High-temperature oxidation behavior of CVD-SiC ceramic coating in wet oxygen and structural evolution of oxidation product: Experiment and first-principle calculations

被引:34
|
作者
Zhang, Pengfei [1 ]
Zhang, Yulei [1 ]
Chen, Guohui [1 ]
Gai, Wenhan [1 ]
Kong, Jingan [1 ]
机构
[1] Northwestern Polytech Univ, Shaanxi Prov Key Lab Fiber Reinforced Light Compo, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
基金
中国国家自然科学基金;
关键词
C; C composites; CVD-SiC ceramic coating; Oxidation behavior; Wet oxygen; First-principle calculation; SILICON-CARBIDE; C/C COMPOSITES; CARBON; ENVIRONMENT; PROTECTION; DYNAMICS; AL2O3;
D O I
10.1016/j.apsusc.2021.149808
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
SiC ceramics and SiC ceramic coatings on carbon/carbon (C/C) composites were prepared by chemical vapor deposition (CVD) method to investigate their oxidation behaviors in wet oxygen at 1773 K. The experimental results demonstrated that water vapor could increase the oxidation rate of SiC, and promote the crystallization of SiO2. By the Raman and infrared spectroscopic analyses, the existence of Si-OH vibration modes in the oxide scales indicated that the reaction between water vapor and silica could occur at high temperatures. Besides, firstprinciple molecular dynamics (FPMD) simulations and the static calculations based on density functional theory (DFT) also confirmed the occurrence of the reaction and illustrated that the reaction was caused by the co-effect of O and H atoms from the water, resulting in the breakage of the Si-O bonds in silica. After oxidation for 30 h, the weight loss of CVD-SiC coated C/C samples in wet oxygen reduced to 3.47%, which was ascribed to that the formation of abundant oxide scale acted as an effective oxidation barrier by healing cracks on SiC coatings. However, the crystallization and structural variation of the oxide scale might be harmful to the long-term oxidation in the condition of high-speed gaseous scour.
引用
收藏
页数:11
相关论文
共 36 条
  • [31] C/SiC Gradient Oxidation Protective Coating on Graphite by Modified Reactive Melt Infiltration Method: Effects of Processing Parameters on Transition Interface Thickness and High-Temperature Anti-oxidation Behavior
    Alireza Abdollahi
    Naser Ehsani
    Metallurgical and Materials Transactions A, 2017, 48 : 265 - 278
  • [32] C/SiC Gradient Oxidation Protective Coating on Graphite by Modified Reactive Melt Infiltration Method: Effects of Processing Parameters on Transition Interface Thickness and High-Temperature Anti-oxidation Behavior
    Abdollahi, Alireza
    Ehsani, Naser
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2017, 48A (01): : 265 - 278
  • [33] Recycling of MoSi2-based industrial solid wastes for the fabrication and high-temperature oxidation behavior of MoSi2-ZrSi2-SiC composite coating
    Zhu, Lu
    Zhang, Shipeng
    Ye, Fan
    Ren, Xuanru
    Feng, Peizhong
    COMPOSITES PART B-ENGINEERING, 2024, 274
  • [34] High-temperature oxidation behavior and mechanism of the Si-based thermal protective coating for SiCf/SiC composites under static oxidation and H2O/O2/Na2SO4 corrosion oxidation
    Quan, Huafeng
    Wang, Lianyi
    Huang, Juntong
    Yang, Huiyong
    Yang, Xiaotian
    Dong, Xiaohui
    Luo, Hao
    Cui, Guangyuan
    Luo, Ruiying
    COMPOSITES PART B-ENGINEERING, 2022, 238
  • [35] Effect of TiC Reinforcement on Densification, Structural Evolution and High-Temperature Oxidation Behaviour of ZrB2-20 vol pct SiC Composite (vol 54, pg 1252, 2023)
    Sengupta, Pradyut
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2023, 54 (08): : 3370 - 3370
  • [36] Multicomponent (Hf0.25Zr0.25Ti0.25Cr0.25)B2 ceramic modified SiC-Si composite coatings: In-situ synthesis and high-temperature oxidation behavior
    Zhang, Pei
    Cheng, Chunyu
    Liu, Bing
    Xie, Wei
    Zhu, Xiaofei
    Zhang, Jiaping
    Fu, Qiangang
    CERAMICS INTERNATIONAL, 2022, 48 (09) : 12608 - 12624