On the effect of heat on the chemical composition and dimensions of thermally-modified wood

被引:142
|
作者
Gonzalez-Pena, Marcos M. [1 ]
Curling, Simon F. [1 ]
Hale, Michael D. C. [1 ]
机构
[1] Bangor Univ, Sch Environm & Nat Resources, Bangor LL57 2UW, Gwynedd, Wales
关键词
Beech (Fagus sylvatica L.); Chemical degradation; Heat-treatment; Mass loss; Norway spruce (Picea abies L.); Scots pine (Pinus sylvestris L.); NORWAY SPRUCE; CRYSTALLINE-STRUCTURE; BEHAVIOR; BEECH; CELLULOSE; SOFTWOOD; LIGNIN; COLOR;
D O I
10.1016/j.polymdegradstab.2009.09.003
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Heat-induced weight loss (WL) and chemical and dimensional changes of small specimens of beech (Fagus sylvatica L.), Scots pine (Pinus sylvestris L) and Norway spruce (Picea abies L) wood were examined after thermal modification in the 190-245 degrees C temperature range. Treated specimens exhibited reductions in their oven-dry weight in line with the severity of the treatment, with the effect of increasing the temperature of exposure being greater than extending the period of treatment. Wood polysaccharides were found to be distinctly more labile than the lignin constituent; the latter increased possibly as a result of repolymerisation reactions trapping some degradation products in the process. Specimens shrank in the transversal plane in a tangential to radial ratio of 2:1 regardless of the treatment regime, while their length increased marginally for WL < 10-12%. It is proposed that the thermal modification leaves the cell wall material in a permanent strained state. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2184 / 2193
页数:10
相关论文
共 50 条
  • [41] Spectroscopic studies of surface chemical composition and wettability of modified wood
    Englund, Finn
    Bryne, Lars Elof
    Ernstsson, Marie
    Lausmaa, Jukka
    Walinder, Magnus
    WOOD MATERIAL SCIENCE & ENGINEERING, 2009, 4 (1-2) : 80 - 85
  • [42] Chemical composition and bioavailability of thermally, altered Pinus resinosa (Red Pine) wood
    Baldock, JA
    Smernik, RJ
    ORGANIC GEOCHEMISTRY, 2002, 33 (09) : 1093 - 1109
  • [43] Correlation between dynamic wetting behavior and chemical components of thermally modified wood
    Wang, Wang
    Zhu, Yuan
    Cao, Jinzhen
    Sun, Wenjing
    APPLIED SURFACE SCIENCE, 2015, 324 : 332 - 338
  • [44] Colorimetry and chemical properties of thermally modified Parkia pendula and Simarouba amara wood
    De Souza, Leonardo Vinicius
    Stangerlin, Diego Martins
    De Melo, Rafael Rodolfo
    Lengowski, Elaine Cristina
    Bonfatti Junior, Eraldo Antonio
    De Vasconcelos, Leonardo Gomes
    Pimenta, Alexandre Santos
    ACTA AMAZONICA, 2024, 54 (03)
  • [45] Changes in Chemical Structure of Thermally Modified Spruce Wood Due to Decaying Fungi
    Vidholdova, Zuzana
    Kacik, Frantisek
    Reinprecht, Ladislav
    Kucerova, Viera
    Luptakova, Jana
    JOURNAL OF FUNGI, 2022, 8 (07)
  • [46] INVESTIGATION OF THE CHEMICAL CHANGES IN THE STRUCTURE OF WOOD THERMALLY MODIFIED WITH IN A NITROGEN ATMOSPEHERE AUTOCLAVE
    Hofmann, Tamas
    Retfalvi, T.
    Albert, L.
    Niemz, Peter
    WOOD RESEARCH, 2008, 53 (03) : 85 - 98
  • [47] Effect on thermal stability of microstructure and morphology of thermally-modified electrospun fibers of polybenzoxazines (PBz) blended with sulfur copolymers (SDIB)
    Parreno, Ronaldo P., Jr.
    Liu, Ying-Ling
    Beltran, Arnel B.
    RSC ADVANCES, 2021, 11 (17) : 10002 - 10009
  • [48] HARDNESS OF THERMALLY MODIFIED BEECH WOOD AND HORNBEAM WOOD
    Sedlar, Tomislav
    Sinkovic, Tomislav
    Peric, Ivana
    Jarc, Andrej
    Stojnic, Srdan
    Sefc, Bogoslav
    SUMARSKI LIST, 2019, 143 (9-10): : 425 - 433
  • [49] Sorption isotherms of thermally modified wood
    Olek, Wieslaw
    Majka, Jerzy
    Czajkowski, Lukasz
    HOLZFORSCHUNG, 2013, 67 (02) : 183 - 191
  • [50] Swelling kinetics of thermally modified wood
    Cermak, Petr
    Suchomelova, Pavlina
    Hess, Dominik
    EUROPEAN JOURNAL OF WOOD AND WOOD PRODUCTS, 2021, 79 (05) : 1337 - 1340