Characterization of titanium-hydroxyapatite biocomposites processed by dip coating

被引:10
|
作者
Baptista, R. [1 ,4 ]
Gadelha, D. [2 ]
Bandeira, M. [2 ]
Arteiro, D. [2 ]
Delgado, M. I. [2 ]
Ferro, A. C. [3 ,5 ]
Guedes, M. [1 ,5 ]
机构
[1] Inst Politecn Setubal, Setubal Sch Technol, Dept Mech Engn, P-2910761 Setubal, Portugal
[2] Inst Politecn Setubal, Setubal Sch Technol, P-2910761 Setubal, Portugal
[3] Univ Lisbon, Inst Super Tecn, Dept Mech Engn, Av Rovisco Pais, P-1049001 Lisbon, Portugal
[4] Inst Super Tecn, IDMEC, Av Rovisco Pais, P-1049001 Lisbon, Portugal
[5] Inst Super Tecn, CeFEMA, Av Rovisco Pais, P-1049001 Lisbon, Portugal
关键词
Biocomposites; orthopaedic implants; hydroxyapatite coating; titanium substrate; dip coating; SUBSTRATE; CERAMICS;
D O I
10.1007/s12034-015-1122-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Ti orthopaedic implants are commonly coated with hydroxyapatite (HA) to achieve increased biocompatibility and osseointegration with natural bone. In this work the dip-coating technique was used to apply HA films on Ti foil. A gel was used as the support vehicle for commercial HA particles. The experimental parameters like surface roughness of the metallic substrate and immersion time were studied. All coated substrates were heat treated and sintered under vacuum atmosphere. The produced coatings were characterized by field-emission gun scanning electron microscopy coupled with energy-dispersive spectroscopy, X-ray diffraction, Raman spectroscopy, microhardness, scratch test and profilometry. Additionally, the apatite-forming ability of the produced material was tested by exposure to a simulated body fluid. Higher substrate surface roughness and longer immersion time produce thicker, denser films, with higher surface roughness. Lower film porosity is accompanied by higher hardness values. However, thicker coating promotes differential shrinkage and crack formation during sintering. Both coating thickness and coating roughness increase with coating time. HA films similar to 30-40 mu m thick with 45-50% HA theoretical density produced on Ti substrates with surface roughness of R (z)similar to 1.0-1.7 mu m, display an attractive combination of high hardness and resistance to spallation. Attained results are encouraging regarding the possibility of straightforward production of biocompatible and bioactive prosthetic coatings for orthopaedic applications using commercial HA.
引用
收藏
页码:263 / 272
页数:10
相关论文
共 50 条
  • [41] Preparation and characterization of polylactide-hydroxyapatite biocomposites
    Gültekin, N
    Tihminlioglu, F
    Çiftçioglu, R
    Çiftçioglu, M
    Harsa, S
    EURO CERAMICS VIII, PTS 1-3, 2004, 264-268 : 1953 - 1956
  • [42] Hydroxyapatite coating of titanium by biomimetic method
    A. Costantini
    G. Luciani
    F. Branda
    L. Ambrosio
    G. Mattogno
    L. Pandolfi
    Journal of Materials Science: Materials in Medicine, 2002, 13 : 891 - 894
  • [43] Electrophoretic coating of hydroxyapatite on titanium implants
    Stoch, A
    Brozek, A
    Kmita, G
    Stoch, J
    Jastrzebski, W
    Rakowska, A
    JOURNAL OF MOLECULAR STRUCTURE, 2001, 596 : 191 - 200
  • [44] Hydroxyapatite coating of titanium by biomimetic method
    Costantini, A
    Luciani, G
    Branda, F
    Ambrosio, L
    Mattogno, G
    Pandolfi, L
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 2002, 13 (09) : 891 - 894
  • [45] Surface properties in titanium with hydroxyapatite coating
    Dudek, Agata
    OPTICA APPLICATA, 2009, 39 (04) : 825 - 831
  • [46] CHARACTERISATION OF THE TITANIUM-HYDROXYAPATITE BIOCOMPATIBLE COMPOSITE LAYERS DEPOSITED BY HVOF THERMAL SPRAYING METHOD
    Rosu, Radu Alexandru
    Serban, Viorel Aurel
    Utu, Dragos
    Locovei, Cosmin
    Sfirloaga, Paula
    METAL 2011: 20TH ANNIVERSARY INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, 2011, : 711 - 716
  • [47] Effect of sintering temperature in physical-mechanical behaviour and in titanium-hydroxyapatite composite sinterability
    Weinard, W. R.
    Goncalves, F. F. R.
    Lima, W. M.
    ADVANCED POWDER TECHNOLOGY V, 2006, 530-531 : 249 - +
  • [48] INFLUENCE OF SINTERING TEMPERATURE ON THE PROPERTIES OF SOME SPARK PLASMA SINTERED TITANIUM-HYDROXYAPATITE MATERIALS
    Talpeanu, Dorinel
    Lungu, Magdalena Valentina
    Patroi, Delia
    Cojocaru, Anca
    REVISTA ROMANA DE MATERIALE-ROMANIAN JOURNAL OF MATERIALS, 2021, 51 (02): : 169 - 177
  • [49] Calcium fructoborate coating of titanium-hydroxyapatite implants by chemisorption deposition improves implant osseointegration in the femur of New Zealand White rabbit experimental model
    Varut, Renata-Maria
    Melinte, Petru Razvan
    Pirvu, Andreea Silvia
    Gingu, Oana
    Sima, Gabriela
    Oancea, Carmen Nicoleta
    Teisanu, Alina Cristina
    Dragoi, Gheorghe
    Bita, Andrei
    Manolea, Horia Octavian
    Mitrut, Ioana
    Rogoveanu, Otilia Constantina
    Scorei, Ion Romulus
    Neamtu, Johny
    ROMANIAN JOURNAL OF MORPHOLOGY AND EMBRYOLOGY, 2020, 61 (04): : 1235 - 1247
  • [50] Surface Characterization and Biocompatibility of Selenium-Doped Hydroxyapatite Coating on Titanium Alloy
    Yilmaz, Bengi
    Evis, Zafer
    Tezcaner, Aysen
    Banerjee, Sreeparna
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2016, 13 (06) : 1059 - 1068