Influence of As-Cast Microstructure on the Impact Wear Resistance of 27 mass%Cr Cast Iron

被引:7
|
作者
Ngo Huynh Kinh Luan [1 ]
Koizumi, Koreaki [1 ]
Mizuno, Kuniaki [1 ]
Yamada, Yutaka [1 ]
Okuyama, Tetsuya [2 ]
机构
[1] ITOH KIKOH Co Ltd, Tokai, Ibaraki 4760001, Japan
[2] Kurume Coll, Natl Inst Technol, Adv Engn Sch, Kurume, Fukuoka 8308555, Japan
关键词
high-chromium cast iron; as-cast microstructure; impact wear resistance; BEHAVIOR; ELEMENTS;
D O I
10.2320/matertrans.F-M2019844
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The impact wear resistance of 27 mass%Cr cast iron which as-cast microstructure influenced by cooling rate during solidification was investigated by using abrasive blasting machine. Hardness and volume fraction of martensite of samples with and without contacting with an iron chiller were measured before and after abrasive blasting test. Refinement of microstructure which was due to increase of cooling rate gave adverse effect on the impact wear resistance. Through impact of abrasive media on the surface, austenite in matrix was easy to transform into martensite, and it was obvious that there were much more micro-cracks in carbide and boundary of carbide and matrix. As volume of martensite increased, the abrasion occurred remarkably. This is explained by impingement heat generated which causes self-temper softening of martensite occur during abrasive blasting test.
引用
收藏
页码:2475 / 2480
页数:6
相关论文
共 50 条
  • [21] Effect of niobium on the as-cast microstructure of hypereutectic high chromium cast iron
    Zhi, Xiaohui
    Xing, Jiandong
    Fu, Hanguang
    Xiao, Bing
    MATERIALS LETTERS, 2008, 62 (6-7) : 857 - 860
  • [22] Effect of potassium on as-cast microstructure of a hypereutectic high chromium cast iron
    Liu Qing
    Yang Hua
    Ding Haimin
    Zhang Tian
    CHINA FOUNDRY, 2011, 8 (02) : 202 - 206
  • [23] Effect of cerium on the as-cast microstructure of a hypereutectic high chromium cast iron
    Qu, Yinhu
    Xing, Jiandong
    Zhi, Xiaohui
    Peng, Jiyun
    Fu, Hanguang
    MATERIALS LETTERS, 2008, 62 (17-18) : 3024 - 3027
  • [24] Effect of Si on the microstructure of eutectic cementite in as-cast malleable cast iron
    Zhou, Rong
    Lang, Benzhi
    Wu, Yongsheng
    Zhuzao/Foundry, 1997, (01): : 21 - 24
  • [25] Effect of potassium on as-cast microstructure of a hypereutectic high chromium cast iron
    *Liu Qing1
    2.School of Power and Mechanical Engineering
    ChinaFoundry, 2011, 8 (02) : 202 - 206
  • [26] As-cast microstructure investigation of two iron aluminides
    Schon, Claudio Geraldo
    Scuracchio, Bruno Geoffroy
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 2006, 203 (10): : 2365 - 2369
  • [27] MICROSTRUCTURE OF AS-CAST ALUMINUM BRONZE CONTAINING IRON
    HASAN, F
    IQBAL, J
    RIDLEY, N
    MATERIALS SCIENCE AND TECHNOLOGY, 1985, 1 (04) : 312 - 315
  • [28] Effect of Cu Addition on Microstructure and Hardness of As-Cast and Heat-Treated High-Cr Cast Iron
    Sarkar, Tapan
    Mukherjee, Manidipto
    Pal, Tapan Kumar
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2018, 71 (06) : 1455 - 1461
  • [29] Effect of Cu Addition on Microstructure and Hardness of As-Cast and Heat-Treated High-Cr Cast Iron
    Tapan Sarkar
    Manidipto Mukherjee
    Tapan Kumar Pal
    Transactions of the Indian Institute of Metals, 2018, 71 : 1455 - 1461
  • [30] As-cast austempered ductile cast iron
    Hui, Mengjun
    Li, Chaorong
    Liang, Ji
    Liu, Bokai
    Wu, Dehai
    Jixie goneheng Xuebao, 1988, 24 (02): : 6 - 11