摘要
For the thermal and thermooxidative degradation in fullerene (C-60, C-70)-Polymer (PMMA, polystyrene) systems, concentration limits were observed for the stabilizing effect of fullerenes that depend on the solubility of the fullerene in a polymer: for polystyrene and PMMA, these values are 4 x 10(-3) and 8 x 10(-3) Mol/kg of fullerene, respectively. Thermal and thermooxidative degradation occurred in the presence of fullerenes were also characterized by the existence of temperature limits for the effective action of inhibitors. For polystyrene-based systems containing C-60 or C-70, the temperature limit of thermal degradation was 380degreesC; for PMMA-based systems, this parameter amounted to 339 and 336degreesC for C-60 and C-70, respectively. For the thermooxidative degradation of these polymers and a polycarbonate, the temperature range 335-340degreesC was the highest temperature limit for fullerene C-60 as an antioxidant, which was much lower than 370degreesC, the temperature corresponding to the onset of the intense oxidation of fullerene.
引用
收藏
页码:951 / 956
页数:6
相关论文
共 50 条
  • [31] Ozone addition to C60 and C70 fullerenes: A DFT study
    Sabirov, D. Sh.
    Khursan, S. L.
    Bulgakov, R. G.
    JOURNAL OF MOLECULAR GRAPHICS & MODELLING, 2008, 27 (02): : 124 - 130
  • [32] Synthesis and structure of allylated derivatives of fullerenes C60 and C70
    Gubskaya, V. P.
    Islamova, L. N.
    Fazleeva, G. M.
    Latypov, Sh. K.
    Saifina, A. F.
    Gubaidullin, A. T.
    Sharafutdinova, D. R.
    Nuretdinov, I. A.
    Sinyashin, O. G.
    RUSSIAN CHEMICAL BULLETIN, 2016, 65 (06) : 1556 - 1565
  • [33] THE HEAT OF FORMATION AND THE BOND LENGTHS FOR THE FULLERENES - C60 AND C70
    IONOV, SP
    ALIKHANYAN, AS
    SPITSYNA, NG
    YARZHEMSKY, VG
    DOKLADY AKADEMII NAUK, 1993, 331 (04) : 449 - 451
  • [34] Simultaneous determination of C60 and C70 fullerenes by a spectrophotometric method
    Çiçek, B
    Kenar, A
    Nazir, H
    FULLERENE SCIENCE AND TECHNOLOGY, 2001, 9 (01): : 103 - 111
  • [35] Structural organization of fullerenes C60, C70, C84
    Saint-Gregoire, P
    Almairac, R
    Snoeck, E
    Moret, J
    Kopsky, V
    FERROELECTRICS, 1999, 221 (1-4) : 37 - 46
  • [36] Technology for manufacture of pure fullerenes C60, C70 and a concentrate of higher fullerenes
    Grushko, Yu. S.
    Sedov, V. P.
    Shilin, V. A.
    RUSSIAN JOURNAL OF APPLIED CHEMISTRY, 2007, 80 (03) : 448 - 455
  • [37] Natural frequencies of C60, C70, and C80 fullerenes
    Sakhaee-Pour, A.
    Vafai, A.
    APPLIED PHYSICS LETTERS, 2010, 96 (02)
  • [38] LANGMUIR-BLODGETT-FILMS OF THE FULLERENES C70 AND C60
    WILLIAMS, G
    MOORE, AJ
    BRYCE, MR
    LVOV, YM
    PETTY, MC
    SYNTHETIC METALS, 1993, 56 (2-3) : 2955 - 2960
  • [39] Structure, dynamics and optical properties of fullerenes C60, C70
    Prilutski, YI
    Buzaneva, EV
    Bulavin, LA
    Scharff, P
    CARBON, 1999, 37 (05) : 835 - 838
  • [40] Electron energy loss spectra of C60 and C70 fullerenes
    Lee, SM
    Nicholls, RJ
    Nguyen-Manh, D
    Pettifor, DG
    Briggs, GAD
    Lazar, S
    Pankhurst, DA
    Cockayne, DJH
    CHEMICAL PHYSICS LETTERS, 2005, 404 (1-3) : 206 - 211