Creep Failure and Damage Mechanism of Inconel 718 Alloy at 800-900 °C

被引:12
|
作者
Chen, Kai [1 ]
Dong, Jianxin [1 ]
Yao, Zhihao [1 ]
机构
[1] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Beijing 100083, Peoples R China
基金
中国国家自然科学基金;
关键词
Inconel; 718; Creep failure; Damage mechanism; Microstructure degradation; TENSILE DEFORMATION; DELTA-PHASE; FRACTURE CHARACTERISTICS; PRECIPITATION BEHAVIOR; HEAT-TREATMENT; EVOLUTION; MICROSTRUCTURE; STRESS;
D O I
10.1007/s12540-019-00447-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The creep behavior and damage mechanisms of 718 alloys were investigated at 800-900 degrees C in air. The fracture morphology and microstructure evolution were observed by optical, scanning and transmission electron microscope. Besides, the creep damage tolerance (lambda) and creep strain evolution curve were also calculated. The results showed that the creep curves of 718 alloys at 800 or 850 degrees C consisted of primary and tertiary stages, while the steady-state region became apparent at 900 degrees C. The apparent creep activation energy of 718 alloy was in the range from 446.3 to 491.8 kJ/mol. The alloy presented ductile fracture at 800 degrees C due to the nucleation, growth and linkage of creep voids. However, the failure of alloys at 850 or 900 degrees C presented necking to a point due to the microstructure degradation. Further investigations showed the softening of materials and the loss of mechanical performance could be mainly attributed to the coarsening or decrease of strengthening precipitates. Above 850 degrees C, it was found that gamma ' phases would dissolve into matrix and stress promoted the re-dissolution of gamma ' phases or led to the break of delta phases. Moreover, the creep strain evolution curves indicated that 718 alloys kept a relative stable state at 800-900 degrees C when the strain fraction was below 1. Graphic
引用
收藏
页码:970 / 984
页数:15
相关论文
共 50 条
  • [21] Creep feed grinding Inconel 718 with ABN 800 in vitrified bond grinding wheels
    Tuffy, Karl
    Nailer, S.
    O'Sullivan, M.
    Industrial Diamond Review, 2008, 68 (03): : 46 - 48
  • [22] Anti-oxidation properties of iron-nickel alloys at 800-900 °C
    Shi, Zhonging
    Zhao, Xingliang
    Xu, Junli
    Cao, Xiaozhou
    Wang, Zhaowen
    Gao, Bingliang
    LIGHT METALS 2008, 2008, : 1051 - +
  • [23] Creep deformation and mechanisms in Haynes 230 at 800 °C and 900 °C
    Pataky, Garrett J.
    Sehitoglu, Huseyin
    Maier, Hans J.
    JOURNAL OF NUCLEAR MATERIALS, 2013, 443 (1-3) : 484 - 490
  • [24] The influence of grain boundary character distribution on the high-temperature creep behavior and damage mechanism of Inconel 718
    Hao, Dongyang
    Wang, Qian
    Ma, Haikun
    Wu, Dayong
    Kang, Jie
    Dong, Huicong
    You, Baocai
    Li, Ning
    Su, Ru
    Materials and Design, 2024, 248
  • [25] The effect of sheet processing on the microstructure, tensile, and creep behavior of INCONEL alloy 718
    C. J. Boehlert
    D. S. Dickmann
    NY. N. C. Eisinger
    Metallurgical and Materials Transactions A, 2006, 37 : 27 - 40
  • [26] Microstructure and creep anisotropy of Inconel 718 alloy processed by selective laser melting
    Shi, J. J.
    Zhou, S. A.
    Chen, H. H.
    Cao, G. H.
    Russell, A. M.
    Zhou, Z. J.
    Qi, X. B.
    Li, C. P.
    Chen, G. F.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 805
  • [27] The effect of sheet processing on the microstructure, tensile, and creep behavior of INCONEL alloy 718
    Boehlert, CJ
    Dickmann, DS
    Eisinger, NC
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2006, 37A (01): : 27 - 40
  • [28] STUDIES ON THE ORIGIN OF THE NEAR-INFRARED (800-900 NM) ABSORPTION OF CYTOCHROME-C OXIDASE
    BEINERT, H
    SHAW, RW
    HANSEN, RE
    HARTZELL, CR
    BIOCHIMICA ET BIOPHYSICA ACTA, 1980, 591 (02) : 458 - 470
  • [29] Aging of the Inconel 718 alloy between 500 and 750 °C
    C. Slama
    C. Servant
    G. Cizeron
    Journal of Materials Research, 1997, 12 : 2298 - 2316
  • [30] CREEP-STRUCTURAL RELATIONSHIP IN STEEL ALLOY 800-H AT 900-1000-DEGREES-C
    GUTTMANN, V
    BURGEL, R
    METAL SCIENCE, 1983, 17 (11): : 549 - 555