High catalytic performance of Fe-Ni/Palygorskite in the steam reforming of toluene for hydrogen production

被引:94
|
作者
Zou, Xuehua [1 ,2 ]
Chen, Tianhu [1 ]
Zhang, Ping [3 ]
Chen, Dong [1 ]
He, Junkai [4 ]
Dang, Yanliu [4 ]
Ma, Zhiyuan [1 ]
Chen, Ye [1 ]
Toloueinia, Panteha [2 ]
Zhu, Chengzhu [1 ]
Xie, Jingjing [1 ]
Liu, Haibo [1 ]
Suib, Steven L. [2 ,4 ]
机构
[1] Hefei Univ Technol, Sch Resources & Environm Engn, Lab Nanominerals & Environm Mat, Hefei 230009, Anhui, Peoples R China
[2] Univ Connecticut, Dept Chem, Storrs, CT 06269 USA
[3] Chinese Acad Sci, Guangzhou Inst Geochem, Guangzhou, Guangdong, Peoples R China
[4] Univ Connecticut, Inst Mat Sci, Storrs, CT 06269 USA
关键词
Fe-Ni/Palygorskite catalyst; Awaruite (Ni-Fe alloy); Steam reforming; Toluene; Biomass tar; Kinetic study; NICKEL-BASED CATALYST; FLUIDIZED-BED GASIFICATION; BIOMASS GASIFICATION; MODEL-COMPOUND; TAR REMOVAL; SYNGAS PRODUCTION; SYNTHESIS GAS; CRACKING; NI; DECOMPOSITION;
D O I
10.1016/j.apenergy.2018.06.005
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
The inexpensive and abundant material, palygorskite, was used as a promising catalyst support to prepare Fe-Ni/Pal catalysts. Catalytic steam reforming of toluene as a biomass tar model compound over these catalysts was investigated in a fixed-bed reactor under different parameters, including reaction temperatures and S/C molar ratios. The stability and lifetime of Fe3Ni8/Palygorskite catalyst was evaluated under optimal conditions and its kinetic parameters were determined as well. The fresh and used catalysts were characterized using X-ray diffraction (XRD), H-2 temperature-programmed reduction (H-2-TPR), transmission electron microscopy (TEM), and Raman spectra. The results showed that the Fe3Ni8/Palygorskite catalyst with high dispersion was successfully prepared and exhibited superior catalytic performance compared with those of the monometallic catalysts (Fe-3/Palygorskite and Ni-8/Palygorskite) and the bare Palygorskite. Increasing the reaction temperature from 500 degrees C to 700 degrees C was beneficial for the toluene conversion and gaseous yields. The catalytic activity of Fe3Ni8/Palygorskite varied distinctly with the increase of S/C molar ratio and reached maximum at the the S/C molar ratio of 1.0. The apparent activation energy of 41.55 kJ mol I and the pre-exponential factor of 1.35 x 10(3) m(3) kg(-1) h were obtained for Fe3Ni8/Palygorskite in kinetic studies under optimal reaction conditions, respectively. The carbon deposition analysis of the used catalysts revealed that the formation of graphitic carbon rather than amorphous carbon was the main reason for the deactivation of Fe3Ni8/Palygorskite catalysts. When ceased the injection of steam into the reaction system, the graphitic carbon would be accelerating formed on the surface of the Fe3Ni8/Palygorskite and decreased its catalytic activity for toluene conversion. But owing to the water gas shift reaction, the catalytic activity of Fe3Ni8/Palygorskite seemed to recover gradually to its optimum.
引用
收藏
页码:827 / 837
页数:11
相关论文
共 50 条
  • [31] Effects of Cu and Fe Additives on Low-Temperature Catalytic Steam Reforming of Toluene Over Ni/AC Catalysts
    Yang, Xiaoqin
    Liu, Xuejing
    Guo, Tong
    Liu, Chuang
    [J]. CATALYSIS SURVEYS FROM ASIA, 2019, 23 (02) : 54 - 63
  • [32] Hydrogen Production By Ethanol Steam Reforming On Ni/oxide Catalysts
    Lazar, Mihaela D.
    Dan, Monica
    Mihet, Maria
    Borodi, George
    Almasan, Valer
    [J]. PROCESSES IN ISOTOPES AND MOLECULES (PIM 2011), 2012, 1425 : 131 - 134
  • [33] Steam reforming of glycerin for hydrogen production over Ni catalyst
    Adhikari, Sushil
    Fernando, Sandun
    Haryanto, Agus
    [J]. ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2007, 233
  • [34] Catalytic toluene steam reforming using Ni supported catalyst from pyrolytic peat
    Wang, Shuxiao
    Gu, Jing
    Shan, Rui
    Yuan, Haoran
    Yong, Chen
    [J]. Fuel Processing Technology, 2021, 224
  • [35] Catalytic toluene steam reforming using Ni supported catalyst from pyrolytic peat
    Wang, Shuxiao
    Gu, Jing
    Shan, Rui
    Yuan, Haoran
    Yong, Chen
    [J]. FUEL PROCESSING TECHNOLOGY, 2021, 224
  • [36] Oxidation resistance and effect of Pt addition to Ni/La0.7Sr0.3AlO3-δ for catalytic steam reforming of toluene for hydrogen production
    Sugiura, Yukihiro
    Mukai, Daiki
    Imori, Masaya
    Hashimoto, Takashi
    Ogo, Shuhei
    Sekine, Yasushi
    [J]. ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2014, 248
  • [37] Catalytic hydrogen production through WGS or steam reforming of alcohols over Cu, Ni and Co catalysts
    Kubacka, A.
    Fernandez-Garcia, M.
    Martínez-Arias, A.
    [J]. APPLIED CATALYSIS A-GENERAL, 2016, 518 : 2 - 17
  • [38] INFLUENCE OF THE SUPPORT ON NI BASED CATALYSTS FOR HYDROGEN PRODUCTION IN THE BIOMASS PYROLYSIS-CATALYTIC STEAM REFORMING
    Santamaria, L.
    Lopez, G.
    Amutio, M.
    Artetxe, M.
    Barbarias, I.
    Arregi, A.
    Cortazar, M.
    Olazar, M.
    [J]. PAPERS OF THE 26TH EUROPEAN BIOMASS CONFERENCE: SETTING THE COURSE FOR A BIOBASED ECONOMY, 2018, : 1142 - 1147
  • [39] Catalytic performance of nickel immobilized on organically modified montmorillonite in the steam reforming of ethanol for hydrogen production
    Yin X.-M.
    Xie X.-M.
    Wu X.
    An X.
    [J]. Xie, Xian-Mei (yxm6686@yeah.net), 1600, Science Press (44): : 689 - 697
  • [40] Hydrogen Production By Steam Reforming
    Elshout, Ray
    [J]. CHEMICAL ENGINEERING, 2010, 117 (05) : 34 - 38