Effect of temperature and hydrogen concentration on the threshold stress intensity factor of radial delayed hydride cracking in fuel cladding

被引:7
|
作者
Colldeweih, Aaron W. [1 ]
Bertsch, Johannes [1 ]
机构
[1] Paul Scherrer Inst, Lab Nucl Mat LNM, Villigen, Switzerland
基金
英国工程与自然科学研究理事会;
关键词
TERMINAL SOLID SOLUBILITY; ZIRCONIUM; EMBRITTLEMENT; ZIRCALOY-2; DIRECTION; GROWTH;
D O I
10.1016/j.jnucmat.2022.153737
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Three-point bending tests provide the ability to measure the propagation of axially oriented cracks in thin-walled fuel cladding in a radial outside-in direction. Via three-point bending, unirradiated Zircaloy-2 cladding containing 155 and 305 wppm hydrogen was mechanically loaded at different temperatures, sufficient to initiate delayed hydride cracking (DHC) whereupon the unloading rate was fast enough to arrest further propagation. The crack front dimensions were measured through fractography and implemented with the final load into a finite element model (FEM). Given the average crack length and final load, the FEM was able to back-calculate the stress intensity factor. Over a temperature range of 210-330 degrees C, around 6 MPa root m was calculated as the minimum threshold stress intensity factor for DHC. The trend shows that the ideal temperature for DHC with lowest threshold stress intensity factors may depend on the hydrogen concentration, and that the threshold stress intensity factors quickly increase with higher test temperatures. It has also been shown that creep affects the threshold stress intensity factor for optimal DHC less for lower hydrogen concentrations than for higher hydrogen concentrations. At low hydrogen concentration, the temperature of terminal solid solubility for precipitation (TSSP) is low enough so that creep-induced crack tip rounding plays a less significant role compared to the hydrogen kinetics. (C) 2022 The Authors. Published by Elsevier B.V.
引用
收藏
页数:11
相关论文
共 50 条
  • [31] Anisotropic threshold stress intensity factor, KIH and crack growth rate in delayed hydride cracking of Zr-2.5Nb pressure tubes
    Young Suk Kim
    Sung Soo Kim
    Sang Chul Kwon
    Yong Moo Cheong
    Kyung Soo Im
    [J]. Metallurgical and Materials Transactions A, 2002, 33 : 919 - 925
  • [32] Effect of Variable Stress Intensity Factor on Hydrogen Environment Assisted Cracking
    Hall, M. M., Jr.
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2011, 42A (02): : 304 - 318
  • [33] Effect of Variable Stress Intensity Factor on Hydrogen Environment Assisted Cracking
    M.M. Hall
    [J]. Metallurgical and Materials Transactions A, 2011, 42 : 304 - 318
  • [34] An assessment of delayed hydride cracking in zirconium alloy cladding tubes under stress transients
    Chan, K. S.
    [J]. INTERNATIONAL MATERIALS REVIEWS, 2013, 58 (06) : 349 - 373
  • [35] HYDROGEN-CONTROLLED CRACKING - APPROACH TO THRESHOLD STRESS INTENSITY
    GERBERICH, WW
    CHEN, YT
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1975, 6 (02): : 271 - 278
  • [36] Measurements of delayed hydride cracking propagation rate in the radial direction of Zircaloy-2 cladding tubes
    Kubo, T.
    Kobayashi, Y.
    Uchikoshi, H.
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2012, 427 (1-3) : 18 - 29
  • [37] Influence of temperature and hydrogen content on stress-induced radial hydride precipitation in Zircaloy-4 cladding
    Desquines, J.
    Drouan, D.
    Billone, M.
    Puls, M. P.
    March, P.
    Fourgeaud, S.
    Getrey, C.
    Elbaz, V.
    Philippe, M.
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2014, 453 (1-3) : 131 - 150
  • [38] A study on the effects of hydrogen content and peak temperature on threshold stress for hydride reorientation in Zircaloy-4 cladding
    Lee, Ji-Min
    Kim, Ho-A.
    Kook, Dong-Hak
    Kim, Yong-Soo
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2018, 509 : 285 - 294
  • [39] Delayed-hydride cracking (DHC) of cladding materials: An analysis for storage and disposal of spent nuclear fuel
    Ahn, Tae M.
    [J]. NUCLEAR ENGINEERING AND DESIGN, 2019, 350 : 128 - 136
  • [40] HYDROGEN CONCENTRATION LIMIT AND CRITICAL-TEMPERATURES FOR DELAYED HYDRIDE CRACKING IN ZIRCONIUM ALLOYS
    SHI, SQ
    SHEK, GK
    PULS, MP
    [J]. JOURNAL OF NUCLEAR MATERIALS, 1995, 218 (02) : 189 - 201