Study of Al alloy corrosion in neutral NaCl by the pitting scan technique

被引:143
|
作者
Trueba, Monica [1 ]
Trasatti, Stefano P. [1 ]
机构
[1] Univ Milan, Dept Phys Chem & Electrochem, I-20133 Milan, Italy
关键词
Aluminium alloys; Single-cycle polarization; Localized corrosion; Electrochemical parameters; BINARY ALUMINUM-ALLOYS; LOCALIZED CORROSION; ELECTROCHEMICAL-BEHAVIOR; INTERGRANULAR CORROSION; HIGH-PURITY; INTERMETALLIC PHASES; CHLORIDE MEDIA; CU ALLOYS; MG ALLOY; PROTECTION;
D O I
10.1016/j.matchemphys.2010.02.022
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The corrosion behavior of commercial Al alloys was studied in neutral 0.6 mol L(-1) NaCl by using single-cycle polarization. Qualitative interpretation of pitting scans in both deaerated and naturally aerated NaCl solution, with the aid of corrosion morphology characterization, allowed for inference of the features of localized corrosion as a function of Al substrate nature. Electrochemical characteristic parameters such as pitting (E(pit)), repassivation or protection (E(prot)) potentials and pit transition potential (E(ptp)) were determined. The validity of the difference Delta E = vertical bar E(pit)-E(prot)vertical bar as criterion for susceptibility to localized corrosion of aluminium alloys is discussed. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:523 / 533
页数:11
相关论文
共 50 条
  • [21] Microstructure and pitting corrosion of partially melted zones of Al alloy GTA welds
    Rao, KS
    Rao, KP
    MATERIALS SCIENCE AND TECHNOLOGY, 2005, 21 (10) : 1199 - 1208
  • [22] Pitting corrosion of zinc in neutral halide solutions
    Assaf, FH
    Abd El-Rehiem, SS
    Zaky, AM
    MATERIALS CHEMISTRY AND PHYSICS, 1999, 58 (01) : 58 - 63
  • [23] INHIBITION OF PITTING CORROSION OF COPPER NEUTRAL MEDIA
    RYLKINA, MV
    KUSNETSOV, YI
    PROTECTION OF METALS, 1993, 29 (03): : 388 - 394
  • [24] EVALUATION OF THE CORROSION BEHAVIOR OF THE Al-356 ALLOY IN NaCl SOLUTIONS
    Vasquez Rendon, Mauricio
    Andres Calderon, Jorge
    Fernandez, Patricia
    QUIMICA NOVA, 2011, 34 (07): : 1163 - 1166
  • [25] Corrosion behaviour of Al-29at%Co alloy in aqueous NaCl
    Palcut, Marian
    Priputen, Pavol
    Kusy, Martin
    Janovec, Jozef
    CORROSION SCIENCE, 2013, 75 : 461 - 466
  • [26] Study on Corrosion Behavior of Alloy 600 in NaCl Solution
    Li Yuchun
    Zhang Fang
    Jiang Ya
    Pang Feifei
    Deng Fenfang
    Gao Fan
    ADVANCED MATERIALS, PTS 1-4, 2011, 239-242 : 2537 - 2540
  • [27] The Corrosion Behavior of Al-Cu-Li Alloy in NaCl Solution
    Wang, Ziyu
    Zhang, Peng
    Zhao, Xinsheng
    Rao, Sixian
    COATINGS, 2022, 12 (12)
  • [28] Occurrence of pitting attack in Al-Zn alloy galvanically coupled to titanium in NaCl solution
    Seri, Osami
    Sumitani, Mitsugu
    Tagashira, Kohsuke
    Keikinzoku/Journal of Japan Institute of Light Metals, 1993, 43 (06): : 303 - 307
  • [29] Chronoamperometric studies of pitting corrosion of Al and (Al-Si) alloys by halide ions in neutral sulphate solutions
    Rehim, SSA
    Hassan, HH
    Amin, MA
    CORROSION SCIENCE, 2004, 46 (08) : 1921 - 1938
  • [30] Inhibitory effect of konjac glucomanan on pitting corrosion of AA5052 aluminium alloy in NaCl solution
    Zhang, Kegui
    Yang, Wenzhong
    Xu, Bin
    Chen, Yun
    Yin, Xiaoshuang
    Liu, Ying
    Zuo, Huanzhen
    JOURNAL OF COLLOID AND INTERFACE SCIENCE, 2018, 517 : 52 - 60