Constitutive relations on creep for SnAgCuRE lead-free solder joints

被引:63
|
作者
Chen, ZG [1 ]
Shi, YW [1 ]
Xia, ZD [1 ]
机构
[1] Beijing Univ Technol, Sch Mat Sci & Engn, Minist Educ, Key Lab Adv Funct Mat, Beijing 100022, Peoples R China
关键词
SnAgCu; lead-free solder; rare earth (RE); creep; constitutive relations;
D O I
10.1007/s11664-004-0023-z
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Taking the most promising substitute of the Sn-3.8Ag-0.7Cu solder as the research base, investigations were made to explore the effect of rare earths (REs) on the creep performance of the Sn-3.8Ag-0.7Cu solder joints. The SnAgCu-0.1RE solder with the longest creep-rupture life was selected for subsequent research. Creep strain tests were conducted on Sn-3.8Ag-0.7Cu and SnAgCu-0.1RE solder joints in the intermediate temperature range from 298 K to 398 K, corresponding to the homologous temperatures eta = 0.606, 0.687, 0.748, and 0.809 and eta = 0.602, 0.683, 0.743, and 0.804, respectively, to acquire the relevant creep parameters, such as stress exponent and activation energy, which characterize the creep mechanisms. The final creep constitutive equations for Sn-3.8Ag-0.7Cu and SnAgCu-0.1RE solder joints were established, demonstrating the dependence of steady-state creep rate on stress and temperature. By correcting the apparent creep-activation energy of Sn-3.8Ag-0.7Cu and SnAgCu-0.1RE solder joints from the experiments, the true creep-activation energy is obtained. Results indicated that at low stress, the true creep-activation energy of Sn-3.8g-0.7Cu and SnAgCu-0.1RE solder joints is close to the lattice self-diffusion activation energy, so the steady-state creep rates of these two solder joints are both dominated by the rate of lattice self-diffusion. While at high stress, the true creep-activation energy of Sn-3.8Ag-0.7Cu and SnAgCu-0.1RE solder joints is close to the dislocation-pipe diffusion activation energy, so the steady-state creep rates are dominated by the rate of dislocation-pipe diffusion. At low stress, the best-fit stress exponents n of Sn-3.8Ag-0.7Cu and SnAgCu-0.1RE solder joints are 6.9 and 8.2, respectively, and the true creep-activation energy of them both is close to that of lattice self-diffusion. At high stress, it equals 11.6 and 14.6 for Sn-3.8Ag-0.7Cu and SnAgCu-0.1RE solder joints, respectively, and the true creep-activation energy for both is close to that of the dislocation-pipe diffusion. Thus, under the condition of the experimental temperatures and stresses, the dislocation climbing mechanism serves as the controlling mechanism for creep deformation of Sn-3.8Ag-0.7Cu and SnAgCu-0.1RE solder joints. The creep values of Sn-3.8Ag-0.7Cu and SnAgCu-0.1RE solder joints are both controlled by dislocation climbing. Dislocation glide and climb both contribute to creep deformation, but the controlling mechanism is dislocation climb. At low stress, dislocation climbing is dominated by the lattice self-diffusion process in the Sn matrix and dominated by the dislocation-pipe diffusion process at high stress.
引用
收藏
页码:964 / 971
页数:8
相关论文
共 50 条
  • [21] Electromigration issues in lead-free solder joints
    Chen, Chih
    Liang, S. W.
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2007, 18 (1-3) : 259 - 268
  • [22] How good are lead-free solder joints?
    Melton, Cindy
    Surface mount technology, 1995, 9 (06):
  • [23] Constitutive models of creep for lead-free solders
    Hongtao Ma
    Journal of Materials Science, 2009, 44 : 3841 - 3851
  • [24] Constitutive models of creep for lead-free solders
    Ma, Hongtao
    JOURNAL OF MATERIALS SCIENCE, 2009, 44 (14) : 3841 - 3851
  • [25] Comparative study of microstructures and properties of three valuable SnAgCuRE lead-free solder alloys
    Xiao, Weimin
    Shi, Yaowu
    Lei, Yongping
    Xia, Zhidong
    Gu, Fu
    JOURNAL OF ELECTRONIC MATERIALS, 2006, 35 (05) : 1095 - 1103
  • [26] Comparative study of microstructures and properties of three valuable SnAgCuRE lead-free solder alloys
    Weimin Xiao
    Yaowu Shi
    Yongping Lei
    Zhidong Xia
    Fu Guo
    Journal of Electronic Materials, 2006, 35 : 1095 - 1103
  • [27] Anand constitutive model of lead-free solder joints in 3D IC device
    Zhang, Liang
    Liu, Zhi-quan
    Ji, Yu-tong
    5TH INTERNATIONAL CONFERENCE ON MATHEMATICAL MODELING IN PHYSICAL SCIENCES (IC-MSQUARE 2016), 2016, 738
  • [28] Size and constraining effects in lead-free solder joints
    Cugnoni, J
    Botsis, J
    Janczak-Rusch, J
    ADVANCED ENGINEERING MATERIALS, 2006, 8 (03) : 184 - 191
  • [29] EVALUATION OF LEAD-FREE SOLDER JOINTS IN ELECTRONIC ASSEMBLIES
    ARTAKI, I
    JACKSON, AM
    VIANCO, PT
    JOURNAL OF ELECTRONIC MATERIALS, 1994, 23 (08) : 757 - 764
  • [30] Aspects of the structural evolution of lead-free solder joints
    Zribi, A
    Kinyanjui, R
    Borgesen, P
    Zavalij, L
    Cotts, EJ
    JOM-JOURNAL OF THE MINERALS METALS & MATERIALS SOCIETY, 2002, 54 (06): : 38 - 40