LAFAD Hard Ceramic and Cermet Coatings for Erosion Protection of Turbomachinery Components

被引:0
|
作者
Gorokhovsky, Vladimir
Bowman, Chris
Wallace, John
VanVorous, Dave
O'Keefe, John
Champagne, Victor
Pepi, Marc
Tabakoff, Widen
机构
关键词
DEPOSITION; TIN;
D O I
暂无
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
To mitigate costly surface damage, compressor blades are coated with materials that resist corrosion and resist wear from particle impact Large Area Filtered Arc Deposition (LAFAD) technology has demonstrated the capability of depositing relatively thick cermet coatings with microlaminated architectures forming a stack of metallic/ceramic bi-layers These coatings have nearly defect-free morphology and an extremely smooth surface with high surface energy, which improves the aerodynamics of airfoils. Yet, the deposition process can be earned out at a speed that produces coatings sufficiently thick to provide long life protection from particle damage at a cost-effective production rate. The basic mechanical properties and erosion resistance of LAFAD microlaminated cermet coatings deposited on Ti6Al4V and 17-4PH steel substrates have been investigated as a function of coating composition and architecture.
引用
收藏
页码:807 / 817
页数:11
相关论文
共 50 条
  • [21] DEVELOPMENT OF COATINGS FOR CORROSION/EROSION PROTECTION OF INTERNAL COMPONENTS OF COAL GASIFICATION VESSELS.
    Anon
    Annual Conference on Materials for Coal Conversion and Utilization (Proceedings), 1979,
  • [22] Friction and wear mechanisms of thermally sprayed ceramic and cermet coatings
    Laboratoire d'Etudes et de Recherches sur les Materiaux et Propriétés de Surfaces, IPSé, BP 449, 90010 Belfort, Cedex, France
    不详
    Surf. Coat. Technol., 2-3 (255-262):
  • [23] DEVELOPMENT OF COATINGS FOR CORROSION/EROSION PROTECTION OF INTERNAL COMPONENTS FOR COAL GASIFICATION VESSELS.
    Anon
    Annual Conference on Materials for Coal Conversion and Utilization (Proceedings), 1979,
  • [24] Study on the Use of Elastomeric Coatings for Protection of Hydraulic Turbine Components Against Cavitation Erosion
    Frunzaverde, Doina
    Ciubotariu, Costel Relu
    Secosan, Evelina Roxana
    Campian, Constantin Viorel
    Fanica, Cristian
    MATERIALE PLASTICE, 2016, 53 (03) : 557 - 560
  • [25] Evaluation of Ceramic Hard Thin Coatings
    Iwai, Yoshiro
    Matsubara, Toru
    JOURNAL OF JAPANESE SOCIETY OF TRIBOLOGISTS, 2010, 55 (08) : 556 - 562
  • [26] Friction and wear mechanisms of thermally sprayed ceramic and cermet coatings
    Fervel, V
    Normand, B
    Liao, H
    Coddet, C
    Bêche, E
    Berjoan, R
    SURFACE & COATINGS TECHNOLOGY, 1999, 111 (2-3): : 255 - 262
  • [27] Erosion Resistance of Cermet Coatings Deposited by Supersonic Atmospheric Plasma Spraying
    Yu Fangli
    Bai Yu
    Xie Hui
    Liu Yinchao
    Wang Haijun
    Wu Jiuhui
    RARE METAL MATERIALS AND ENGINEERING, 2018, 47 (06) : 1884 - 1889
  • [28] Erosion-oxidation behavior of thermal sprayed steels and cermet coatings
    Kunioshi, CT
    Correa, OV
    Ramanathan, LV
    SURFACE ENGINEERING IN MATERIALS SCIENCE III, 2005, : 255 - 265
  • [29] THE WEAR AND EROSION RESISTANCE OF HARD PVD COATINGS
    RICKERBY, DS
    BURNETT, PJ
    SURFACE & COATINGS TECHNOLOGY, 1987, 33 (1-4): : 191 - 211
  • [30] SUPERSONIC RAIN EROSION RESISTANT CERAMIC COATINGS
    WALTON, JD
    AMERICAN CERAMIC SOCIETY BULLETIN, 1970, 49 (08): : 744 - &