relating weight change to temperature after 5 h oxidation was found to fit the test results quite well over the whole temperature range. This approach was used to interpret the different oxidation mechanisms. There were two cracking temperatures of the matrix and the coating for the C-SIC composite. Oxidation behavior of the C-SIC composite was nearly the same as that of the coated C-C composite above the coatings cracking temperature, but weight loss of the C-SiC composite was half an order lower than that of the coated C-C composite below the cracking temperature. As an inhibitor, the SiC matrix increased the oxidation resistance of C-SiC composites by decreasing active sites available for oxidation. As an interfacial layer, pyrolytic carbon decreased the activation energy below 700 degreesC. From 800 degreesC to 1030 degreesC, uniform oxidation took place for the C-SiC composite, but non-uniform oxidation took place for the coated C-C composite in the same temperature range. The Knudsen diffusion coefficient could be used to explain the relationship between weight loss and temperature below the coating cracking temperature and the matrix cracking temperature. (C) 2000 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:2133 / 2138
页数:6
相关论文
共 50 条
  • [31] Preparation, ablation behavior and mechanism of C/C-ZrC-SiC and C/C-SiC composites
    Zhao, Zhigang
    Li, Kezhi
    Li, Wei
    Liu, Qing
    Kou, Gang
    Zhang, Yulei
    CERAMICS INTERNATIONAL, 2018, 44 (07) : 7481 - 7490
  • [32] Oxidation Resistant Behaviour of Mullite/Yttrium Silicate Multilayer Coating for C/SiC Composites at 1500 °C
    Zhao, Shuang
    Zhou, Xingui
    Wang, Honglei
    HIGH-PERFORMANCE CERAMICS VIII, 2014, 602-603 : 430 - 433
  • [33] Manufacture and Tribological Behavior of C/C-SiC Brake Composites Modified with Fe-Si Alloy
    Lu, Y-H.
    Li, Z.
    Zhou, W.
    Xiao, P.
    JOURNAL OF CERAMIC SCIENCE AND TECHNOLOGY, 2017, 8 (02): : 213 - 222
  • [34] Oxidation behavior and mechanical properties of C/SiC composites with Si-MoSi2 oxidation protection coating
    Yongdong Xu
    Laifei Cheng
    Litong Zhang
    Hongfeng Ying
    Wancheng Zhou
    Journal of Materials Science, 1999, 34 : 6009 - 6014
  • [35] Oxidation behavior and mechanical properties of C/SiC composites with Si-MoSi2 oxidation protection coating
    Xu, YD
    Cheng, LF
    Zhang, LT
    Ying, HF
    Zhou, WC
    JOURNAL OF MATERIALS SCIENCE, 1999, 34 (24) : 6009 - 6014
  • [36] Oxidation resistance behavior of SiC nanowires/Si layer on the C/SiC composites
    Wang, Bo
    Li, Jiayan
    Zhang, Fan
    He, Ping
    Shi, Wei
    Tan, Yi
    MATERIALS CHARACTERIZATION, 2023, 197
  • [38] SiC/Si-W-Mo coating for protection of C/C composites at 1873 K
    Hou, Dangshe
    Li, Kezhi
    Li, Hejun
    Fu, Qiangang
    Zhang, Yulei
    JOURNAL OF UNIVERSITY OF SCIENCE AND TECHNOLOGY BEIJING, 2008, 15 (06): : 822 - 826
  • [39] Influence of High Temperature Treatment of C/C Porous Preform on Friction and Wear Behavior of C/C-SiC Composites
    Zhang Shuo
    Fu Qiangang
    Zhang Pei
    Fei Jie
    Li Wei
    JOURNAL OF INORGANIC MATERIALS, 2023, 38 (05) : 561 - 568
  • [40] Toughening by SiC Nanowires in a Dense SiC-Si Ceramic Coating for Oxidation Protection of C/C Composites
    Chu, Yanhui
    Li, Hejun
    Fu, Qiangang
    Qi, Lehua
    Zou, Xu
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2012, 95 (11) : 3691 - 3697