Photocatalytic degradation of phenanthrene and pyrene on soil surfaces in the presence of nanometer rutile TiO2 under UV-irradiation

被引:89
|
作者
Dong, Dianbo [1 ,2 ]
Li, Peijun [1 ]
Li, Xiaojun [1 ]
Xu, Chengbin [3 ]
Gong, Dawei [4 ]
Zhang, Yinqiu [1 ,2 ]
Zhao, Qing [1 ,2 ]
Li, Peng [2 ,5 ]
机构
[1] Chinese Acad Sci, Inst Appl Ecol, Shenyang 110016, Peoples R China
[2] Chinese Acad Sci, Grad Univ, Beijing 100049, Peoples R China
[3] Liaoning Univ, Sch Environm Sci, Shenyang 110036, Peoples R China
[4] Liaoning Prov Ctr Dis Control & Prevent, Shenyang 110005, Peoples R China
[5] Chinese Acad Sci, Fujian Inst Res Struct Matter, Fuzhou 350002, Peoples R China
基金
国家高技术研究发展计划(863计划); 中国国家自然科学基金;
关键词
Nanometer rutile TiO2; Photocatalytic degradation; Phenanthrene; Pyrene; Soil surfaces; UV-irradiation; POLYCYCLIC AROMATIC-HYDROCARBONS; HUMIC SUBSTANCES; PHOTODEGRADATION; PHOTOLYSIS; MOISTURE; ATRAZINE; ACID; PHOTOCHEMISTRY; MINERALIZATION; NANOPARTICLES;
D O I
10.1016/j.cej.2009.12.046
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Photocatalytic degradation of phenanthrene and pyrene on soil surfaces in the presence of nanometer rutile TiO2 was investigated. After being spiked with phenanthrene and pyrene, soil samples loaded with different dosages of nanometer futile TiO2 (0, 1, 2, 3, and 4 wt%) were exposed to UV-irradiation for 25 h. The results indicated that the photocatalytic degradation of phenanthrene and pyrene followed the pseudo-first-order kinetics. The catalyst dosage of 2 wt% was chosen as the optimal one for further studies. According to the half-life, the degradation rate of the phenanthrene and pyrene on soil surfaces was related to their absorption spectra in soil and oxidation-half-wave-potential. In addition, the degradation of phenanthrene and pyrene increased along with increasing H2O2, light intensity and humic acids. All results indicated that the photocatalytic method in the presence of nanometer rutile TiO2 was an advisable choice for the treatments of PAHs polluted soil in the future. (C) 2010 Elsevier By. All rights reserved.
引用
收藏
页码:378 / 383
页数:6
相关论文
共 50 条
  • [11] Photocatalytic behavior of TiO2 and TiO2/CS nanoparticles under UV irradiation
    Mosquera-Vargas, Edgar
    Herrera-Molina, Daniela
    Diosa, Jesus E.
    UIS INGENIERIAS, 2022, 21 (03): : 77 - 83
  • [12] Degradation of Rhodamine B in Wastewater using Nanometer TiO2 Film under UV Light Irradiation
    Tian, Peng
    Shi, Zhenyan
    Kang, Yanhong
    Liu, Gang
    Liu, Liyan
    Zhang, Hui
    ADVANCED MATERIALS, PTS 1-4, 2011, 239-242 : 1690 - +
  • [13] Degradation of Alizarin Red Solution using Nanometer TiO2 Film under UV Light Irradiation
    Tian, Peng
    Sun, Lu
    Liu, Gang
    Kang, Yanhong
    Duan, Jidong
    Du, Wenle
    ADVANCED RESEARCH ON BIOCHEMICAL MATERIALS AND NANOTECHNOLOGY APPLICATION, 2013, 643 : 170 - +
  • [14] Degradation of Congo Red in Wastewater using Nanometer TiO2 Film under UV Light Irradiation
    Tian, Peng
    Du, Wenle
    Zheng, Zhiguo
    Lu, Jie
    Chen, Qingyang
    Sun, Lu
    ADVANCED RESEARCH ON BIOCHEMICAL MATERIALS AND NANOTECHNOLOGY APPLICATION, 2013, 643 : 178 - +
  • [15] Influence of anatase and rutile phase in TiO2 upon the photocatalytic degradation of methylene blue under solar irradiation in presence of activated carbon
    Matos, J.
    Montana, R.
    Rivero, E.
    Escudero, A.
    Uzcategui, D.
    WATER SCIENCE AND TECHNOLOGY, 2014, 69 (11) : 2184 - 2190
  • [16] PHOTOCATALYTIC DEGRADATION OF THE ORGANOPHOSPHORUS PESTICIDE FENTHION IN AQUEOUS SUSPENSIONS OF TiO2 UNDER UV IRRADIATION
    Petsas, A. S.
    Vagi, M. C.
    Kostopoulou, M. N.
    Lekkas, T. D.
    PROCEEDINGS OF THE 13TH INTERNATIONAL CONFERENCE ON ENVIRONMENTAL SCIENCE AND TECHNOLOGY, 2013,
  • [17] Photocatalytic Degradation of Methylene Blue under UV Light Irradiation on Prepared Carbonaceous TiO2
    Ramli, Zatil Amali Che
    Asim, Nilofar
    Isahak, Wan N. R. W.
    Emdadi, Zeynab
    Ahmad-Ludin, Norasikin
    Yarmo, M. Ambar
    Sopian, K.
    SCIENTIFIC WORLD JOURNAL, 2014,
  • [18] PHOTOCATALYTIC DEGRADATION OF PYRENE IN POROUS Pt/TiO2-SiO2 PHOTOCATALYST SUSPENSION UNDER UV IRRADIATION
    Luo, Zhaohui
    Katayama-Hirayama, Keiko
    Hirayama, Kimiaki
    Akitsu, Tetsuya
    Kaneko, Hidehiro
    NANO, 2008, 3 (05) : 317 - 322
  • [19] Photocatalytic degradation of methamidophos by UV irradiation in the presence of nano-TiO2
    Zhang, Lei
    Yan, Fei
    Wang, Yingnan
    Guo, Xingjia
    Zhang, Peng
    INORGANIC MATERIALS, 2006, 42 (12) : 1379 - 1387
  • [20] Photocatalytic degradation of methamidophos by UV irradiation in the presence of nano-TiO2
    Lei Zhang
    Fei Yan
    Yingnan Wang
    Xingjia Guo
    Peng Zhang
    Inorganic Materials, 2006, 42 : 1379 - 1387