Thickness impacts on permeation reduction factor of Er2O3 hydrogen isotopes permeation barriers prepared by magnetron sputtering

被引:25
|
作者
Li, Qun [1 ]
Wang, Jie [1 ]
Xiang, Qing-Yun [1 ]
Tang, Tao [2 ]
Rao, Yong-Chu [2 ]
Cao, Jiang-Li [1 ]
机构
[1] Univ Sci & Technol Beijing, Inst Adv Mat & Technol, Beijing 100083, Peoples R China
[2] China Acad Engn Phys, POB 919-71, Mianyang 621907, Sichuan, Peoples R China
关键词
Er2O3-HIPB; Hydrogen energy; Deuterium invasion; Coating crack; THIN-FILMS; ERBIUM OXIDE; TRITIUM PERMEATION; STAINLESS-STEEL; DEUTERIUM PERMEATION; THERMAL-EXPANSION; SOL-GEL; IN-SITU; COATINGS; STRESSES;
D O I
10.1016/j.ijhydene.2015.11.046
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In hydrogen energy and thermal fusion energy, hydrogen isotopes permeation barriers (HIPB) are used to reduce hydrogen isotopes permeation, which may result in hydrogen isotopes leak and construction materials brittleness. Here, we made Er2O3 HIPB by magnetron sputtering and studied the relation between deuterium-permeation reduction factor (D-PRF) and coating thickness, micro-morphology. The 0.2 mu m Er2O3 coatings can reduce deuterium permeation by 1/10 similar to 1/20 at 600 degrees C similar to 300 degrees C. However, the reduction ability decreases gradually with the increase in coating thickness when the coatings are thicker than 0.2 mu m. The reason may be ascribed to the deuterium invasion in deuterium permeation test. After deuterium invasion into coatings, the coatings suffer intrinsic stress, thermal stress and expansion stress from deuterium invasion. As a result of grain size dependence on coating thickness in PVD-derived coatings, i.e. grains become coarse with increasing coating thickness, the sum of stresses in various type increases with increasing coating thickness. The coatings crack easily when they suffer more strong tensile stress. So, the damages of coatings become serious and D-PRF reduces with increasing coating thickness. Copyright (C) 2015, Hydrogen Energy Publications, LLC. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:3299 / 3306
页数:8
相关论文
共 50 条
  • [31] Fe effect on hydrogen interactions with intrinsic point defects and hydrogen migration in α-Al2O3 based tritium permeation barriers
    Xiang, Xin
    Zhu, Ligui
    Yang, Feilong
    Hu, Li
    Zhang, Guikai
    JOURNAL OF NUCLEAR MATERIALS, 2020, 542
  • [32] Effect of film thickness on photoelectric properties of β-Ga2O3 films prepared by radio frequency magnetron sputtering
    Li Xiu-Hua
    Zhang Min
    Yang Jia
    Xing Shuang
    Gao Yue
    Li Ya-Ze
    Li Si-Yu
    Wang Chong-Jie
    ACTA PHYSICA SINICA, 2022, 71 (04)
  • [33] Tritium permeation characterization of Al2O3/FeAl coatings as tritium permeation barriers on 321 type stainless steel containers
    Yang, Feilong
    Xiang, Xin
    Lu, Guangda
    Zhang, Guikai
    Tang, Tao
    Shi, Yan
    Wang, Xiaolin
    JOURNAL OF NUCLEAR MATERIALS, 2016, 478 : 144 - 148
  • [34] Evaluation of hydrogen permeation on Al2O3-PZT composite membrane
    Kim, Kyeong-Ii
    Ju, Hyun-Chul
    Kim, Dong-Min
    Kim, Whan-Gi
    Hong, Tae-Whan
    SOLID STATE IONICS, 2012, 225 : 712 - 715
  • [35] Study of α-Al2O3 about hydrogen permeation resistance and micromechanism
    Li Lei
    Sang Ge
    Zhang, Peng-Cheng
    Jiang Gang
    ACTA PHYSICO-CHIMICA SINICA, 2007, 23 (12) : 1912 - 1916
  • [36] Preparation of Cr2O3 film by MOCVD as hydrogen permeation barrier
    He, Di
    Li, Shuai
    Liu, Xiaopeng
    Zhang, Chao
    Yu, Qinghe
    Wang, Shumao
    Jiang, Lijun
    FUSION ENGINEERING AND DESIGN, 2014, 89 (01) : 35 - 39
  • [37] Simulation of thermal stress in Er2O3 and Al2O3 tritium penetration barriers by finiteelement analysis
    Liu, Ze
    Wang, Yuan
    Yu, Guogang
    He, Anping
    Wang, Ling
    PLASMA SCIENCE & TECHNOLOGY, 2017, 19 (09)
  • [38] Microstructure, hardness and optical properties of Er2O3 films deposited on diamond-coated and Si(100) substrates by radio frequency magnetron sputtering
    Huang, Yabo
    Chen, Liangxian
    Jia, Xin
    Shao, Mingyang
    Shao, Siwu
    Zhu, Xiaohua
    An, Kang
    Liu, Jinlong
    Wei, Junjun
    Li, Chengming
    THIN SOLID FILMS, 2020, 709
  • [39] The Role of Carbon in the Formation of Intrinsic Point Defects and Hydrogen Migration in α-Al2O3-Based Tritium Permeation Barriers
    Xiang, Xin
    Yang, Feilong
    Hu, Li
    Zhang, Guikai
    Chen, Chang'an
    PHYSICA STATUS SOLIDI B-BASIC SOLID STATE PHYSICS, 2022, 259 (11):
  • [40] Efficient hydrogen and deuterium permeation reduction in Al2O3 coatings with enhanced radiation tolerance and corrosion resistance
    Iadicicco, D.
    Bassini, S.
    Vanazzi, M.
    Munoz, P.
    Morono, A.
    Hernandez, T.
    Garcia-Cortes, I
    Sanchez, F. J.
    Utili, M.
    Ferre, F. Garcia
    Di Fonzo, F.
    NUCLEAR FUSION, 2018, 58 (12)