CO methanation on ordered mesoporous Ni-Cr-Al catalysts: Effects of the catalyst structure and Cr promoter on the catalytic

被引:127
|
作者
Liu, Qing [1 ]
Zhong, Ziyi [2 ,3 ]
Gu, Fangna [1 ]
Wang, Xiaoyan [1 ]
Lu, Xiaopeng [1 ]
Li, Huifang [1 ]
Xu, Guangwen [1 ]
Su, Fabing [1 ]
机构
[1] Chinese Acad Sci, Inst Proc Engn, State Key Lab Multiphase Complex Syst, Beijing 100190, Peoples R China
[2] Inst Chem & Engn Sci, 1 Pesek Rd, Singapore 627833, Singapore
[3] Nanyang Technol Univ, Sch Chem & Biomed Engn, 62 Nanyang Dr, Singapore 637459, Singapore
基金
中国国家自然科学基金;
关键词
CO methanation; Ordered mesoporous material; Ni-Cr-Al catalyst; Stability; WATER-GAS SHIFT; HYDROGEN-PRODUCTION; CARBON DEPOSITION; NICKEL; DECOMPOSITION; PERFORMANCE; OXIDES; RESISTANCE; KINETICS; COKING;
D O I
10.1016/j.jcat.2016.01.023
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
CO methanation is the main route in industry to produce synthetic natural gas (SNG), and the conventional Ni-based catalysts for this reaction often deactivate severely because of sintering of the Ni particles and coke formation on them. To overcome these technical barriers, we designed and synthesized a group of ternary Ni-Cr-Al metal oxide composites with ordered mesoporous structure and various Cr and Ni contents via a one-pot evaporation-induced self-assembly strategy and tested them for CO methanation to produce SNG. The support and the catalysts before and after the catalytic reaction were thoroughly characterized. It was found that, after reduction at 700 degrees C, metallic Ni particles were generated and anchored in the ordered mesoporous alumina channels while the Cr species started to surround the metallic Ni particles. The long-range ordered mesoporous structure could be maintained well when the total loading of nickel and chromium oxides was below 22 wt.%. In general, the optimized ordered mesoporous Ni-Cr-Al catalysts show much better anti-coking and anti-sintering properties and much higher catalytic activity and stability than the conventional Ni catalysts. The improved catalytic performance is attributed to the reduced Ni particle size, the confinement effect of the mesoporous materials, and the promoting effect of Cr, which can significantly reduce the Ni particle size and increase the H-2 uptake. These findings shed light on the design of ordered mesoporous alumina-supported materials with high loading of active metal oxides for many high-temperature reactions. (C) 2016 Elsevier Inc. All rights reserved.
引用
收藏
页码:221 / 232
页数:12
相关论文
共 50 条
  • [31] FORMATION OF STRUCTURE DUE TO HEATING OF AN AMORPHOUS OR ULTRA-FINE-GRAINED ALLOY NI-CR-AL
    PETROV, VA
    STROKATOV, RD
    SUKHOVAROV, VF
    IZVESTIYA VYSSHIKH UCHEBNYKH ZAVEDENII FIZIKA, 1984, 27 (09): : 104 - 105
  • [32] The influence of Ce, La, and Y promoters on the catalytic performance of Ni/Cr2O3 catalysts for CO2 methanation
    Ebrahimi, Nastaran
    Bibak, Fatemeh
    Shakeri, Mahdi
    Meshkani, Fereshteh
    JOURNAL OF MOLECULAR STRUCTURE, 2025, 1328
  • [33] CO2 methanation over Ca doped ordered mesoporous Ni-Al composite oxide catalysts: The promoting effect of basic modifier
    Xu, Leilei
    Yang, Haoming
    Chen, Mindong
    Wang, Fagen
    Nie, Dongyang
    Qi, Lu
    Lian, Xinbo
    Chen, Hanxiang
    Wu, Mei
    JOURNAL OF CO2 UTILIZATION, 2017, 21 : 200 - 210
  • [34] Effects of composite oxide supports on catalytic performance of Ni-based catalysts for CO methanation
    Zhang Han
    Dong Yunyun
    Fang Weiping
    Lian Yixin
    CHINESE JOURNAL OF CATALYSIS, 2013, 34 (02) : 330 - 335
  • [35] THERMAL-EXPANSION IN NI-CR-AL AND CO-CR-AL SYSTEMS TO 1200 DEGREESC DETERMINED BY HIGH-TEMPERATURE X-RAY-DIFFRACTION
    LOWELL, CE
    GARLICK, RG
    HENRY, B
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1976, 7 (05): : 655 - 660
  • [36] The promotion effects of Ni on the properties of Cr/Al catalysts for propane dehydrogenation reaction
    Li, Pei-Pei
    Lang, Wan-Zhong
    Xia, Ke
    Luan, Luan
    Yan, Xi
    Guo, Ya-Jun
    APPLIED CATALYSIS A-GENERAL, 2016, 522 : 172 - 179
  • [37] Catalytic activity and durability of a mesoporous silica-coated Ni-alumina-based catalyst for selective CO methanation
    Miyao, Toshihiro
    Tanaka, Junya
    Shen, Weihua
    Hayashi, Katsuhiko
    Higashiyama, Kazutoshi
    Watanabe, Masahiro
    CATALYSIS TODAY, 2015, 251 : 81 - 87
  • [38] ZrO2-modified Ni/LaAl11O18 catalyst for CO methanation: Effects of catalyst structure on catalytic performance
    Ai, Hongmei
    Yang, Hongyuan
    Liu, Qing
    Zhao, Guoming
    Yang, Jing
    Gu, Fangna
    CHINESE JOURNAL OF CATALYSIS, 2018, 39 (02): : 297 - 308
  • [39] Preparation and catalytic activity of a mesoporous silica-coated Ni-alumina-based catalyst for selective CO methanation
    Miyao, Toshihiro
    Sakurabayashi, Satoru
    Shen, Weihua
    Higashiyama, Kazutoshi
    Watanabe, Masahiro
    CATALYSIS COMMUNICATIONS, 2015, 58 : 93 - 96
  • [40] CATALYTIC PROPERTIES AND STRUCTURE OF FE-CO-CR CATALYSTS FOR EXHAUSTIVE OXIDATION OF HYDROCARBONS
    SHIBANOVA, MD
    KADENATSI, BM
    MAKSIMOV, YV
    GOLUBEV, AV
    MATVEEV, AI
    SUZDALEV, IP
    KINETICS AND CATALYSIS, 1986, 27 (01) : 174 - 179