Two distinct fracture modes of copper alloys in fluoride environments

被引:7
|
作者
Chen, YY [1 ]
Tzou, RJ [1 ]
Chang, YS [1 ]
Wang, LH [1 ]
Oung, JC [1 ]
Shih, HC [1 ]
机构
[1] Natl Tsing Hua Univ, Dept Mat Sci & Engn, Hsinchu 300, Taiwan
关键词
stress corrosion cracking; aluminum brass; aluminum bronze; slow strain rate technique; transgranular; intergranular;
D O I
10.1016/j.corsci.2004.05.010
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The susceptibility of aluminum brass and aluminum bronze to stress corrosion cracking (SCC) was evaluated in fluoride environments by means of the slow strain rate technique. The effects of fluoride concentration and applied electrochemical potential on the SCC susceptibility were investigated. The SCC mechanism of aluminum brass was found to be dependent upon the de-alloying phenomenon while that of aluminum bronze on the film-rupture mechanism occurring within a certain range of applied electrochemical potentials. For aluminum brass, both the stress ratio and the time-to-fracture ratio were closely related to the logarithmic concentration of F- ions. The fracture modes were ductile dimpled tearing fracture for the aluminum brass at the corrosion potential while intergranular for the aluminum bronze at various anodic potentials. The micro-galvanic effects of the constituent elements were used to estimate the anodic equilibrium potentials of the two alloys. (C) 2004 Elsevier Ltd. All rights reserved.
引用
收藏
页码:79 / 93
页数:15
相关论文
共 50 条
  • [31] Distinct Reactivity Modes of a Copper Hydride Enabled by an Intramolecular Lewis Acid
    Norwine, Emily E.
    Kiernicki, John J.
    Zeller, Matthias
    Szymczak, Nathaniel K.
    JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2022, 144 (33) : 15038 - 15046
  • [32] Corrosion of copper-nickel alloys in simulated vapourside environments
    Al-Subaie, KZ
    Hodgkiess, T
    DESALINATION, 2003, 158 (1-3) : 43 - 50
  • [33] APPLICATION OF COPPER-ALUMINUM ALLOYS IN POTASH AND ALKALI ENVIRONMENTS
    MEDLEY, DF
    CIM BULLETIN, 1982, 75 (845): : 61 - 61
  • [34] HYDROGEN EFFECTS ON THE PROPERTIES AND FRACTURE MODES OF IRON-BASED ALLOYS
    MOODY, NR
    ROBINSON, SL
    GARRISON, WM
    RES MECHANICA, 1990, 30 (02): : 143 - 206
  • [35] ALL MODES FRACTURE-TOUGHNESS OF 2 ALUMINUM-ALLOYS
    TSANGARAKIS, N
    ENGINEERING FRACTURE MECHANICS, 1987, 26 (03) : 313 - &
  • [36] Surface tension and density of copper–Zirconium alloys in contact with fluoride refractories
    V. P. Krasovskyy
    Y. V. Naidich
    N. A. Krasovskaya
    Journal of Materials Science, 2005, 40 : 2367 - 2369
  • [37] Kinematics of persistent random walkers with two distinct modes of motion
    Shaebani, M. Reza
    Rieger, Heiko
    Sadjadi, Zeinab
    PHYSICAL REVIEW E, 2022, 106 (03)
  • [38] Two distinct modes of protein-induced bending in DNA
    El Hassan, MA
    Calladine, CR
    JOURNAL OF MOLECULAR BIOLOGY, 1998, 282 (02) : 331 - 343
  • [39] Two distinct modes of control for object-directed action
    Goodale, MA
    Westwood, DA
    Milner, AD
    ROOTS OF VISUAL AWARENESS: A FESTSCHRIFT IN HONOR OF ALAN COWEY, 2003, 144 : 131 - 144
  • [40] Two distinct anion-binding modes and their relative stabilities
    Kim, Nam-Kyun
    Chang, Kyoung-Jin
    Moon, Dohyun
    Lah, Myoung Soo
    Jeong, Kyu-Sung
    CHEMICAL COMMUNICATIONS, 2007, (32) : 3401 - 3403