Metal-support interactions in Pt/Al2O3 and Pd/Al2O3 catalysts for CO oxidation

被引:342
|
作者
Ivanova, A. S. [1 ]
Slavinskaya, E. M. [1 ]
Gulyaev, R. V. [1 ]
Zaikovskii, V. I. [1 ]
Stonkus, O. A. [2 ]
Danilova, I. G. [1 ]
Plyasova, L. M. [1 ]
Polukhina, I. A. [1 ]
Boronin, A. I. [1 ,2 ]
机构
[1] Boreskov Inst Catalysis SB RAS, Novosibirsk 630090, Russia
[2] Novosibirsk State Univ, Novosibirsk 630090, Russia
关键词
Supported catalysts; Alumina; Palladium; Platinum; CO oxidation; SMSI; HRTEM; XPS; TPR-H-2; Catalysis; SURFACE ELEMENTARY STEPS; RAY PHOTOELECTRON-SPECTROSCOPY; PALLADIUM-ALUMINA CATALYSTS; LOW-LOADED PALLADIUM; LIGHTING-OFF TESTS; INFRARED-SPECTROSCOPY; ELECTRON-MICROSCOPY; METHANE COMBUSTION; SILVER CATALYSTS; GAMMA-ALUMINA;
D O I
10.1016/j.apcatb.2010.03.024
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Platinum and palladium catalysts supported on gamma-Al203 were studied by XRD, UV-vis DRS, HRTEM. TPR-H-2, XPS together with measurements of their catalytic properties. The properties of the catalysts denoted as Pt(Pd)/Al2O3(X)-Y (X-the calcination temperature of support. degrees C. Y-the calcination temperciture of catalyst, C) were studied as a function of the temperatures used for calcination of the support and/or the catalyst in oxygen or in a reaction mixture of CO + O-2 It was found that the deposition of Pt or Pd on gamma-Al2O3 did not alter the structure of the support Two types of the Pt and Pd particles were typically present on the gamma-Al2O3 surface individual particles with dimensions of 1 5-3 nm and agglomerates about 100 nm in size In the catalysis calcined at relatively low temperatures (Pt/Al2O3(550)-450). platinum was present in the form of metal clusters However, in the Pd/Al2O3(550)-450 catalyst, the palladium particles were almost completely decorated with a thin layer of an alummate phase These structures are not reduced in hydrogen in the temperature range of -15 to 450 degrees C, and are stable to treatment in a reaction mixture of CO + O-2. Pd deposition on the gamma-Al2O3-800 support was found to result in stabilization of the active component in two main forms. Pd and PdO. with varying degrees of interaction due to the decoration effect Calcination at the low temperature of 550 degrees C led to the formation of a so-called "core-shell structure", where a palladium metal core is covered with a thin shell of an alummate phase Depending on the calcination temperature of the catalyst in the range of 450-1000 degrees C, the morphological form of the active component was converted from the "core-shell" state to a state consisting of two phases. Pd-o and PdO. with a gradual decrease of the Pd-o/PdO ratio, weakening the interaction with the support and the growth of palladium particles. Under the action of the reaction mixture, the Pd/Al2O3(800)-(450,600,800.1000) catalysts underwent changes in the Pd-o/PdO ratio, which regulates the light-off temperature After catalyst calcination at the highest temperature used in this study. 1200 degrees C. the palladium particles became much larger due to the loss of the palladium interaction with the support Only the metal phase of palladium was observed in these catalysts, and their catalytic activity decreases substantially. (C) 2010 Elsevier B.V All rights reserved
引用
收藏
页码:57 / 71
页数:15
相关论文
共 50 条
  • [31] Performance of Pt/Cr2O3, Pt/ZrO2, and, Pt/γ-Al2O3 Catalysts in Total Oxidation of Methane: Effect of Metal-Support Interaction
    Corro, Grisel
    Cruz-Merida, Jorge
    Montalvo, Daniel
    Pal, Umapada
    INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2021, 60 (51) : 18841 - 18852
  • [32] Selective Electrocatalytic Hydrogenation of Linolenic Acid on Pd/Al2O3 and Pd-Co/Al2O3 Catalysts
    Breton, Sylvie
    Brisach-Wittmeyer, Anne
    Rios Martin, Jose Julian
    Leon Camacho, Manuel
    Lasia, Andrzej
    Menard, Hugues
    INTERNATIONAL JOURNAL OF ELECTROCHEMISTRY, 2011, 2011
  • [33] Electrochemically Synthesized Pt/Al2O3 Oxidation Catalysts
    Dmitry E. Doronkin
    Aleksandra B. Kuriganova
    Igor N. Leontyev
    Sina Baier
    Henning Lichtenberg
    Nina V. Smirnova
    Jan-Dierk Grunwaldt
    Catalysis Letters, 2016, 146 : 452 - 463
  • [34] THE PARTICIPATION OF AL2O3 HYDROXYL COVERAGE OXYGEN IN THE REACTION OF CARBON-MONOXIDE OXIDATION ON PD/AL2O3 AND PD.CU/AL2O3 CATALYSTS
    GELBSHTEIN, AI
    MISHCHENKO, IA
    DULIN, DA
    KOLOTYRKIN, IJ
    KAKHNIASHVILI, GN
    DOKLADY AKADEMII NAUK SSSR, 1985, 284 (04): : 900 - 903
  • [35] Reduction of stored NOx on Pt/Al2O3 and Pt/BaO/Al2O3 catalysts with H2 and CO
    Szailer, T
    Kwak, JH
    Kim, DH
    Hanson, JC
    Peden, CHF
    Szanyi, J
    JOURNAL OF CATALYSIS, 2006, 239 (01) : 51 - 64
  • [36] Reactivation of sintered Pt/Al2O3 oxidation catalysts
    Galisteo, FC
    Mariscal, R
    Granados, ML
    Fierro, JLG
    Daley, RA
    Anderson, JA
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2005, 59 (3-4) : 227 - 233
  • [37] Electrochemically Synthesized Pt/Al2O3 Oxidation Catalysts
    Doronkin, Dmitry E.
    Kuriganova, Aleksandra B.
    Leontyev, Igor N.
    Baier, Sina
    Lichtenberg, Henning
    Smirnova, Nina V.
    Grunwaldt, Jan-Dierk
    CATALYSIS LETTERS, 2016, 146 (02) : 452 - 463
  • [38] RADIAL PROFILES IN PT/AL2O3, RE/AL2O3, AND PT-RE/AL2O3
    DEMIGUEL, SR
    SCELZA, OA
    CASTRO, AA
    BARONETTI, GT
    ARDILES, DR
    PARERA, JM
    APPLIED CATALYSIS, 1984, 9 (03): : 309 - 315
  • [39] Size effect of γ-Al2O3 supports on the catalytic performance of Pd/γ-Al2O3 catalysts for HCHO oxidation
    Xiang, Ning
    Han, Xiaojin
    Bai, Yarong
    Li, Qiaoyan
    Zheng, Jianfeng
    Li, Yulin
    Hou, Yaqin
    Huang, Zhanggen
    MOLECULAR CATALYSIS, 2020, 494
  • [40] Oxidation of CO and Propane on Pt-Au/Al2O3 Catalysts
    Ruszel, M.
    Grzybowska-Swierkosz, B.
    Karpinski, Z.
    Juszczyk, W.
    POLISH JOURNAL OF CHEMISTRY, 2008, 82 (10) : 1991 - 1997